| 铝合金挤压铸造过程微观孔洞形成的建模与仿真 |
| 韩志强1), 李金玺1), 杨文1), 赵海东2), 柳百成1,3) |
1) 清华大学机械工程系, 先进成形制造教育部重点实验室, 北京 100084
2) 华南理工大学机械与汽车工程学院, 广州 510640
3) 清华大学汽车工程系, 汽车安全与节能国家重点实验室, 北京 100084 |
|
| MODELING AND SIMULATION ON MICROPOROSITY FORMED DURING SQUEEZE CASTING OF ALUMINUM ALLOY |
| HAN Zhiqiang1), LI Jinxi1), YANG Wen1), ZHAO Haidong2), LIU Baicheng1,3) |
1) Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2) School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640
3) State Key Laboratory of Automotive Safety and Energy, Department of Automotive Engineering, Tsinghua University, Beijing 100084 |
引用本文:
韩志强 李金玺 杨文 赵海东 柳百成. 铝合金挤压铸造过程微观孔洞形成的建模与仿真[J]. 金属学报, 2011, 47(1): 7-16.
,
,
.
MODELING AND SIMULATION ON MICROPOROSITY FORMED DURING SQUEEZE CASTING OF ALUMINUM ALLOY[J]. Acta Metall Sin, 2011, 47(1): 7-16.
| [1] Ghomashchi M R, Vikhrov A. J Mater Process Technol, 2000; 101: 1[2] Qi P X. Spec Cast Nonferrous Alloys, 1998; 18(4): 32(齐丕骧. 特种铸造及有色合金, 1998; 18(4): 32)[3] Luo S J, Chen B G, Qi P X. Liquid Forging and Squeeze Casting Technology. Beijing: Chemical Industry Press, 2007: 1(罗守靖, 陈炳光, 齐丕骧. 液态模锻与挤压铸造技术. 北京: 化学工业出版社, 2007: 1)[4] Major J F. AFS Trans, 1998; 105: 901[5] Samuel A M, Samuel F H. Metall Mater Trans, 1995; 26A: 2359[6] Lee C D. Mater Sci Eng, 2007; A464: 249[7] Lee P D, Chirazi A, See D. J Light Met, 2001; (1): 15[8] Stefanescu D M. Int J Cast Met Res, 2005; 18(3): 129[9] Gui Z L, Dai T, Zhu M F. Spec Cast Nonferrous Alloys, 2007; 27: 766(桂仲林, 戴挺, 朱鸣芳. 特种铸造及有色合金, 2007; 27: 766)[10] Kubo K, Pehlke R D. Metall Trans, 1985; 16B: 359[11] Poirier D R, Yeum K, Maples A L. Metall Trans, 1987; 18A: 1979[12] Shivkumar S, Apelian D, Zou J. AFS Trans, 1990; 98: 897[13] Sabau A S, Viswanathan S. Metall Mater Trans, 2002; 33B: 243[14] Pequet C H, Gremaud M, Rappaz M. Metall Mater Trans, 2002; 33A: 2095[15] Zhao H D, Wu C Z, Li Y Y, Ohnaka I. Acta Metall Sin, 2008; 44: 1340(赵海东, 吴朝忠, 李元元, 大中逸雄. 金属学报, 2008; 44: 1340)[16] Atwood R C, Sridhar S, Zhang W, Lee P D. Acta Mater, 2000; 48: 405[17] Lee P D, Chirazi A, Atwood R C, Wang W. Mater Sci Eng, 2004; A365: 57[18] Wang J S, Lee P D. Int J Cast Met Res, 2007; 20(3): 151[19] Backer G, Wang Q G. Metall Mater Trans, 2007; 38B: 533[20] Carlson K D, Lin Z P, Beckermann C. Metall Mater Trans, 2007; 38B: 541[21] Han Z Q, Zhu W, Liu B C. Acta Metall Sin, 2009; 45: 356(韩志强, 朱维, 柳百成. 金属学报, 2009 45: 356)[22] Zhu W, Han Z Q, Liu B C. Acta Metall Sin, 2009 45: 363(朱维, 韩志强, 柳百成. 金属学报, 2009; 45: 363)[23] Anyalebechi P N. Acta Metall, 1995; 33: 1209[24] Lewis R W, Han Z Q, Gethin D T. C R Mec, 2007: 335: 287[25] Yang W, Li J X, Han Z Q, Zhao H D, Liu B C. Spec Cast Nonferrous Alloys, 2010; 30: 54(杨文, 李金玺, 韩志强, 赵海东, 柳百成. 特种铸造及有色合金, 2010; 30: 54) |
|