金属学报  2013, Vol. 49 Issue (8): 925-931    DOI: 10.3724/SP.J.1037.2013.00166
  论文 本期目录 | 过刊浏览 |
试样温度对激光重熔Zr55Cu30Al10Ni5块体非晶合金晶化的影响
杨高林,林鑫,胡桥,宋梦华,汪志太,黄卫东
西北工业大学凝固技术国家重点实验室, 西安 710072
EFFECT OF SPECIMEN TEMPERATURE ON CRYSTALLIZATION DURING LASER REMELTITNG Zr55Cu30Al10Ni5 BULK METALLIC GLASS
YANG Gaolin, LIN Xin, HU Qiao, SONG Menghua, WANG Zhitai, HUANG Weidong
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072
引用本文:

杨高林,林鑫,胡桥,宋梦华,汪志太,黄卫东. 试样温度对激光重熔Zr55Cu30Al10Ni5块体非晶合金晶化的影响[J]. 金属学报, 2013, 49(8): 925-931.
YANG Gaolin, LIN Xin, HU Qiao, SONG Menghua, WANG Zhitai, HUANG Weidong. EFFECT OF SPECIMEN TEMPERATURE ON CRYSTALLIZATION DURING LASER REMELTITNG Zr55Cu30Al10Ni5 BULK METALLIC GLASS[J]. Acta Metall Sin, 2013, 49(8): 925-931.

全文: PDF(735 KB)  
摘要: 

分别对在液N冷却、液Ar冷却、置于室温环境和加热到473 K条件下的Zr55Cu30Al10Ni5非晶合金试样进行脉冲激光重熔实验,以研究试样温度对激光重熔非晶合金晶化的影响. 结果显示, 在采用有、无Ar气侧吹的情况下基材温度, 特别是基材温度较低时,对激光重熔块体非晶合金晶化的影响规律明显不同. 激光重熔实验中, 无Ar气侧吹时,对在液Ar冷却和置于室温环境下的试样, 激光重熔后热影响区的晶化程度类似,在液Ar冷却下的试样熔池较深. 对于加热到473 K的试样,热影响区的晶化程度最为严重, 且熔池最深. 激光重熔实验中采用Ar气侧吹时,与室温环境的试样相比, 液N冷却对于激光重熔非晶合金的晶化有明显的抑制作用.试样温度对非晶合金晶化的影响源于: 一、试样本身的温度越低,热影响区的冷速越快, 晶化越少; 二、试样周围的气氛温度越低, 激光重熔过程中,等离子体对激光的屏蔽效应也越小, 实际能量输入越高, 晶化越严重. 有Ar气侧吹时,气氛温度为侧吹气体的温度, 所以试样温度较低, 晶化较少. 在没有Ar气侧吹时,气氛温度接近于试样温度, 上述2个因素同时作用,导致试样温度对晶化的影响规律非单调变化.

关键词 : Zr55Cu30Al10Ni5非晶合金,  试样温度,  激光重熔,  晶化    
Abstract:

Zr55Cu30Al10Ni5 bulk metallic glasses were remelted by pulsed laser at liquid N (Ar) cooling, room temperature and 473 K. The results show that the effect of specimen temperatures on the crystallization of specimens during laser remelting metallic glasses depends on the Ar blowing. If there is no Ar blowing, the crystallization of the specimen during laser remelting under liquid Ar cooling and room temperature is similar while the molten pool is deeper for liquid Ar cooling. And the specimen remelted at 473 K was most seriously crystallized with the deepest molten pool. But comparing the specimen at room temperature, the crystallization of the specimen at liquid N was suppressed during laser remelting with Ar blowing. The effects of specimen temperatures on the crystallization of metallic glasses during laser remelting are: First, the lower specimen temperature can increase the cooling rate of specimen and therefore reduce its crystallization. Secondly, the lower specimentemperature makes  the atmosphere around the specimen cooled down, reduces the shielding effect of plasma and increases the actual laser energy input into the specimen, resulting in more serious crystallization of the specimen. If there is Ar blowing, the atmosphere temperatures are similar to that at the liquid Ar cooling leading to the crystallization of the specimen to reduced. If there is no Ar blowing, the atmosphere temperature is similar to the temperature of specimen itself. In this case, the crystallization of the specimens is jointly determined by the temperature of the specimen itself and the atmosphere temperature around the specimens, which is not monotonous.

