| 变形温度对Fe-23Mn-2Al-0.2C TWIP钢变形机制的影响 |
| 秦小梅, 陈礼清, 邸洪双, 邓伟 |
| 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| EFFECT OF DEFORMATION TEMPERATURE ON TENSILE DEFORMATION MECHANISM OF Fe-23Mn-2Al-0.2C TWIP STEEL |
| QIN Xiaomei, CHEN Liqing, DI Hongshuang, DENG Wei |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
引用本文:
秦小梅 陈礼清 邸洪双 邓伟. 变形温度对Fe-23Mn-2Al-0.2C TWIP钢变形机制的影响[J]. 金属学报, 2011, 47(9): 1117-1122.
,
,
,
.
EFFECT OF DEFORMATION TEMPERATURE ON TENSILE DEFORMATION MECHANISM OF Fe-23Mn-2Al-0.2C TWIP STEEL[J]. Acta Metall Sin, 2011, 47(9): 1117-1122.
| [1] Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387–389: 158[2] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438[3] Hokka M, Kuokkala V T, Curtze S, Vuoristo T, Apostol M. J Phy IV, 2006; 134: 1301[4] Gr¨assel O, Kr¨uger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391[5] Wang S H, Liu Z Y, Wang G D. Acta Metall Sin, 2009; 45: 1083(王书晗, 刘振宇, 王国栋. 金属学报, 2009; 45: 1083)[6] Hamada A S, Karjalainen L P, Somani M C. Mater Sci Eng, 2007; A467: 114[7] Huang B X, Wang X D, Wang L, Rong Y H. Metall Mater Trans, 2008; 39A: 717[8] Lu F Y, Yang P, Meng L, Mao W M. Acta Metall Sin, 2010; 46: 1153(鲁法云, 杨平, 孟 利, 毛卫民. 金属学报, 2010; 46: 1153)[9] Barbier D, Gey N, Allain S, Bozzolo N, Humbert M. Mater Sci Eng, 2009; A500: 196[10] Chen L, Kim H S, Kim S K, Cooman B C. ISIJ Int, 2007; 47: 1804[11] Jim´enez J A, Frommeyer G. Mater Charact, 2010; 61: 221[12] Renard K, Ryelandt S, Jacquies P J. Mater Sci Eng, 2010; A527: 2969[13] Brahmi A, Borrelly R. Acta Mater, 1997; 45: 1889[14] Frommeyer G, Brux U. Steel Res Int, 2006; 77: 627[15] Yoo J D, Park K T. Mater Sci Eng, 2008; A496: 417[16] Dumay A, Chateau J P, Allain S, Migot S, Bouaziz O. Mater Sci Eng, 2008; A483–484: 184[17] Ehab E D, Surya R K, Roger D D. Metall Mater Trans, 1999; 30A: 1223[18] Surya R K. Int J Plast, 1998; 14: 1265 |
|