| 动态压缩LY12铝合金微结构的XRD线形分析 |
| 樊志剑1), 宋振飞2), 肖大武2), 陈波1) |
1) 中国工程物理研究院核物理与化学研究所, 绵阳 621900
2) 中国工程物理研究院流体物理研究所, 绵阳 621900 |
|
| XRD LINE PROFILE ANALYSIS OF LY12 ALUMINUM ALLOY UNDER DYNAMIC COMPRESSIVE EXPERIMENT |
| FAN Zhijian1), SONG Zhenfei2), XIAO Dawu2), CHEN Bo1) |
1) Institute of Nuclear Physics and Chemistry, China Academy of Engineering Physics, Mianyang 621900
2) Institute of Fluid Physics, China Academy of Engineering Physics, Mianyang 621900 |
引用本文:
樊志剑 宋振飞 肖大武 陈波. 动态压缩LY12铝合金微结构的XRD线形分析[J]. 金属学报, 2011, 47(5): 559-565.
,
,
,
.
XRD LINE PROFILE ANALYSIS OF LY12 ALUMINUM ALLOY UNDER DYNAMIC COMPRESSIVE EXPERIMENT[J]. Acta Metall Sin, 2011, 47(5): 559-565.
| [1] Wilkens M. Krist Technol, 1976; 11: 1159[2] Langford J I, Lou¨er D, Scardi P. J Appl Cryst, 2000; 33: 964[3] Scardi P, Leoni M. Acta Cryst, 2001; 57A: 604[4] Ung´ar T, Gubicza J, Rib´arik G, Borb´ely A. J Appl Cryst, 2001; 34: 298[5] Williamson G K, Hall W H. Acta Metall, 1953; 1: 22[6] Klug H P, Alexander L E. X–Ray Diffraction Procedures for Polycrystalline and Amorphous Materials. New York: John Wiley, 1974: 634[7] Balzar D, Popovi´c S. J Appl Cryst, 1996; 29: 16[8] Warren B E, Averbach B L. J Appl Phys, 1950; 21: 595[9] Warren B E. X–Ray Diffraction. Reading: Addison–Wesley, 1969: 264[10] Stephens P W. J Appl Cryst, 1999; 32: 281[11] Popa N C. J Appl Cryst, 1998; 31: 176[12] Krivoglaz M A, Ryaboshapka K P. Phys Met Metallogr, 1963; 15: 18[13] Krivoglaz M A, Martynenko O V, Ryaboshapka K P. Phys Met Metallogr, 1983; 55: 318[14] Krivoglaz M A. X–Ray and Neutron Diffraction in Nonideal Crystals. New York: Springer–Verlag, 1996: 357[15] Wilkens M. Phys Status Solidi, 1970; 2A: 359[16] Wilkens M. In: Simmons J A, De Wit R, Bullough R, eds., Fundamental Aspects of Dislocation Theory National Bureau of Standards Special Publication 317(II).Washington DC: National Bureau of Standards, 1970: 1195[17] Wilkens M. Phys Status Solidi, 1987; 104A: K1[18] Klimanek P, Kuzel R. J Appl Cryst, 1988; 21: 59[19] Kuzel R, Klimanek P. J Appl Cryst, 1988; 21: 363[20] Ung´ar T, Tichy G. Phys Status Solidi, 1999; 171A: 425[21] Gubicza J, Kassem M, Rib´arik G, Ung´ar T. Mater Sci Eng, 2004; A372: 115[22] F´atay D, Bastarash E, Nyilas K, Dobatkin S, Gubicza J, Ung´ar T. Z Metall, 2003; 94: 1[23] Ung´ar T, Borb´ely A. Appl Phys Lett, 1996; 69: 3173[24] De Keijser T H, Langford J I, Mittemeijer E J, Vogels A B P. J Appl Cryst, 1982; 15: 308[25] Thompson P, Cox D E, Hastings J B. J Appl Cryst, 1987; 20: 79[26] Dieter G E. Mechanical Metallurgy. New York: McGraw–Hill, 1988: 58[27] Ung´ar T. Mater Sci Eng, 2001; A309–310: 14[28] Ung´ar T, Tichy G, Gubicza J, Hellming R J. Powder Diffr, 2005; 20: 366[29] Ung´ar T, Gubicza J, Han´ak P, Alexandrov I. Mater Sci Eng, 2001; A319–321: 274[30] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 5: 103[31] Estrin Y, Molinari, Toth L S, Brechet Y. Acta Mater, 1998; 46: 5509[32] Arzt E, Ashby M F, Verrall R A. Acta Metall, 1983; 31: 1977[33] Brammer J A, Percival C M. Exp Mech, 1970; 10(6): 245 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|