Key words: Zr55Cu30Al10Ni5 bulk metallic glass    specimen temperature    laser remelt    crystallization
收稿日期: 2013-04-07     
基金资助:

国家重点基础研究发展计划项目2011CB610402,国家高技术研究发展计划项目2013AA031103,高等学校博士学科点专项科研基金项目20116102110016和高等学校学科创新引智计划项目08040资助

作者简介: 杨高林, 男, 1980年生, 博士生

[1] Wang C, Zhang Q S, Jiang F, Zhang H F, Hu Z Q.  Acta Metall Sin, 2002; 38: 765
(王成, 张庆生, 江峰, 张海峰, 胡壮麒. 金属学报, 2002; 38: 765)
[2] Inoue A, Takeuchi A.  Acta Mater, 2011; 59: 2243
[3] Byrne C, Eldrup M.  Science, 2008; 321: 502
[4] Kumagai N, Samata Y, Kawashima A, Asami K, Hashimoto K.  J Non-Cryst Solids, 1987; 93: 78
[5] Kim J H, Lee C, Lee D M, Sun J H, Shin S Y, Bae J C.  Mater Sci Eng, 2007; A449-451: 872
[6] Chen B, Pang S, Han P, Li Y, Yavari A R, Vaughan G, Zhang T.  J Alloys Compd, 2010; 504: S45
[7] Yue T M, Su Y P, Yang H O.  Mater Lett, 2007; 61: 209
[8] Yang G L, Lin X, Liu F C, Hu Q, Ma L, Li J F, Wei D H.  Intermetallics, 2012; 22: 110
[9] Lin X, Yang H O, Chen J, Huang W D.  Acta Metall Sin, 2006; 42: 361
(林鑫, 杨海欧, 陈静, 黄卫东. 金属学报, 2006; 42: 361
[10] Cao J, Liu F C, Lin X, Huang C P, Chen J, Huang W D.  Opt Laser Technol, 2013; 45: 228
[11] Liu F C, Lin X, Huang C P, Song M H, Yang G L, Chen J, Huang W D.  J Alloys Compd,2011; 509: 4505
[12] Cervo R, Ferro P, Tiziani A, Zucchi F.  J Mater Sci, 2010; 45: 4378
[13] Liu F C, Lin X, Yang G L, Song M H, Chen J, Huang W D.  Opt Laser Technol, 2011; 43: 208
[14] Jia W P, Chen J, Lin X, Zhong C W, Huang W D.  Acta Metall Sin, 2007; 43: 546
(贾文鹏, 陈静, 林鑫, 钟诚文, 黄卫东. 金属学报, 2007; 43: 546)
[15] Liu F C, Lin X, Yang G L, Huang C P, Chen J, Huang W D.  Acta Metall Sin, 2010; 46: 1047
(刘奋成, 林鑫, 杨高林, 黄春平, 陈静, 黄卫东. 金属学报, 2010; 46: 1047)
[16] Laeng J, Stewart J G, Liou F W.  Int J Prod Res, 2000; 38: 3973
[17] Sun H, Flores K M.  Metall Mater Trans, 2010; 41A: 1752
[18] Zheng B, Zhou Y, Smugeresky J E, Lavernia E J.  Metall Mater Trans, 2009; 40A: 2009
[19] Wang H S, Chen H G, Jang J S C, Chiou M S.  Mater Sci Eng, 2010; A528: 338
[20] Yamasaki M, Kagao S, Kawamura Y.  Scr Mater, 2005; 53: 63
[21] Hu Q, Lin X, Yang G L, Huang W D, Li J F.  Acta Metall Sin, 2012; 48: 1467
(胡桥, 林鑫, 杨高林, 黄卫东, 李金富. 金属学报, 2012; 48: 1467)
[22] Xing D W, Shen J, Zhang L F, Sun J F, Wang X D, Wang H.  J Alloys Compd, 2009; 481: 531
[23] Zheng Q G, Gu J H.  Interaction between Laser and Matter. Wuhan: Huazhong
University of Science and Technology Press, 1996: 129
(郑启光, 辜建辉. 激光与物质相互作用. 武汉: 华中理工大学出版社, 1996: 129)
[24] Kuo T Y, Lin Y D.  Mater Trans, 2007; 48: 219
[25] Shao D, Hu B, Zheng Q G.  Advanced Laser Manufacturing Technology and
Device Integration. Beijing: Science Press, 2009: 44
(邵丹, 胡兵, 郑启光. 激光先进制造技术与设备集成. 北京: 科学出版社, 2009: 44)

