| 碳化对模拟混凝土孔溶液中HRB335钢腐蚀行为的影响 |
| 施锦杰 , 孙伟, 耿国庆 |
| 东南大学材料科学与工程学院~江苏省土木工程材料重点实验室, 南京 211189 |
|
| INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION |
| SHI Jinjie, SUN Wei, GENG Guoqing |
| College of Materials Science and Engineering, Jiangsu Key Laboratory of Construction Materials, Southeast University, Nanjing 211189 |
引用本文:
施锦杰 孙伟 耿国庆. 碳化对模拟混凝土孔溶液中HRB335钢腐蚀行为的影响[J]. 金属学报, 2011, 47(1): 17-24.
,
,
.
INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION[J]. Acta Metall Sin, 2011, 47(1): 17-24.
| [1] Kulakowski M P, Pereira F M, Dal-Molin D C C. Constr Build Mater, 2009; 23: 1189[2] Aperador W, Gutiérrez R M, Bastidas D M. Corros Sci, 2009; 51: 2027[3] Bertolini L, Carsana M, Redaelli E. J Cult Herit, 2008; 9: 376[4] Moreno M, Morris W, Alvarez M G, Duffo G S. Corros Sci, 2004; 46: 2681[5] Valcarce M B, Vázquez M. Mater Chem Phys, 2009; 115: 313[6] Huet B, L'Hostis V, Tricheux L, Idrissi H. Mater Corros, 2010; 61: 111[7] Huet B, L’Hostis V, Miserque F, Idrissi H. Electrochimi Acta, 2005; 51: 172[8] Kitowski C J, Wheat H G. Corrosion, 1997; 53: 216[9] Etteyeb N, Dhouibi L, Sanchez M, Alonso C, Andrade C, Triki E. J Mater Sci, 2007; 42: 4721[10] Sanchez M, Gregori J, Alonso C, Garcia-Jareno J J, Takenouti H, Vicente F. Electrochimi Acta, 2007; 52: 7634[11] Jamil H E, Shriri A, Boulif R, Montemor M F, Ferreira M G S. Cem Concr Compos, 2005; 27: 671[12] Vedalakshmi R, Palaniswamy N. Mag Concr Res, 2010; 62: 177[13] Hinatsu J T, Graydon W F, Foulkes F R. J Appl Electrochem, 1988; 19: 868[14] Veleva L, Alpuche-Aviles M A, Graves-Brook M K, Wipf D O. J Electroanal Chem, 2005; 578: 45[15] Foulkes F R, McGrath P. Cem Concr Res, 1999; 29: 873[16] Videm K. Electrochimi Acta, 2001; 46: 3895[17] Qian S Y, Cusson D. Cem Concr Compos, 2004; 26: 217[18] Andrade C, Keddam M, Novoa X R. Electrochimi Acta, 2001; 46: 3905[19] Flis J, Pickering H W, Osseo-Asare K. Electrochimi Acta, 1998; 43: 1921[20] Ghods P, Isgor O B, McRae G, Miller T. Cem Concr Compos, 2009; 31: 2 |
|