| 熔态AZ91D合金在含SO2的保护气氛中的保护膜特征 |
| 王先飞,熊守美 |
| 清华大学机械工程系, 清华大学汽车安全与节能国家重点实验室, 北京 100084 |
|
| CHARACTERIZATION OF THE SURFACE FILM FORMED ON MOLTEN AZ91D MAGNESIUM ALLOY PROTECTED BY SO2 MIXTURES |
| WANG Xianfei, XIONG Shoumei |
| State Key Laboratory of Automotive Safety and Energy, Department of Mechanical Engineering, Tsinghua University, Beijing 100084 |
引用本文:
王先飞 熊守美. 熔态AZ91D合金在含SO2的保护气氛中的保护膜特征[J]. 金属学报, 2010, 46(12): 1529-1533.
,
.
CHARACTERIZATION OF THE SURFACE FILM FORMED ON MOLTEN AZ91D MAGNESIUM ALLOY PROTECTED BY SO2 MIXTURES[J]. Acta Metall Sin, 2010, 46(12): 1529-1533.
| [1] Ricketts N, Cashion S, Bailey R. In: Dahle A ed., Proceedings of the First International Light Metals Technology Conference, Brisbane: Australia: CAST, 2003: 275
[2] Cashion S P. PhD Thesis, Australia: University of Queensland, 1998
[3] Cashion S P, Ricketts N J, Hayes P C. J Light Met, 2002; 2: 37
[4] Cashion S P, Ricketts N J, Hayes P C. J Light Met, 2002; 2: 43
[5] Pettersen G, ?vrelid E, Tranell G, Fenstad J, Gjestland H. Mater Sci and Eng, 2002; A332: 285
[6] Aarstad K, Tranell G, Pettersen G, Engh T A. In: Kaplan H ed., Magnesium Technology 2003, Warrendale, PA:TMS, 2003:5
[7] Liu X L, Xiong S M. Rare Met Mater Eng, 2006; 35(9): 1396
(刘晓龙, 熊守美. 稀有金属材料与工程, 2006; 35(9): 1396)
[8] Gjestland H, Schubert W. In: Kainer K U ed., Magnesium alloy and their applications, Weinheim: Chichester: Wiley, 2000: 761
[9] Aarstad K. PhD Thesis, Norway:Norwegian Universtity of Science and Technology, 2004
[10] Chen H K, Liu J R, Huang W D. Acta Metall Sin, 2007; 43(6): 625
(陈虎魁, 刘建睿, 黄卫东. 金属学报, 2007; 43(6): 625)
[11] Mrowec S, Przybylski K. Oxid Met, 1985; 23:107
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|