| 多向压缩中AZ31镁合金变形行为的EBSD跟踪研究 |
| 黄洪涛1),Godfrey Andrew1),刘伟1),付宝勤1),刘庆2) |
1)清华大学材料学院先进材料教育部重点实验室, 北京100084
2)重庆大学材料科学与工程学院,重庆400044 |
|
| DEFORMATION BEHAVIOR OF AZ31 MAGNESIUM ALLOY DURING MULTIAXIAL COMPRESSION BY EBSD TRACKING |
| HUANG Hongtao1), Godfrey Andrew1), LIU Wei1), FU Baoqin1),LIU Qing2) |
1)Key Laboratory of Advanced Materials (MOE), School of Materials Science and Engineering, Tsinghua University, Beijing 100084
2)School of Materials Science and Engineering, Chongqing University, Chongqing 400044 |
引用本文:
黄洪涛,Godfrey Andrew,刘伟,付宝勤,刘庆. 多向压缩中AZ31镁合金变形行为的EBSD跟踪研究[J]. 金属学报, 2013, 49(8): 932-938.
HUANG Hongtao,
Godfrey Andrew,
LIU Wei,
FU Baoqin,
LIU Qing.
DEFORMATION BEHAVIOR OF AZ31 MAGNESIUM ALLOY DURING MULTIAXIAL COMPRESSION BY EBSD TRACKING[J]. Acta Metall Sin, 2013, 49(8): 932-938.
| [1]Lou X Y, Li M, Boger R K, Agnew S R, Wagoner R H.Int J Plast, 2007; 23: 44
[2]Liu Q. Acta Metall Sin, 2010; 46: 1458
(刘庆. 金属学报, 2010; 46: 1458)
[3]Barnett M R. Mater Sci Eng, 2007; A464: 1
[4]Barnett M R. Mater Sci Eng, 2007; A464: 8
[5]Martin E, Capolungo L, Jiang L, Jonas J J. Acta Mater, 2010; 58: 3970
[6]Luo J R, Godfrey A, Liu W, Liu Q. Acta Mater, 2012;60: 1986
[7]Luo J R, Liu Q, Liu W, Godfrey A. Acta Metall Sin,2011; 47: 1567
(罗晋如, 刘庆, 刘伟, Godfrey A. 金属学报, 2011; 47:1567)
[8]Luo J R, Liu Q, Liu W, Godfrey A. Acta Metall Sin,2012; 48: 717
(罗晋如, 刘庆, 刘伟, Godfrey A. 金属学报, 2012; 48:717)
[9]Huang H T, Liu W, Godfrey A, Tang R H, Liu Q. Acta Metall Sin, 2012; 48: 357
(黄洪涛, 刘伟, Godfrey A, 唐瑞鹤, 刘庆. 金属学报,2012; 48: 357)
[10]Wang Y N, Huang J C. Acta Mater, 2007; 55: 897
[11]Proust G, Tome C N, Jain A, Agnew S R. Int JPlast, 2009; 25: 861
[12]Chapelle D, Darrieulat M. Mater Sci Eng, 2003;A347: 32
[13]Lineau C, Rey C, deLesegno P V. Mater Sci Eng,1997; A234: 853
[14]Delaire F, Raphanel J L, Rey C. Acta Mater, 2000;48: 1075
[15]Barnett M R, Jacob S, Gerard B F, Mullins J G. Scr Mater, 2008; 59: 1035
[16]Allais L, Bornert M, Bretheau T, Caldemasion D.Acta Mater, 1994; 42: 3865
[17]Huang H T,PhD Dissertation, Tsinghua University,Beijing, 2013
(黄洪涛. 清华大学博士学位论文, 北京, 2013)
[18]Huang H T, Godfrey A, Liu W, Tang R H, Liu Q. Acta Metall Sin, 2012; 48: 915 (黄洪涛, Godfrey A, 刘伟, 唐瑞鹤, 刘庆. 金属学报,2012; 48: 915)
[19]Nave M D, Barnett M R. Scr Mater, 2004; 51: 881
[20]Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303
(杨续跃, 张雷. 金属学报, 2009; 45: 1303)
[21]Brown D W, Agnew S R, Bourke M A M, Holden T M, Vogel S C,Tome C N. Mater Sci Eng, 2005; A399: 1
[22]Clausen B, Tome C N, Brown D W, Agnew S R. Acta Mater, 2008; 56: 2456
[23]Lou C, Zhang X Y, Wang R H, Duan G L, Liu Q. Acta Metall Sin, 2013; 49: 291
(娄超,张喜燕, 汪润红, 段高林, 刘庆.金属学报, 2013; 49: 291)
[24]Wu L, Agnew S R, Brown D W, Stoica G M, Clausen B, Jain A,Fielden D E, Liaw P K. Acta Mater, 2008; 56: 3699
[25]Wu L, Jain A, Brown D W, Stoica G M, Agnew S R, Clausen B,Fielden D E, Liaw P K. Acta Mater, 2008; 56: 688
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|