Al-Sc合金相结构的第一原理研究
苏振兴; 王雨晨; 王绍青
中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳 110016
FIRST-PRINCIPLES STUDY OF THE PHASE STRACTURES OF Al-Sc ALLOYS
SU Zhenxing; WANG Yuchen; WANG Shaoqing
Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
引用本文:

苏振兴 王雨晨 王绍青. Al-Sc合金相结构的第一原理研究[J]. 金属学报, 2010, 46(5): 623-628.
, . FIRST-PRINCIPLES STUDY OF THE PHASE STRACTURES OF Al-Sc ALLOYS[J]. Acta Metall Sin, 2010, 46(5): 623-628.

全文: PDF(709 KB)  
摘要: 

采用第一原理赝势平面波方法计算了Al-Sc合金固溶体、有序相和无序相结构对应的形成焓. 在无序合金的电子结构研究中, 引入了可以描述无序合金结构环境的小尺寸超单胞模型-SQS模型. 计算结果表明: 超饱和固溶体中的Sc原子具有偏聚产生L12结构的Al3Sc析出相和L10结构的AlSc析出相的趋势. 依据对各相的电子结构及电子密度分析结果, 初步探讨了时效处理导致超饱和固溶体Al(Sc)中偏聚产生L12结构Al3Sc析出相的形成机理.

关键词 : Al-Sc合金,  第一原理,  准随机结构,  析出相    
Abstract:

The formation enthalpies of the Al-Sc compounds and the Al-rich solid solution phase have been studied from first-principles based on plane--wave pseudopotential method. To calculate the electronic structure of the disordered Al-Sc alloys, the small-size special quasirandom structures (SQS), which exhibited similar structure environments as that of the disordered Al-Sc alloys, are employed. It is shown that the Sc atoms in supersaturated solid solution tend to segregation forming ordered Al3Sc< (L12) and AlSc (L10) precipitations. The nucleation mechanism of Al3Sc precipitation phase in the supersaturated Al(Sc) solid solution is analyzed in terms of the calculated densities of states and distributions of electron densities.

Key words: Al-Sc alloy    first-principles    quasirandom structure    precipitate
收稿日期: 2009-12-10     
基金资助:

国家重点基础研究发展计划资助项目2006CB605103

作者简介: 苏振兴, 男, 1984年生, 硕士生

[1] Du Y Y, Su X K, Zou J X, Nie Z R. Heat Treat Met, 2007; 32(2): 12
(杜元元, 苏学宽, 邹景霞, 聂祚仁. 金属热处理, 2007; 32(2): 12)

[2] Iwamura S, Miura Y. Acta Mater, 2004; 52: 519
[3] Hyde K B, Norman A F, Prangnell P B. Acta Mater, 2001; 49: 1327
[4] Woodward C, Asta M. Phys Rev, 2001; 63B: 094103
[5] Ozolin V, Asta M. Phys Rev Lett, 2001; 86: 448
[6] Asta M, Ozolins V. Phys Rev, 2001; 64B: 094104
[7] Marquis E A, Seidman D N, Asta M,Woodward C, Ozolins V. Phys Rev Lett, 2003; 91: 036101
[8] Asta M, Foiles S M, Quong A A. Phys Rev, 1998; 57B: 11265
[9] Zunger A, Wei S H, Ferreira L G, Bernard J E. Phys Rev Lett, 1990; 65: 3353
[10] Wei S H, Ferreira L G, Bernard J E, Zunger A. Phys Rev, 1990; 42B: 159622
[11] Jiang C, Wolverton C, Sofo J, Chen L Q, Liu Z K. Phys Rev, 2004; 69B: 214202
[12] Van De Walle A, Asta M, Ceder G. CALPHAD: Comput Coupl Phase Diagrams Thermochem, 2004; 26: 539
[13] Giannozzi P, Baroni S, Bonini N, Calandra M, Car R, Cavazzoni C, Ceresoli D, Chiarotti G L, Cococcioni M, Dabo I, Dal Corso A, Fabris S, Fratesi G, De Gironcoli S, Gebauer R, Gerstmann U, Gougoussis C, Kokalj A, Lazzeri M, Martinsamos L, Marzari N, Mauri F, Mazzarello R, Paolini S, Pasquarello A, Paulatto L, Sbraccia C, Scandolo
S, Sclauzero G, Seitsonen A P, Smogunov A, Umari P, Wentzcovitch R M. J Phys: Condens Matter, 2009; 21: 395502
[14] Monkhorst H J, Pack J D. Phys Rev, 1972; 13B: 5188
[15] Villars P, Calvert L D. Pearson’s Handbook of Crystallographic Data for Inter–metallic Phases. 2nded.,Materials Park, Ohio: ASM Intermational, 1991: 999

