| NiCoCrAlYSiB+AlSiY梯度涂层恒温氧化行为 |
| 王维新1, 2), 姜肃猛1), 卫广智2), 马军1), 宫骏1), 孙超1) |
1) 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
2) 贵州大学材料与冶金学院, 贵阳 550003 |
|
| ISOTHERMAL OXIDATION BEHAVIOR OF A NiCoCrAlYSiB+AlSiY GRADIENT COATING |
| WANG Weixin1, 2), JIANG Sumeng1), WEI Guangzhi2), MA Jun1), GONG Jun1), SUN Chao1) |
1) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) The Materials and Metallurgical College, Guizhou University, Guiyang 550003 |
引用本文:
王维新 姜肃猛 卫广智 马军 宫骏 孙超. NiCoCrAlYSiB+AlSiY梯度涂层恒温氧化行为[J]. 金属学报, 2011, 47(5): 578-586.
,
,
,
,
,
.
ISOTHERMAL OXIDATION BEHAVIOR OF A NiCoCrAlYSiB+AlSiY GRADIENT COATING[J]. Acta Metall Sin, 2011, 47(5): 578-586.
| [1] Brandl W, Toma D. Surf Coat Technol, 1997; 94: 21[2] Czech N, Schmitz F. Mater Manuf Processes, 1995; 10: 1021[3] Goward G W. Surf Coat Technol, 1998; 68: 73[4] Padture N P, Gell M. Jordan E H. Science, 2002; 296: 280[5] Choquet P, Indrigo C, Mevrel R. Mater Sci Eng, 1987; A88: 97[6] Tawancy H M, Abbas N M, Bennett A. Surf Coat Technol, 1994; 68: 10[7] Brandl W, Grabke H J, Toma D, Kruger J. Surf Coat Technol, 1996; 87: 41[8] Jiang S M, Li H Q,Ma J, Xu C Z, Gong J, Sun C. Corros Sci, 2010; 52: 7[9] Tang F, Ajdelsztajn L, Schoenung J M. Ozid Met, 2004; 61: 219[10] Eskner M. PhD Thesis, Royal institute of technology, Stockholm, 2004[11] Nicholls J R, Simms N J, Evans H E. Surf Coat Technol, 2002; 149: 236[12] Tien J K, Pettit F S. Metall Trans, 1972; 3: 1587[13] Clemens D, Nickel H. J Anal Chem, 1996; 355: 703[14] Wang Q M, Wu Y N, Ke P L, Gong J, Sun C, Wen L S. Surf Coat Technol, 2004; 186: 389[15] Guo M H, Wang Q M, Gong J, Sun C, Wen L S. Surf Coat Technol, 2006; 201: 1302[16] El–Aiat M M, Kroger F A. J Am Ceram Soc, 1982; 65: 280[17] Nijdam T J, Sloof W G. Surf Coat Technol, 2006; 201: 3894[18] Li T F. High Temperature Oxidation And Corrosion of Mater. BeiJing: Chemical Industry Press, 2003: 104(李铁藩. 金属的高温氧化和热腐蚀. 北京: 化学工业出版社, 2003: 104)[19] Sun C, Wang Q M, Tang Y J, Guan Q F, Gong J, Wen L S. Acta Metall Sin, 2005; 41: 1167(孙 超, 王启民, 唐永吉, 关庆丰, 宫 俊, 闻立时. 金属学报, 2005; 41: 1167)[20] Brumm M W, Grabke H J. Corros Sci, 1992; 33: 1677[21] Rusovic N, War]imont H. Phys Status Solidi, 1977; 44A: 609[22] Li M S. High Temperature Corrosion of Mater. Beijing: Metallurgical Industry Press, 2001: 420(李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 420)[23] Doychak J. PhD Thesis. CaseWestern Reserve University, Ohio, 1986 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|