| Ti36Zr40Ni20Pd4准晶的热稳定性与室温储氘性能 |
| 黄火根1); 陈亮2); 李嵘2); 罗德礼2) |
| 1) 表面物理与化学国家重点实验室; 绵阳 621907
2) 中国工程物理研究院; 绵阳 621900 |
|
| THERMAL STABILITY AND DEUTERIUM ABSORPTION AT ROOM TEMPERATURE OF Ti36Zr40Ni20Pd4 QUASICRYSTAL |
| HUANG Huogen1); CHEN Liang2); LI Rong2); LUO Deli2) |
| 1) National Key Lab for Surface Physics and Chemistry; Mianyang 621907
2) China Academy of Engineering Physics; Mianyang 621900 |
引用本文:
黄火根 陈亮 李嵘 罗德礼. Ti36Zr40Ni20Pd4准晶的热稳定性与室温储氘性能[J]. 金属学报, 2010, 46(5): 629-633.
,
,
.
THERMAL STABILITY AND DEUTERIUM ABSORPTION AT ROOM TEMPERATURE OF Ti36Zr40Ni20Pd4 QUASICRYSTAL[J]. Acta Metall Sin, 2010, 46(5): 629-633.
| [1] Bogdanovic B, Schwickardi M. Appl Phys, 2001; 72A: 221
[2] Chen P, Xiong Z T, Luo J Z, Lin J Y, Tan K L. Nature, 2002; 420: 302
[3] Xiong Z T, Yong C K, Wu G T, Chen P, Shaw W, Karkamkar A, Autrey T, Jones M O, Johnson S R, Edwards P P, David W I F. Nat Mater, 2008; 7: 138
[4] Feng K M. Chin Nucl Power, 2009; 2: 212
(冯开明. 中国核电, 2009; 2: 212)
[5] Gibbons P C, Hennig R G, Huett V T, Kelton K F. J Non–Cryst Solids, 2004; 334: 461
[6] Kelton K F, Hartzell J J, Hennig R G, Huett V T, Takasaki A. Philos Mag, 2006; 86: 957
[7] Liu B Z, Liu D M, Wu Y M, Li L Q, Wang L M. Int J Hydro Energy, 2007; 32: 2429
[8] Liu B Z, Wu Y M, Wang L M. J Power Source, 2006; 162: 713
[9] Liu B Z, Wu Y M, Wang L M. J Power Source, 2006; 159: 1458
[10] Liu B Z, Wu Y M, Wang L M. Int J Hydrogen Energy, 2006; 31: 1394
[11] Liu B Z, Wu Y M, Wang L M. Rare Met, 2007; 26: 440
[12] Takasaki A, Huett V T, Kelton K F. J Non–Cryst Solids, 2004; 334: 457
[13] Takasaki A, Kelton K F. Int J Hydrogen Energy, 2006; 31: 183
[14] Hennig R G, Majzoub E H, Carlsson A E, Kelton K F, Henley C L, Yelon W B, Misture S. Mater Sci Eng, 2000; 294A: 361
[15] Kim J Y, Hennig R, Huett V T, Gibbons P C, Kelton K F. J Alloys Compd, 2005; 404: 388
[16] Huang H G, Dong P, Yin C, Zhang P C, Bai B, Dong C. Int J Hydrogen Energy, 2008; 33: 722
[17] Huang H G, Li R, Yin C, Zheng S T, Zhang P C. Int J Hydrogen Energy, 2008; 33: 4607
[18] Liu B Z, Liu J J, Mi G F, Zhang Z, Wu Y M, Wang L M. J Alloys Compd, 2009; 475: 881
[19] Liu B Z, Zhang Y D, Mi G F, Zhang Z, Wang L M. Int J Hydrogen Energy, 2009; 34: 6925
[20] Huang H G, Yin C, Wu J, Zhang P C. Chin J Nonferrous Met, 2008; 18: 108
(黄火根, 银陈, 吴江, 张鹏程. 中国有色金属学报, 2008; 18: 108)
[21] Cahn J W, Shechtman D, Gratias D. J Mater Res, 1986; 1: 13
[22] Qiang J B, Wang Y M, Wang D H, Dong C. Rare Met Mater Eng, 2004; 33: 949
(羌建兵, 王英敏, 王德和, 董闯. 稀有金属材料与工程, 2004; 33: 949)
[23] Huang H G, Jia J P, Li R. Acta Metall Sin, 2009; 45: 1272
(黄火根, 贾建平, 李嵘. 金属学报, 2009; 45: 1272)
[24] Hirooka Y, Miyake M, Sano T. J Nucl Mater, 1981; 96: 227
[25] Huang L J, Yu B X, Gao S J. Met Funct Mater, 1998; 5: 124
(黄利军, 虞炳西, 高树浚. 金属功能材料, 1998; 5: 124)
[26] Wang W W, Long X G. J Nucl Radiochem, 2007; 29: 80
(王伟伟, 龙兴贵. 核化学与放射化学, 2007; 29: 80)
[27] Coddens G, Viano A M, Gibbons P C, Kelton K F, Kramer M J. Solid State Comm, 1997; 104: 179
[28] Faust K R, Pfitsch D W, Stojanovich N A, McDowell A F, Adolphi N L, Majzoub E H, Kim J Y, Gibbons P C, Kelton K F. Phys Rev, 2000; 62B: 11444 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|