[1] 郭璐, 朱乾科, 陈哲, 张克维, 姜勇. Fe76Ga5Ge5B6P7Cu1 合金的非等温晶化动力学[J]. 金属学报, 2022, 58(6): 799-806.
[2] 李金富, 李伟. 铝基非晶合金的结构与非晶形成能力[J]. 金属学报, 2022, 58(4): 457-472.
[3] 张金勇, 赵聪聪, 吴宜谨, 陈长玖, 陈正, 沈宝龙. (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x 高熵非晶合金薄带的结构特征及其晶化行为[J]. 金属学报, 2022, 58(2): 215-224.
[4] 韩录会, 柯海波, 张培, 桑革, 黄火根. 非晶态U60Fe27.5Al12.5 合金的晶化动力学行为[J]. 金属学报, 2022, 58(10): 1316-1324.
[5] 王祖敏,张安,陈媛媛,黄远,王江涌. 金属诱导晶化基础与应用研究进展[J]. 金属学报, 2020, 56(1): 66-82.
[6] 金辰日, 杨素媛, 邓学元, 王扬卫, 程兴旺. 纳米晶化对锆基非晶合金动态压缩性能的影响[J]. 金属学报, 2019, 55(12): 1561-1568.
[7] 杨高林, 林鑫, 卢献钢. 激光多次熔凝Zr55Cu30Al10Ni5非晶合金的晶化形态与演化机理[J]. 金属学报, 2019, 55(12): 1544-1550.
[8] 张媛媛,林鑫,魏雷,任永明. 激光立体成形退火态Zr55Cu30Al10Ni5粉末的晶化行为[J]. 金属学报, 2017, 53(7): 824-832.
[9] 马殿国,王英敏,李艳辉,张伟. Co含量对熔体快淬Fe55-xCoxPt15B30合金的组织结构与磁性能的影响[J]. 金属学报, 2017, 53(5): 609-614.
[10] 王理林, 林鑫, 王永辉, 宇红雷, 黄卫东. 激光重熔熔池凝固组织的实时观察研究[J]. 金属学报, 2015, 51(4): 492-498.
[11] 王向杰 游国强 张均成 龙思远. 压铸AZ91D镁合金母材气孔在重熔过程的遗传性研究[J]. 金属学报, 2012, 48(12): 1437-1445.
[12] 胡桥 林鑫 杨高林 黄卫东 李金富. 不同形态和热历史条件下Zr55Al10Ni5Cu30非晶合金的晶化行为[J]. 金属学报, 2012, 48(12): 1467-1473.
[13] 刘彤 朱亚蓉 张同文 张涛. 加压退火对Gd36La20Al24Co20块体非晶合金晶化行为和热稳定性的影响[J]. 金属学报, 2011, 47(4): 502-506.
[14] 龚静 杨红旺 杨柏俊 王瑞春 李荣德 王建强. 非晶态及部分晶化态Al-Ni-Y合金的磁性[J]. 金属学报, 2011, 47(3): 333-336.
[15] 李玉玲 马伟民 闻雷 温强 苑晓宇. 制备参量对BaZrO3:Ce纳米粉体形貌和发光性能的影响[J]. 金属学报, 2011, 47(1): 95-101.