| Al-Mg合金中层错和孪晶形变能的第一性原理研究 |
| 董明慧, 韩培德, 张彩丽, 杨艳青, 张莉莉, 李洪飞 |
1) 太原理工大学材料科学与工程学院, 太原 030024
2) 太原理工大学新材料界面科学与工程教育部重点实验室, 太原 030024 |
|
| FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS |
| DONG Minghui, HAN Peide, ZHANG Caili, YANG Yanqing, ZHANG Lili, LI Hongfei |
1) College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024
2) Key Laboratory of Interface Science and Engineering in Advanced Materials of Taiyuai University of Technology, Ministry of Education, Taiyuan 030024 |
引用本文:
董明慧 韩培德 张彩丽 杨艳青 张莉莉 李洪飞. Al-Mg合金中层错和孪晶形变能的第一性原理研究[J]. 金属学报, 2011, 47(5): 573-577.
,
,
,
,
,
.
FIRST-PRINCIPLES STUDY OF STACKING FAULT ENERGY AND DEFORMATION TWIN\par ENERGY IN Al-Mg ALLOYS[J]. Acta Metall Sin, 2011, 47(5): 573-577.
| [1] Fanourgakis G S, Pontikis V, Zerah G. Phys Rev, 2003; 67B: 094102[2] Gang L, Kioussis N, Bulatov V V, Kaxiras E. Phys Rev, 2000; 62B: 3099[3] Rester M, Motz C, Pippan R. Scr Mater, 2008; 58: 187[4] Zhu Y T, Narayan J, Hirth J P, Mahajan S, Wu X L, Liao X Z. Acta Mater, 2009; 57: 3763[5] Zhao Y H, Zhu Y T, Liao X Z, Horita Z, Langdon T G. Appl Phys Lett, 2006; 89: 121906[6] Yamakov V, Wolf D, Phillpot S R. Acta Mater, 2002; 50: 5005[7] Hai S, Tadmor E B. Acta Mater, 2003; 51: 117[8] Chen M W, Ma E, Hemker K J, Sheng H W, Wang Y M, Cheng X M. Science, 2003; 300: 1275[9] Liu M, Roven H J, Murashkin M, Valiev R Z. Mater Sci Forum, 2008; 579: 147[10] Zhang J M, Xie L J, Xu K W. Acta Metall Sin, 2007; 43: 182(张建民, 解丽娟, 徐可为. 金属学报, 2007; 43: 182)[11] Wu X Z, Wang R, Wang S F, Wei Q Y. Appl Surf Sci, 2010; 256: 6345[12] Wu J, Wen L, Tang B Y, Peng L M, Ding W J. Solid State Sci, 2011; 13: 120[13] Heino P, Perondi L, Kaski K, Ristolainen E. Phys Rev, 1999; 60B: 14625[14] Schulthess T C, Turchi P E A, Gonis A, Nieh T G. Acta Mater, 1998; 46: 2215[15] Kohn W, Sham L. Phys Rev, 1965; 140: A1133[16] Milman V, Winkler B, White J A, Pickard C J, Payne M C, Akhmatskaya E V, Nobes R H. Int J Quant Chem, 2000; 77: 895[17] Segall M D, Lindan P J D, Probert M J, Pickard C J, Hasnip P J, Clark S J, Payne M C. J Phys, 2002; 14: 2717[18] Mattsson A E, Schultz P A, Desjarlais M P, Mattsson T R, Leung K. Model Simul Mater Sci Eng, 2005; 13: R1[19] Payne M C, Teter M P, Allan D C, Arials T A, Joannopoulos J D. Rev Mod Phys, 1992; 64: 1045[20] Perdew J P, Chevary J A, Vosko S H, Jackson K A, Perderson M R, Singh D J, Fiolhais C. Phys Rev, 1992; 46B: 6671[21] Meyer R, Lewis L J. Phys Rev, 2002; 66B: 052106[22] Hirth J P, Lothe J. Theory of Dislocations. 2nd Ed., New York: Wiley, 1982: 839[23] Baskes M I. Phys Rev, 1992; 46B: 2727[24] Ogata S, Li J, Yip S. Science, 2002; 298: 807[25] Hartford J, Von Sydow B, Wahnstr¨om G, Lundqvist B I. Phys Rev, 1998; 58B: 2487[26] Wang Y F, Zhang W B, Wang Z Z, Deng Y H, Yu N, Tang B Y, Zeng X Q, Ding W J. Comput Mater Sci, 2007; 41: 78[27] Zhang C L, Han P D, Yan X, Wang C, Xia L Q, Xu B S. J Phys, 2009; 42D: 125403[28] Mola R, Dziado´n A. Arch Foundry Eng, 2008; 8: 127 |
|