| Al-Cu-Mg-Ag耐热铝合金高温蠕变行为 |
| 刘晓艳1), 潘清林1, 2), 陆智伦1), 曹素芳1), 何运斌1), 李文斌1) |
1) 中南大学材料科学与工程学院, 长沙 410083
2) 中南大学有色金属材料科学与工程教育部重点实验室, 长沙 410083 |
|
| CREEP BEHAVIOR OF Al-Cu-Mg-Ag HEAT-RESISTANT ALLOY AT ELEVATED TEMPERATURE |
| LIU Xiaoyan1), PAN Qinglin1, 2), LU Zhilun1), CAO Sufang1), HE Yunbin1), LI Wenbin1) |
1) School of Materials Science and Engineering, Central South University, Changsha 410083
2) The Key Laboratory of Nonferrous Materials Science and Engineering of Ministry of Education, Central South University, Changsha 410083 |
引用本文:
刘晓艳 潘清林 陆智伦 曹素芳 何运斌 李文斌. Al-Cu-Mg-Ag耐热铝合金高温蠕变行为[J]. 金属学报, 2011, 47(1): 53-60.
,
,
,
,
,
.
CREEP BEHAVIOR OF Al-Cu-Mg-Ag HEAT-RESISTANT ALLOY AT ELEVATED TEMPERATURE[J]. Acta Metall Sin, 2011, 47(1): 53-60.
| [1] Sukumaran K, Ravikumar K K, Pillai S G K, Rajan T P D, Ravi M, Pillai R M, Pai B C. Mater Sci Eng, 2008; A490: 235[2] Naga R P, Srinivasa R K, Reddy G M, Kamaraj M, Prasad R K. Mater Sci Eng, 2007; A464: 192[3] Wang J, Yi D, Su X, Yin F. Mater Charact, 2008; 59: 965[4] Yu K, Li W, Li S, Zhao J. Mater Sci Eng, 2004; A368: 88[5] Chang C H, Lee S L, Lin J C, Yeh M S, Jeng R R. Mater Chem Phys, 2005; 91: 454[6] Xiao D H, Wang J N, Ding D Y, Chen S P. J Alloys Compd, 2002; 343: 77[7] Bakavos D, Prangnell P B, Bes B, Eberl F. Mater Sci Eng, 2008; A491: 214[8] Somi R A. Mater Des, 2008; 29: 763[9] Lumley R N, Morton A J, Polmear I J. Acta Mater, 2002; 50: 3597[10] Yan J L, Sun Y S, Xue F, Tao W J. Acta Metall Sin, 2008; 44: 1354(晏井利, 孙扬善, 薛烽, 陶卫建. 金属学报, 2008; 44: 1354)[11] Spigarelli S, Evangelista E, Cucchieri S. Mater Sci Eng, 2004; A387–389: 702[12] Qi Y H, Guo J T, Cui C Y. Acta Metall Sin, 2001; 37: 957(齐义辉, 郭建亭, 崔传勇. 金属学报, 2001; 37: 957)[13] Kermanidis A T, Zervaki A D, Haidemenopoulos G N, Pantelakis Sp G. Mater Des, 2010; 31: 42[14] Das G, Das M, Ghosh S, Dubey P, Ray A K. Mater Sci Eng, 2010; A527: 1590[15] Xia Q K, Liu Z Y, Li Y T. Trans Nonferrous Met Soc China, 2008; 18: 789[16] Seeger A T. Naturforschung, 1956; 9: 758[17] Sha G Y, Han E H, Yu T, Xu Y B, Liu L, Gao G Z. Acta Metall Sin, 2003; 39: 1025(沙桂英, 韩恩厚, 于 涛, 徐永波, 刘 路, 高国忠. 金属学报, 2003; 39: 1025)[18] Li B Q, Wawner F E. Acta Mater, 1998; 46: 5483[19] Mukherjee A K, Bird J E, Dorn J E. Trans ASM, 1969; 62: 155 |
|