| [011]取向镍基单晶合金在拉伸蠕变期间的组织演化与有限元分析 |
| 张姝1,2), 田素贵1), 于慧臣3), 苏勇1), 于兴福1), 于莉丽1) |
1) 沈阳工业大学材料科学与工程学院, 沈阳 110870
2) 沈阳化工大学机械工程学院, 沈阳 110142
3) 北京航空材料研究院, 北京 100095 |
|
| MICROSTRUCTURE EVOLUTION AND FEM ANALYSIS OF [011] ORIENTED SINGLE CRYSTAL OF A Ni-BASED SUPERALLOY DURING TENSILE CREEP |
| ZHANG Shu1,2), TIAN Sugui1), YU Huichen3), SU Yong1), YU Xingfu1), YU Lili1) |
1) School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
2) School of Machinary Engineering, Shenyang University of Chemical Technology, Shenyang 110142
3) Beijing Institute of aeronautical Material, Beijing 100095 |
引用本文:
张姝 田素贵 于慧臣 苏勇 于兴福 于莉丽. [011]取向镍基单晶合金在拉伸蠕变期间的组织演化与有限元分析[J]. 金属学报, 2011, 47(1): 61-68.
,
,
,
,
,
.
MICROSTRUCTURE EVOLUTION AND FEM ANALYSIS OF [011] ORIENTED SINGLE CRYSTAL OF A Ni-BASED SUPERALLOY DURING TENSILE CREEP[J]. Acta Metall Sin, 2011, 47(1): 61-68.
| [1] Feng H, Biermann H, Mughrabi H. Metall Mater Trans, 2000; 31A: 585[2] Yu X F, Tian S G, Du H Q, Yu H C, Wang M G, Shang L J, Cui S S. Mater Sci Eng, 2009; A506: 80[3] Tien J K, Copley S M. Metall Trans, 1971; 2: 543[4] Buffiere J Y, Ignat M. Acta Metall Mater, 1995; 43: 1791[5] Pollock T M, Argon A S. Acta Metall Mater, 1994; 42: 1859[6] Kuhn H A, Biermann H, Ungar T. Acta Metall Mater, 1991; 39: 2783[7] Biermann H, Strehler M, Mughrabi H. Metall Mater Trans, 1996; 27A: 1003[8] Tian S G, Zhang J H, Yang H C, Xu Y B, Hu Z Q. J Aeronautic Mater, 2000; 20: 1(田素贵, 张静华, 杨洪才, 徐永波, 胡壮麒. 航空材料学报, 2000; 20: 1)[9] Tian S G, Chen C R, Yang H C, Hu Z Q. Acta Metall Sin, 2000; 36: 465(田素贵, 陈昌荣, 杨洪才, 胡壮麒. 金属学报, 2000; 36: 465)[10] Tian S G, Wang M G, Yu H C, Yu X F, Li T, Qian B J. Mater Sci Eng, A527: 4458[11] Sha Y H, Chen C R, Zhang J H, Xu Y B, Hu Z Q. Acta Metall Sin, 1999; 36: 254(沙玉辉, 陈昌荣, 张静华, 徐永波, 胡壮麒. 金属学报, 1999; 36: 254)[12] Zhou L, Yu X L. Trans Shenyang Ligong Univ, 2008; 27: 1(周丽, 于晓琳. 沈阳理工大学学报, 2008; 27: 1)[13] Nabarro F R N. Metall Mater Trans, 1996; 27A: 513[14] Tian S G, Zhang J H, Yang H C, Hu Z Q. Mater Sci Technol, 2000; 16, 451[15] Shui L, Yang Y H, Yu J J. Mater Mech Eng, 2009; 33: 6(水丽, 杨彦红, 于金江. 机械工程材料, 2009; 33: 6)[16] Shui L, Jin T, Tian S, Hu Z Q. Rare Met Mater Eng, 2009; 38: 826(水丽, 金涛, 田素贵, 胡壮麒. 稀有金属材料与工程, 2009; 38: 826) |
|