| 电流及其极性对浸铜碳滑板摩擦磨损性能的影响 |
| 汪逸安, 李金许, 乔利杰 |
| 北京科技大学腐蚀与防护中心环境断裂教育部重点实验室, 北京 100083 |
|
| EFFECTS OF ELECTRICAL CURRENT AND ITS POLARITY ON THE PROPERTIES OF FRICTION AND WEAR OF COPPER-IMPREGNATED METALLIZED CARBON |
| WANG Yian, LI Jinxu, QIAO Lijie |
| Corrosion and Protection Center, Key Laboratory for Environment Fracture Laboratory (MOE), University of Science and Technology Beijing, Beijing 100083 |
引用本文:
汪逸安, 李金许, 乔利杰. 电流及其极性对浸铜碳滑板摩擦磨损性能的影响[J]. 金属学报, 2012, 48(4): 480-484.
,
,
.
EFFECTS OF ELECTRICAL CURRENT AND ITS POLARITY ON THE PROPERTIES OF FRICTION AND WEAR OF COPPER-IMPREGNATED METALLIZED CARBON[J]. Acta Metall Sin, 2012, 48(4): 480-484.
| [1] Kubo S, Tsuchiya H, Ikeuchi J. Q Rep RTRI, 1997; 38: 76[2] Qu C Y, Lu Z K. Carbon, 2008; 3: 45 (曲春浴, 陆宗奎. 炭素, 2008; 3: 45)[3] Correia J B, Davies H A, Sellars C M. Acta Mater, 1997; 45: 177[4] Jia S G, Liu P, Ren F Z, Tian B H, Zheng M S, Zhou G S. Mater Sci Eng,2005; A398: 262[5] Batra I S, Dey G K, Kulkarni U D, Banerjee S. J Nucl Mater,2001; 299: 91[6] Yasar I, Canakci A, Arslan F. Tribology Int, 2007; 40: 1381[7] Wang G M, Zhang Y Z, Du S M, Liu W M. Tribology, 2007; 27: 346 (王观民, 张永振, 杜三明, 刘维民. 摩擦学学报, 2007; 27: 346)[8] Yang X W, Zhang Y Z, Qiu M, Du S M. Tribology, 2007; 27: 25 (杨晓伟, 张永振, 邱明, 杜三明.摩擦学学报, 2007; 27: 25)[9] Dow T A, Kannel J W. Wear, 1982; 79: 93[10] Jia S G, Liu P, Ren F Z, Tian B H, Zheng M S, Zhou G S. Wear, 2007; 262: 772[11] Ma X C, He G Q, He D H, Chen C S, Hu Z F. Wear, 2008; 265: 1087[12] Zheng R G, Zhan Z J, Wang W K. Wear, 2010; 268: 72[13] Tu C J, Chen Z H, Chen D, Yan H G, He F Y. Trans Nonferr Met Soc China, 2008; 18: 1157[14] Kubo S, Kato K. Wear, 1998; 216: 172[15] Dong L, Chen G X, Zhu M H, Zhou Z R. Wear, 2007; 263: 598[16] Kotake S, Sakurada H, Suzuki T, Suzuki Y. Tribology Int,2008; 41: 44[17] Kogut L, Komvopoulos K. J Appl Phys, 2003; 94: 3153[18] Kogut L. J Appl Phys, 2005; 97: 103723[19] Nagasawa H, Kato K. Wear, 1998; 216: 179[20] Bryant M D, Wang J P. Wear, 1995; 181-183: 668[21] Bhushan B, Davis R E, Gordon M. Thin Solid Films, 1985; 123: 93[22] Chen G X, Li F X, Dong L, Zhu M H, Zhou Z R. Tribology Int,2009; 42: 934[23] Ding T, Chen G X, Wang X, Zhu M H, Zhang W H, Zhou W X. Tribology Int, 2011; 44: 437[24] Hu Z L, Chen Z H, Xia J T. Wear, 2008; 264: 11[25] Gershman J S, Bushe N A. Surf Coat Technol, 2004; 186: 405[26] Dong L. PhD Thesis, Southwest Jiaotong University, Chengdu, 2008 (董霖. 西南交通大学博士论文, 成都, 2008)[27] Chen Z Z. Dynamics of Lighting by Ionized Gas. Beijing:Science Press, 1996: 44 (陈宗柱. 电离气体发光动力学. 北京: 科学出版社, 1996: 44)[28] Tu C J. PhD Thesis, Hunan University, Changsha, 2009 (涂川俊. 湖南大学博士论文, 长沙, 2009)[29] Neumark D M, Lykke K R, Andersen T, Lineberger W C. Phys Rev,1985; 32A: 1890[30] Wang J W, Zhong S H. Prog Chem, 1998; 10: 374 (王建伟, 钟顺和. 化学进展, 1998; 10: 374) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|