Please wait a minute...
金属学报  2011, Vol. 47 Issue (3): 344-348    DOI: 10.3724/SP.J.1037.2010.00566
  论文 本期目录 | 过刊浏览 |
MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03)化合物的磁热效应
王冬梅,松林,王耀辉,张伟,毕力格,特古斯
内蒙古师范大学内蒙古自治区功能材料物理与化学重点实验室, 呼和浩特 010022
MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS
WANG Dongmei, SONG Lin, WANG Yaohui, ZHANG Wei, Bilige, Tegus O
Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University,
Hohhot 010022
引用本文:

王冬梅 松林 王耀辉 张伟 毕力格 特古斯. MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03)化合物的磁热效应[J]. 金属学报, 2011, 47(3): 344-348.
, , , , . MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. Acta Metall Sin, 2011, 47(3): 344-348.

全文: PDF(877 KB)  
摘要: 对MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03, 原子分数)化合物的结构和磁热效应(MCE)进行了研究. XRD分析结果表明:MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03)的主相均为Fe2P型六角结构, 空间群为P62m. 随着B含量的增加晶格常数a增大c减小,晶胞体积基本保持不变. 磁性测量表明: 随着B含量由0增加到0.03时, Curie温度(TC)从300 K升到347 K, 热滞分别为20, 17, 11和6 K. 0-1.5 T外磁场下最大磁熵变Δ SM分别为14.83, 11.41, 11.26 和11.8 J/(kg?K).
关键词 : 磁热效应,  热滞,  Curie温度,  相变    
Abstract:Structural and magnetocaloric properties of the MnFeP0.63Ge0.12Si0.25Bx (x=0,0.01, 0.02, 0.03, atomic fraction) compounds have been inestigated. XRD result shows that the MnFeP0.63Ge0.12Si0.25Bx  (x=0, 0.01, 0.02, 0.03) compounds mainly consist of the Fe2P–typhxagonal structure phase with space group P¯62m. It is fond that the lattice paraeter a increases and the lattice parameter c slighly decreases with increasing x, and the unit celvolume does not change. The agnetic measurements show that the Curie temperature increases from 300 K to 347 K, and thermal hysteresis are 20, 17, 11 and 6 K for x= 0 to 0.03. The aximm values of the magnetic entropy chage are 11.1, 11.26 and 11.8 J/(kg·K), respectively, or 0—1.5 T fields.
Key words: magnetocaloric effect    thermal hysteresis    Curie temperature    phase transition
收稿日期: 2010-10-25     
基金资助:

国家自然科学基金项目50961010, 内蒙古自然科学基金项目20080404ZD09和内蒙古师范大学研究生科研创新基金项目CXJJS10034资助

作者简介: 王冬梅, 女, 蒙古族, 1986年生, 硕士生
[1] Tegus O, Br¨uck E, Buschow K H J, de Boer F R. Nature,2002; 415: 150

[2] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903

[3] DagulaW, Tegus O, Li XW, Song L, Br¨uck E, Cam Thanh D T, de Boer F R, Buschow K H J. J Appl Phys, 2006; 99: 08Q105

[4] Br¨uck E, Tegus O, Zhang L, Li XW, de Boer F R, Buschow K H J. J Alloys Compds, 2004; 383: 32

[5] Br¨uck E, Tegus O, Li X W, de Boer F R, Buschow K H J. Physica, 2003; 327: 431

[6] Tegus O, Fuquan B, Dagula W, Zhang L, Br¨uck E, Si P Z, de Boer F R, Buschow K H J. J Alloys Compds, 2005; 396: 6

[7] Cam Thanh D T, Br¨uck E, Tegus O, Klaasse J C P, Gortenmulder T J, Buschow K H J. J Appl Phys, 2006; 99: 08Q107

[8] Br¨uck E, Ilynb M, Tishin A M, Tegus O. J Magn Magn Mater, 2005; 290–291: 8

[9] Tegus O, Br¨uck E, Dagula W, Li X W, Zhang L, Buschow K H J, de Boer F R. J Appl Phys, 2003; 93: 7655

[10] Tegus O, Br¨uck E, Li X W, Zhang L, DagulaW, de Boer F R, Buschow K H J. J Magn Magn Mater, 2004; 272–276: 2389

