| 工业纯Ti在模拟高放废物地质处置环境中的缝隙腐蚀行为 |
| 魏欣1,2),董俊华2),柯伟2) |
1) 大连理工大学材料科学与工程学院, 大连 116024
2) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
|
|
| CREVICE CORROSION OF GRADE-2 Ti IN SIMULATED GROUNDWATER FOR GEOLOGICAL DISPOSAL OF HIGH-LEVEL RADIOACTIVE NUCLEAR WASTE |
| WEI Xin1,2), DONG Junhua2), KE Wei2) |
1) College of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
2) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
魏欣,董俊华,柯伟. 工业纯Ti在模拟高放废物地质处置环境中的缝隙腐蚀行为[J]. 金属学报, 2013, 49(6): 675-681.
WEI Xin,
DONG Junhua,
KE Wei.
CREVICE CORROSION OF GRADE-2 Ti IN SIMULATED GROUNDWATER FOR GEOLOGICAL DISPOSAL OF HIGH-LEVEL RADIOACTIVE NUCLEAR WASTE[J]. Acta Metall Sin, 2013, 49(6): 675-681.
| [1] Lee S G, Solomon A A. Mater Sci Eng, 2006; A434: 114
[2] Su R, Cheng Q F, Wang J, Zhao H G, Guo Y H, Chen W M, Jin Y X. World Nucl Geosci, 2011; 28: 45
(苏锐, 程琦福, 王驹, 赵宏刚, 郭永海, 陈伟明, 金远新. 世界核地质科学, 2011; 28: 45)
[3] Wang J, Chen W M, Su R, Guo Y H, Jin Y X. Chin J Rock Mech Eng, 2006; 25: 649
(王驹, 陈伟明, 苏锐, 郭永海, 金远新. 岩石力学与工程学报, 2006; 25: 649)
[4] Bennett D G, Gens R. J Nucl Mater, 2008; 379: 1
[5] Rempe N T. Prog Nucl Energy, 2007; 49: 365
[6] Chapman N, Hooper A. Proc Geologist Assoc, 2012; 123: 46
[7] Feron D, Crusset D, Gras J M. J Nucl Mater, 2008; 379: 16
[8] Johnson L H, Shoesmith D W, Ikeda B M, King F. Mater Res Soc Symp Proc, 1992; 257: 439
[9] Shoesmith D W, Hocking W H, Ikeda B M, King F, No$\ddot{\rm e$l J J, Sunder S. Can J Chem, 1997; 75: 1566
[10] Nakayama G, Sakakibara Y, Taniyama Y, Cho H, Jintoku T, Kawakami S, Takemoto M. J Nucl Mater, 2008; 379: 174
[11] Nishimura T. J Nucl Mater, 2009; 385: 495
[12] He X, Noel J J, Shoesmith D W. J Electrochem Soc, 2002; 149: B440
[13] Mckay P, Mitton D B. Corrosion, 1985; 41: 52
[14] He X, Noel J J, Shoesmith D W. Corrosion, 2004; 60: 378
[15] Tsujikawa S, Kojima Y. Mater Res Soc Symp Proc, 1991; 212: 261
[16] Tsujikawa S, Kojima Y. Mater Res Soc Symp Proc, 1993; 294: 311
[17] Yan L, Noel J J, Shoesmith D W. Electrochim Acta, 2011; 56: 1810
[18] Yokoyama K, Ogawa T, Asaoka K, Sakai J. Mater Sci Eng, 2004; A384: 19
[19] Nishimura R, Shirono J, Jonokuchi A. Corros Sci, 2008; 50: 2691
[20] Abdulsalam M I. J Mater Eng Perform, 2007; 16: 736
[21] Kennell G F, Evitts R W, Heppner K L. Corros Sci, 2008; 50: 1716
[22] Rajendran N, Nishimura T. Mater Corros, 2007; 58: 334
[23] Han D, Jiang Y M, Shi C, Deng B, Li J. J Mater Sci, 2012; 47: 1018
[24] Han D, Jiang Y M, Deng B, Zhang L, Gao J, Tan H, Li J. Corrosion, 2011; 67: 025004-1
[25] Pickering H W. Corros Sci, 1989; 29: 325
[26] Al-Zahrani A M, Pickering H W. Electrochim Acta, 2005; 50: 3420
[27] Yan M C, Weng Y J. J Chin Soc Corros Prot, 2004; 24: 95
(闫茂成, 翁永基. 中国腐蚀与防护学报, 2004; 24: 95)
[28] Heppner K L, Evitts R W, Postlethwaite J.J Electrochem Soc, 2005; 152: B89
[29] Brigham R J.Corros Sci, 1992; 33: 799
[30] Brigham R J.Corros Sci, 1988; 28: 57
[31] Pickering H W. J Electrochem Soc, 2003; 150: K1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|