| MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03)化合物的磁热效应 |
| 王冬梅,松林,王耀辉,张伟,毕力格,特古斯 |
| 内蒙古师范大学内蒙古自治区功能材料物理与化学重点实验室, 呼和浩特 010022 |
|
| MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS |
| WANG Dongmei, SONG Lin, WANG Yaohui, ZHANG Wei, Bilige, Tegus O |
Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University,
Hohhot 010022 |
引用本文:
王冬梅 松林 王耀辉 张伟 毕力格 特古斯. MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03)化合物的磁热效应[J]. 金属学报, 2011, 47(3): 344-348.
,
,
,
,
.
MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. Acta Metall Sin, 2011, 47(3): 344-348.
| [1] Tegus O, Br¨uck E, Buschow K H J, de Boer F R. Nature,2002; 415: 150[2] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903[3] DagulaW, Tegus O, Li XW, Song L, Br¨uck E, Cam Thanh D T, de Boer F R, Buschow K H J. J Appl Phys, 2006; 99: 08Q105[4] Br¨uck E, Tegus O, Zhang L, Li XW, de Boer F R, Buschow K H J. J Alloys Compds, 2004; 383: 32[5] Br¨uck E, Tegus O, Li X W, de Boer F R, Buschow K H J. Physica, 2003; 327: 431[6] Tegus O, Fuquan B, Dagula W, Zhang L, Br¨uck E, Si P Z, de Boer F R, Buschow K H J. J Alloys Compds, 2005; 396: 6[7] Cam Thanh D T, Br¨uck E, Tegus O, Klaasse J C P, Gortenmulder T J, Buschow K H J. J Appl Phys, 2006; 99: 08Q107[8] Br¨uck E, Ilynb M, Tishin A M, Tegus O. J Magn Magn Mater, 2005; 290–291: 8[9] Tegus O, Br¨uck E, Dagula W, Li X W, Zhang L, Buschow K H J, de Boer F R. J Appl Phys, 2003; 93: 7655[10] Tegus O, Br¨uck E, Li X W, Zhang L, DagulaW, de Boer F R, Buschow K H J. J Magn Magn Mater, 2004; 272–276: 2389[11] Zhang L, Moze O, Prokes K, Tegus O, Br¨uck E. J Magn Magn Mater, 2005; 290–291: 679[12] Ou Z Q, Wang G F, Song L, Tegus O, Br¨uck E, Buschow K J. J Phys: Condens Matter, 2006; 18: 11577[13] Yan A, M¨uller K H, Schultz L, Gutfleisch O. J Appl Phys, 2006; 99: 08K903[14] Wang G F. Master Desertation, Inner Mongolia Normal University, hohhot, 2007(王高峰. 内蒙古师范大学硕士学位论文, 呼和浩特, 2007)[15] Zhang L. PhD Thesis, University of Amsterdam, 2005[16] Hang J H, Song L, Jin P Y, Wang G F, Liu J R, Yan H W, Zhang J X. J Funct Mater, 2006; 37: 1888(黄焦宏, 松林, 金培育, 王高峰, 刘金荣, 闫宏伟, 张久兴. 功能材料, 2006; 37: 1888)[17] Li F A, Song L, Bao L H, Ha S C L, Tegus O, Hang J H. Acta Metall Sin, 2008; 44: 371(李福安, 松林, 包黎红, 哈斯朝鲁, 特古斯, 黄焦宏. 金属学报, 2008; 44: 371)[18] Li F A, Song L, Wang G F, Xie G Q, Zheng L, Hang J H, Tegus O. J Funct Mater, 2010; 41: 515(李福安, 松林, 王高峰, 谢国秋, 郑立, 黄焦宏, 特古斯. 功能材料, 2010; 41: 515)[19] Li F A, Song L, Zheng L, Hang J H, Tegus O. Met Funct Mater, 2010; 17: 22(李福安, 松林, 郑立, 黄焦宏, 特古斯. 金属功能材料, 2010; 17: 22)[20] Beckman O, Lundgren L, Buschow K H J. Handbook of Magnetic Materials. Amsterdam: Elsevier Science Publication, 1991: 186[21] Gschneidner Jr K A, Pecharsky V K. Annu Rev Mater Sci, 2000; 30: 387 |
|