金属学报  2011, Vol. 47 Issue (5): 573-577    DOI: 10.3724/SP.J.1037.2010.00715
  论文 本期目录 | 过刊浏览 |
Al-Mg合金中层错和孪晶形变能的第一性原理研究
董明慧, 韩培德, 张彩丽, 杨艳青, 张莉莉, 李洪飞
1) 太原理工大学材料科学与工程学院, 太原 030024
2) 太原理工大学新材料界面科学与工程教育部重点实验室, 太原 030024
FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS
DONG Minghui, HAN Peide, ZHANG Caili, YANG Yanqing, ZHANG Lili, LI Hongfei
1) College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024
2) Key Laboratory of Interface Science and Engineering in Advanced Materials of Taiyuai University of Technology, Ministry of Education, Taiyuan 030024
引用本文:

董明慧 韩培德 张彩丽 杨艳青 张莉莉 李洪飞. Al-Mg合金中层错和孪晶形变能的第一性原理研究[J]. 金属学报, 2011, 47(5): 573-577.
, , , , , . FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS[J]. Acta Metall Sin, 2011, 47(5): 573-577.

全文: PDF(869 KB)  
摘要: 通过基于密度泛函理论(DFT)的第一性原理计算了纯金属 Al和Al-Mg合金在(111)[112]滑移系的层错能和孪晶形变能, 分析了Mg含量、占位对层错能和孪晶形变能的影响. 计算选用了局域密度近似(LDA)和广义梯度近似 (GGA-PW91)2种近似方法, 发现GGA-PW91所获得的层错能与实验结果符合较好. 研究结果表明, 纯Al的层错能高于孪晶形变能, 随着孪晶层厚度的增加孪晶形变能略有提高, 6层呈完全镜面对称孪晶具有的孪晶形变能最低; Mg含量增加可使Al-Mg合金的层错能、变形孪晶形变能明显降低; Mg在Al-Mg合金中占位对结合能和形成热的影响很小, 当Mg处于层错层时略使层错能和孪晶形变能提高.
关键词 : 第一性原理,  层错能,  孪晶,  Al-Mg合金    
Abstract:By using first--principles method based on the density functional theory (DFT), the stacking fault energy (SFE) and deformation twin energy (DTE) for the (111)[112] slip system of pure Al metal and Al-Mg alloys were investigated. The dependence of these SFE and DTE on solid--solution Mg content and its accupation were specifically analyzed. Two major approximations were made in the process of calculation, which were local density approximation (LDA) and generalized gradient approximation (GGA-PW91), respectively. The calculated SFE values by using GGA-PW91 exhibit an excellent agreement with corresponding experimental measurements. For pure Al metal, the calculated SFE values are greater than those of DTE. Moreover, it is found that under the same deformation conditions, the DTE in pure Al and Al-Mg alloys increase monotonically with the increase of deformation twin thickness. In addition, the calculated results shows that 6-layer twin possesses the lowest DTE, which is probably due to its mirror symmetry structure. Also noteworthy, our calculations reveal a noticeable decreased tendency of SFE and DTE with Mg content increasing, while Mg occupying on stacking fault and twin boundary most likely increases SFE and DTE. There are no considerably detected effects of Mg atomic occupancy variation in Al-Mg alloy on its cohesive energy and formation energy.
Key words: first-principles    stacking fault energy    twin    Al-Mg alloy
收稿日期: 2010-10-15     
ZTFLH: 

TG111.2

 
基金资助:

国家自然科学基金项目50874079和51002102, 太原市科技局大学生创新基金项目100115105及山西省教育厅基金项目20080010资助

作者简介: 董明慧, 男, 1984年生, 硕士生
[1] Fanourgakis G S, Pontikis V, Zerah G. Phys Rev, 2003; 67B: 094102

[2] Gang L, Kioussis N, Bulatov V V, Kaxiras E. Phys Rev, 2000; 62B: 3099

[3] Rester M, Motz C, Pippan R. Scr Mater, 2008; 58: 187

[4] Zhu Y T, Narayan J, Hirth J P, Mahajan S, Wu X L, Liao X Z. Acta Mater, 2009; 57: 3763

[5] Zhao Y H, Zhu Y T, Liao X Z, Horita Z, Langdon T G. Appl Phys Lett, 2006; 89: 121906

[6] Yamakov V, Wolf D, Phillpot S R. Acta Mater, 2002; 50: 5005

[7] Hai S, Tadmor E B. Acta Mater, 2003; 51: 117

[8] Chen M W, Ma E, Hemker K J, Sheng H W, Wang Y M, Cheng X M. Science, 2003; 300: 1275