[1] 梁凯, 姚志浩, 谢锡善, 姚凯俊, 董建新. 新型耐热合金SP2215组织与性能的关联性[J]. 金属学报, 2023, 59(6): 797-811.
[2] 马国楠, 朱士泽, 王东, 肖伯律, 马宗义. SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能[J]. 金属学报, 2023, 59(12): 1655-1664.
[3] 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银. 新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能[J]. 金属学报, 2023, 59(12): 1590-1602.
[4] 陈凯旋, 李宗烜, 王自东, Demange Gilles, 陈晓华, 张佳伟, 吴雪华, Zapolsky Helena. Cu-2.0Fe合金等温处理过程中富Fe析出相的形态演变[J]. 金属学报, 2023, 59(12): 1665-1674.
[5] 李小琳, 刘林锡, 李雅婷, 杨佳伟, 邓想涛, 王海丰. 单一 MX 型析出相强化马氏体耐热钢力学性能及蠕变行为[J]. 金属学报, 2022, 58(9): 1199-1207.
[6] 赵宇宏, 景舰辉, 陈利文, 徐芳泓, 侯华. 装甲防护陶瓷-金属叠层复合材料界面研究进展[J]. 金属学报, 2021, 57(9): 1107-1125.
[7] 陈果, 王新波, 张仁晓, 马成悦, 杨海峰, 周利, 赵运强. 搅拌头转速对2507双相不锈钢搅拌摩擦加工组织及性能的影响[J]. 金属学报, 2021, 57(6): 725-735.
[8] 许坤, 王海川, 孔辉, 吴朝阳, 张战. 一种新分组团簇动力学模型模拟铝合金中的Al3Sc析出[J]. 金属学报, 2021, 57(6): 822-830.
[9] 高一涵, 刘刚, 孙军. 耐热铝基合金研究进展:微观组织设计与析出策略[J]. 金属学报, 2021, 57(2): 129-149.
[10] 郭倩颖, 李彦默, 陈斌, 丁然, 余黎明, 刘永长. 高温时效处理对S31042耐热钢组织和蠕变性能的影响[J]. 金属学报, 2021, 57(1): 82-94.
[11] 刘峰, 王天乐. 基于热力学和动力学协同的析出相模拟[J]. 金属学报, 2021, 57(1): 55-70.
[12] 韩宝帅, 魏立军, 徐严谨, 马晓光, 刘雅菲, 侯红亮. 预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响[J]. 金属学报, 2020, 56(7): 1007-1014.
[13] 梁孟超, 陈良, 赵国群. 人工时效对2A12铝板力学性能和强化相的影响[J]. 金属学报, 2020, 56(5): 736-744.
[14] 刘振宝,梁剑雄,苏杰,王晓辉,孙永庆,王长军,杨志勇. 高强度不锈钢的研究及发展现状[J]. 金属学报, 2020, 56(4): 549-557.
[15] 张正延,柴锋,罗小兵,陈刚,杨才福,苏航. 调质态含Cu高强钢的强化机理及钢中Cu的析出行为[J]. 金属学报, 2019, 55(6): 783-791.