|
|
|
| 超高强度钢疲劳塑性区内的应变诱发马氏体相变 |
| 高惠临;谈育煦;王笑天 |
| 西安交通大学;西安石油学院;西安交通大学;安交通大学强度研究所;教授;西安和平门外西 |
|
| STRAIN INDUCED MARTENSITIC TRANSFORMATION IN FATIGUE CRACK TIP ZONE FOR AN ULTRA-HIGH STRENGTH STEEL |
| GAO Huilin;TAN Yuxu; Xi'an Jiaotong UniversityWANG Xiaotian Professor;Institute of Metallic Materials and Strength;Xi'an Jiaotong Univedrity |
引用本文:
高惠临;谈育煦;王笑天. 超高强度钢疲劳塑性区内的应变诱发马氏体相变[J]. 金属学报, 1988, 24(1): 17-23.
,
,
.
STRAIN INDUCED MARTENSITIC TRANSFORMATION IN FATIGUE CRACK TIP ZONE FOR AN ULTRA-HIGH STRENGTH STEEL[J]. Acta Metall Sin, 1988, 24(1): 17-23.
1 Ritchie R O. Horn R M. Metall Trans, 1978; 9A: 331 2 Kim K J, Schwartz L H. Mater Sci Eng, 1978; 33: 5 3 Syn C K, Fultz B, Morris J W. Metall Trans, 1978; 9A: 1635 4 Sastry C N, Khan K H, Wood W E. Metall Trans, 1982; 13A: 676 5 Hertzberg Rw,王克仁,罗力更,姚蘅,刘国玺译。工程材料的变形与断裂力学,机械工业出版社,1982:397 6 Antolovich S D, Singh B. Metall Trans, 1971; 2: 2135 7 Antolovich S D, Singh B. Metall Trans, 1970; 1: 3463 8 Barnard S J, Smith G D W, Sarikaya M, Thomas G. Scr Metall, 1981; 15: 387 9 Parker E R, Zackay V F. Eng Fract Mech, 1973; 5: 147[ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|