[11] Zhang L, Moze O, Prokes K, Tegus O, Br¨uck E. J Magn Magn Mater, 2005; 290–291: 679

[12] Ou Z Q, Wang G F, Song L, Tegus O, Br¨uck E, Buschow K J. J Phys: Condens Matter, 2006; 18: 11577

[13] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903

[14] Wang G F. Master Desertation, Inner Mongolia Normal University, hohhot, 2007

(王高峰. 内蒙古师范大学硕士学位论文, 呼和浩特, 2007)

[15] Zhang L. PhD Thesis, University of Amsterdam, 2005

[16] Hang J H, Song L, Jin P Y, Wang G F, Liu J R, Yan H W, Zhang J X. J Funct Mater, 2006; 37: 1888

(黄焦宏, 松林, 金培育, 王高峰, 刘金荣, 闫宏伟, 张久兴. 功能材料, 2006; 37: 1888)

[17] Li F A, Song L, Bao L H, Ha S C L, Tegus O, Hang J H. Acta Metall Sin, 2008; 44: 371

(李福安, 松林, 包黎红, 哈斯朝鲁, 特古斯, 黄焦宏. 金属学报, 2008; 44: 371)

[18] Li F A, Song L, Wang G F, Xie G Q, Zheng L, Hang J H, Tegus O. J Funct Mater, 2010; 41: 515

(李福安, 松林, 王高峰, 谢国秋, 郑立, 黄焦宏, 特古斯. 功能材料, 2010; 41: 515)

[19] Li F A, Song L, Zheng L, Hang J H, Tegus O. Met Funct Mater, 2010; 17: 22

(李福安, 松林, 郑立, 黄焦宏, 特古斯. 金属功能材料, 2010; 17: 22)

[20] Beckman O, Lundgren L, Buschow K H J. Handbook of Magnetic Materials. Amsterdam: Elsevier Science Publication, 1991: 186

[21] Gschneidner Jr K A, Pecharsky V K. Annu Rev Mater Sci, 2000; 30: 387
[1] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[3] 王重阳, 韩世伟, 谢峰, 胡龙, 邓德安. 固态相变和软化效应对超高强钢焊接残余应力的影响[J]. 金属学报, 2023, 59(12): 1613-1623.
[4] 张开元, 董文超, 赵栋, 李世键, 陆善平. 固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-Nb原位复合材料的准线性超弹性变形[J]. 金属学报, 2023, 59(11): 1419-1427.
[6] 李小兵, 潜坤, 舒磊, 张孟殊, 张金虎, 陈波, 刘奎. W含量对Ti-42Al-5Mn-xW合金相转变行为的影响[J]. 金属学报, 2023, 59(10): 1401-1410.
[7] 李赛, 杨泽南, 张弛, 杨志刚. 珠光体-奥氏体相变中扩散通道的相场法研究[J]. 金属学报, 2023, 59(10): 1376-1388.
[8] 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中. 3Mn-0.2C中锰钢形变诱导铁素体动态相变机理[J]. 金属学报, 2022, 58(5): 649-659.
[9] 李伟, 贾兴祺, 金学军. 高强韧QPT工艺的先进钢组织调控和强韧化研究进展[J]. 金属学报, 2022, 58(4): 444-456.
[10] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.
[11] 杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥. 成分对真空脱锰法相变控制高硅电工钢{100}织构的影响[J]. 金属学报, 2022, 58(10): 1261-1270.
[12] 胡标, 张华清, 张金, 杨明军, 杜勇, 赵冬冬. 界面热力学与晶界相图的研究进展[J]. 金属学报, 2021, 57(9): 1199-1214.
[13] 李学达, 李春雨, 曹宁, 林学强, 孙建波. 高强管线钢焊接临界再热粗晶区中逆转奥氏体的逆相变晶体学[J]. 金属学报, 2021, 57(8): 967-976.
[14] 冯苗苗, 张红伟, 邵景霞, 李铁, 雷洪, 王强. 耦合热力学相变路径预测Fe-C包晶合金宏观偏析[J]. 金属学报, 2021, 57(8): 1057-1072.
[15] 王金亮, 王晨充, 黄明浩, 胡军, 徐伟. 低应变预变形对变温马氏体相变行为的影响规律及作用机制[J]. 金属学报, 2021, 57(5): 575-585.