| 相场法模拟弹性应变能对Ti-Al-Nb合金 α2→ O相变粗化动力学的影响 |
| 周广钊,王永欣,陈铮 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| PHASE-FIELD METHOD SIMULATION OF THE EFFECT OF ELASTIC STRAIN ENERGY ON COARSENING DYNAMICS DURING THE α2→ O PHASE TRANSFORMATION IN Ti-Al-Nb ALLOYS |
| ZHOU Guangzhao, WANG Yongxin, CHEN Zheng |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
周广钊,王永欣,陈铮. 相场法模拟弹性应变能对Ti-Al-Nb合金 α2→ O相变粗化动力学的影响[J]. 金属学报, 2012, 48(4): 485-491.
,
,
.
PHASE-FIELD METHOD SIMULATION OF THE EFFECT OF ELASTIC STRAIN ENERGY ON COARSENING DYNAMICS DURING THE α2→ O PHASE TRANSFORMATION IN Ti-Al-Nb ALLOYS[J]. Acta Metall Sin, 2012, 48(4): 485-491.
| [1] Zhang Y G, Han Y F, Chen G L, Guo J T, Wan X J, Feng D. Structural Intermetallics. Beijing: National Defence Industrial Press, 2001: 705 (张永刚, 韩雅芳, 陈国良, 郭建亭, 万晓景, 冯涤. 金属间化合物结构材料.北京: 国防工业出版社, 2001: 705)[2] Li C G, Fu H Z, Yu Q. Aerospace Materials. Beijing: National Defence Industrial Press, 2002: 100 (李成功, 傅恒志, 于翘. 航空航天材料. 北京: 国防工业出版社, 2002: 100)[3] Lin D L. J Shanghai Jiao Tong Univ, 1998; 32: 95 (林栋梁. 上海交通大学学报, 1998; 32: 95)[4] Heng Q Y. Mater Sci Eng, 1999; A263: 289[5] Peng C Q, Huang B Y, He Y H. Chin J Nonferrous Met, 2001; 11: 527 (彭超群, 黄伯云, 贺跃辉. 中国有色金属学报. 2001; 11: 527)[6] Xiao G, Huang B Y, Qu X H, He Y H, Zhou K Z. Rare Met, 1996; 20: 50 (肖刚, 黄伯云, 曲选辉, 贺跃辉, 周科朝. 稀有金属, 1996; 20: 50)[7] Brady M P, Brindley W J, Smialek J L. JOM, 1996; 48: 46[8] Kui G Y, Sun L. Mater Rev, 2008; 22: 339 (隗功益, 孙丽. 材料导报, 2008; 22: 339)[9] Maki K, Shioda M, Sayashi M, Shimizu T, Isobe S. Mater Sci Eng,1992; A153: 591[10] Haanappel V A C, Clemens H, Stroosnijder M F. Intermetallics,2002; 10: 293[11] Zhang W J, Chen G L, Sun Z Q. Scr Metall Mater, 1993; 28: 563[12] Darolia R, Lewandowski J J, Liu C T, Martin P L, Miracle D B, Nathal M V. Structural Intermetallics. Warrendale: Metallurgical Society of AIME, 1993: 19[13] Leyens C, Peters M. Titanium and Titanium Alloys. Weinheim: Wiley-VCH Verlag GmbH & Co. KGaA, 2003: 54[14] Banerjee D, Gogia A K, Nandy T K, Joshi V A. Acta Metall, 1988; 36: 871[15] Bendersky L A, Roytburd A, Boettinger W J. J Res Natl Inst Stand Technol, 1993; 98: 561[16] Bendersky L A, Boettinger W J. J Res Natl Inst Stand Technol, 1993; 98: 585[17] Bendersky L A, Boettinger W J. Acta Metall Mater, 1994; 42: 2337[18] Muraleedharan K, Banerjee D. Scr Metall Mater, 1993; 29: 527[19] Muraleedharan K, Banerjee D. Philos Mag, 1995; 71A: 1011[20] Muraleedharan K, Nandy T K, Banerjee D, Lele S. Intermetallics, 1995; 3: 187[21] Pierron X, De Graef M, Thompson A W. Phil Mag, 1998; 77A: 1399[22] Gogia A K, Nandy T K, Banerjee D, Carisey T, Strudel J L, Franchet J M. Intermetallics, 1998; 6: 741[23] Wen Y H, Wang Y, Bendersky L A, Chen L Q. Acta Mater, 2000; 48: 4125[24] Wen Y H, Wang Y, Chen L Q. Acta Mater, 2001; 49: 13[25] Chen L Q, Shen J. Comput Phys Commun, 1998; 10: 147[26] Zhu J Z, Chen L Q. Phys Rev, 1999; 60E: 3565 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|