| 等离子弧焊接小孔形状和穿孔过程的数值分析 |
| 霍玉双1,2,武传松1,陈茂爱1 |
1. 山东大学材料液固结构演变与加工教育部重点实验室, 济南 250061
2. 山东建筑大学材料科学与工程学院, 济南 250101 |
|
| NUMERICAL SIMULATION OF KEYHOLE SHAPE AND TRANSFORMATION FROM PARTIAL TO OPEN STATES IN PLASMA ARC WELDING |
| HUO Yushuang 1,2, WU Chuansong 1, CHEN Maoai 1 |
1. Key Lab for Solid–Liquid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061
2. School of Materials Science and Engineering, Shandong Jianzhu University, Jinan 250101 |
引用本文:
霍玉双 武传松 陈茂爱. 等离子弧焊接小孔形状和穿孔过程的数值分析[J]. 金属学报, 2011, 47(6): 706-712.
,
,
.
NUMERICAL SIMULATION OF KEYHOLE SHAPE AND TRANSFORMATION FROM PARTIAL TO OPEN STATES IN PLASMA ARC WELDING[J]. Acta Metall Sin, 2011, 47(6): 706-712.
| [1] Lucas W. In: Japan Welding Society ed., Proc 8th Int Welding Symposium, Osaka, Japan: Japan Welding Society, 2008: 189[2] Zhang Y M, Zhang S B. Weld J, 1999; 75: 53s[3] Wu C S, Jia C B, Chen M A. Weld J, 2010; 89: 225s[4] Dong C L, Wu L, Shao Y C. China Mech Eng, 2000; 11: 577(董春林, 吴林, 邵亦陈. 中国机械工程, 2000; 11: 577)[5] Keanini R G, Rubinsky B. Int J Heat Mass Transfer, 1993; 36: 3283[6] Fan H G, Kovacevic R. J Phys, 1999; 32D: 2902[7] Li L, Hu S S. J Tianjin Univ, 2007; 40: 260(李力, 胡绳荪. 天津大学学报, 2007; 40: 260)[8] Metcalfe J C, Quigley M B C. Weld J, 1975; 54: 99s[9] Wu C S, Hu Q X, Gao J Q. Comp Mater Sci, 2009; 46: 167[10] Hu Q X, Wu C S, Zhang Y M. China Weld, 2007; 16: 55[11] Huo Y S, Wu C S. China Weld, 2009; 18: 12[12] Nehad A K. Int Comm Heat Mass Transfer, 1995; 22: 779[13] Wang X J, Wu C S, Chen M A. Acta Metall Sin, 2010; 46: 984(王小杰, 武传松, 陈茂爱. 金属学报, 2010; 46: 984)[14] Toit M D, Pistorius P C. Weld J, 2007; 86: 222s[15] Sahoo P, DebRoy T, McNallan M J. Metal Trans, 1988; 19B: 483 |
|