| 镍基690合金中晶界碳化物析出的研究 |
| 李慧, 夏爽, 周邦新, 彭剑超 |
1) 上海大学材料研究所, 上海 200072
2) 上海大学微结构重点实验室, 上海 200444 |
|
| STUDY OF CARBIDE PRECIPITATION AT GRAIN BOUNDARY IN NICKEL BASE ALLOY 690 |
| LI Hui, XIA Shuang, ZHOU Bangxin, PENG Jianchao |
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Laboratory for Microstructures, Shanghai University, Shanghai 200444 |
引用本文:
李慧 夏爽 周邦新 彭剑超. 镍基690合金中晶界碳化物析出的研究[J]. 金属学报, 2011, 47(7): 853-858.
,
,
,
.
STUDY OF CARBIDE PRECIPITATION AT GRAIN BOUNDARY IN NICKEL BASE ALLOY 690[J]. Acta Metall Sin, 2011, 47(7): 853-858.
| [1] Diercks D R, Shack W J, Muscar J. J Nucl Eng Des, 1999; 194: 19[2] Kai J J, Yu G P, Tsai C H, Liu M N, Yao S C. Metall Trans, 1989; 20A: 2057[3] Stiller K, Nilsson J O, Kjell N. Metall Trans, 1996; 27A: 327[4] Murr L E, Advani A, Shankar S, Atteridge D G. Mater Charact, 1990; 24: 135[5] Povich M J. Corrosion, 1978; 34: 60[6] Li Q, Zhou B X. Acta Metall Sin, 2001; 37: 8(李强, 周邦新. 金属学报, 2001; 37: 8)[7] Lim Y S, Kim J S, Kim H P, Cho H D. J Nucl Mater, 2004; 335: 108[8] Wilson F G. J Iron Steel Inst, 1971; 209: 126[9] Trillo E A, Murr L E. J Mater Sci, 1998; 33: 1263[10] Carolan R A, Faulkner R G. Acta Metall, 1988; 36: 257[11] Li H, Xia S, Zhou B X, Chen W J, Ni J S. Acta Metall Sin, 2009; 45: 195(李慧, 夏爽, 周邦新, 陈文觉, 倪建森. 金属学报, 2009; 45: 195)[12] Trillo E A, Murr L E. Acta Mater, 1999; 47: 235[13] Li H, Xia S, Zhou B X, Chen W J, Hu C L. J Nucl Mater, 2010; 399; 108[14] Hong H U, Rho B S, Nam S W. Mater Sci Eng, 2001; A318: 285[15] Xia S, Zhou B X, Chen W J, Wang W G. Scr Mater, 2006; 54: 2019[16] Xia S, Zhou B X, Chen W J. J Mater Sci, 2008; 43: 2990[17] Xia S, Zhou B X, Chen W J. Metall Mater Trans, 2009; 40A: 3016[18] Palumbo G, Aust K T, Lehockey E M. Scr Mater, 1998; 38: 1685[19] Kronberg M L, Wilson F H. Trans AIME, 1949; 185: 501[20] Randle V, Coleman M, Waterton M. Metall Mater Trans, 2011; 42A: 582[21] Gokon N, Kajihara M. Mater Sci Eng, 2008; A477: 121[22] Lewis M H, Hattersley B. Acta Metall, 1965; 13: 1159[23] Hall E L, Briant C L. Metall Trans, 1984; 15A: 793[24] Downey S, Kalu P N, Han K. Mater Sci Eng, 2008; A480: 96[25] Wolff U E. Trans AIME, 1968; 242: 814[26] Li H, Xia S, Zhou B X, Liu W Q. Mater Charact, revised[27] McLean D. Grain Boundaries in Metals. London: Oxford University Press, 1957: 67 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|