[9] Liu M, Roven H J, Murashkin M, Valiev R Z. Mater Sci Forum, 2008; 579: 147

[10] Zhang J M, Xie L J, Xu K W. Acta Metall Sin, 2007; 43: 182

(张建民, 解丽娟, 徐可为. 金属学报, 2007; 43: 182)

[11] Wu X Z, Wang R, Wang S F, Wei Q Y. Appl Surf Sci, 2010; 256: 6345

[12] Wu J, Wen L, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2011; 13: 120

[13] Heino P, Perondi L, Kaski K, Ristolainen E. Phys Rev, 1999; 60B: 14625

[14] Schulthess T C, Turchi P E A, Gonis A, Nieh T G. Acta Mater, 1998; 46: 2215

[15] Kohn W, Sham L. Phys Rev, 1965; 140: A1133

[16] Milman V, Winkler B, White J A, Pickard C J, Payne M C, Akhmatskaya E V, Nobes R H. Int J Quant Chem, 2000; 77: 895

[17] Segall M D, Lindan P J D, Probert M J, Pickard C J, Hasnip P J, Clark S J, Payne M C. J Phys, 2002; 14: 2717

[18] Mattsson A E, Schultz P A, Desjarlais M P, Mattsson T R, Leung K. Model Simul Mater Sci Eng, 2005; 13: R1

[19] Payne M C, Teter M P, Allan D C, Arials T A, Joannopoulos J D. Rev Mod Phys, 1992; 64: 1045

[20] Perdew J P, Chevary J A, Vosko S H, Jackson K A, Perderson M R, Singh D J, Fiolhais C. Phys Rev, 1992; 46B: 6671

[21] Meyer R, Lewis L J. Phys Rev, 2002; 66B: 052106

[22] Hirth J P, Lothe J. Theory of Dislocations. 2nd Ed., New York: Wiley, 1982: 839

[23] Baskes M I. Phys Rev, 1992; 46B: 2727

[24] Ogata S, Li J, Yip S. Science, 2002; 298: 807

[25] Hartford J, Von Sydow B, Wahnstr¨om G, Lundqvist B I. Phys Rev, 1998; 58B: 2487

[26] Wang Y F, Zhang W B, Wang Z Z, Deng Y H, Yu N, Tang B Y, Zeng X Q, Ding W J. Comput Mater Sci, 2007; 41: 78

[27] Zhang C L, Han P D, Yan X, Wang C, Xia L Q, Xu B S. J Phys, 2009; 42D: 125403

[28] Mola R, Dziado´n A. Arch Foundry Eng, 2008; 8: 127
[1] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[3] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.
[4] 万涛, 程钊, 卢磊. 组元占比对层状纳米孪晶Cu力学行为的影响[J]. 金属学报, 2023, 59(4): 567-576.
[5] 张哲峰, 李克强, 蔡拓, 李鹏, 张振军, 刘睿, 杨金波, 张鹏. 层错能对面心立方金属形变机制与力学性能的影响[J]. 金属学报, 2023, 59(4): 467-477.
[6] 邵晓宏, 彭珍珍, 靳千千, 马秀良. 镁合金LPSO/SFs结构间{101¯2}孪晶交汇机制的原子尺度研究[J]. 金属学报, 2023, 59(4): 556-566.
[7] 李昕, 江河, 姚志浩, 董建新. O原子对高温合金基体Ni、Co和NiCr晶界作用的理论计算分析[J]. 金属学报, 2023, 59(2): 309-318.
[8] 高栋, 周宇, 于泽, 桑宝光. 液氮温度下纯Ti动态塑性变形中的孪晶变体选择[J]. 金属学报, 2022, 58(9): 1141-1149.
[9] 韩冬, 张炎杰, 李小武. 短程有序对高层错能Cu-Mn合金拉-拉疲劳变形行为及损伤机制的影响[J]. 金属学报, 2022, 58(9): 1208-1220.
[10] 任师浩, 刘永利, 孟凡顺, 祁阳. 应变工程中Bi(111)薄膜的半导体-半金属转变及其机理[J]. 金属学报, 2022, 58(7): 911-920.
[11] 李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究[J]. 金属学报, 2022, 58(2): 241-249.
[12] 卢磊, 赵怀智. 异质纳米结构金属强化韧化机理研究进展[J]. 金属学报, 2022, 58(11): 1360-1370.
[13] 王硕, 王俊升. Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究[J]. 金属学报, 2022, 58(10): 1325-1333.
[14] 潘庆松, 崔方, 陶乃镕, 卢磊. 纳米孪晶强化304奥氏体不锈钢的应变控制疲劳行为[J]. 金属学报, 2022, 58(1): 45-53.
[15] 杨志昆, 王浩, 张义文, 胡本芙. Ta含量对镍基粉末高温合金高温蠕变变形行为和性能的影响[J]. 金属学报, 2021, 57(8): 1027-1038.