| 奥氏体Fe-Mn合金的低温脆性 |
| 柴寿森 |
| 中国科学院金属研究所;副研究员;沈阳文化路 |
|
| LOW TEMPERATURE EMBRITTLEMENT OF AUSTENITIC Fe-Mn ALLOYS |
| CHAI Shousen Institute of Metal Research; Academia Sinica. Shenyang |
引用本文:
柴寿森. 奥氏体Fe-Mn合金的低温脆性[J]. 金属学报, 1988, 24(1): 24-29.
.
LOW TEMPERATURE EMBRITTLEMENT OF AUSTENITIC Fe-Mn ALLOYS[J]. Acta Metall Sin, 1988, 24(1): 24-29.
1 Morris J W. Hwang S K, Yushchenku K A. Adv Cryogenic Eng, 1978; 2: 91 2 #12 3 #12 4 #12 5 #12 6 #12 7 #12 8 Hansen. Constitution of Binary Alloys, 2nd edition, 1958 9 Umebayashi H, Ishikawa Y. J Phys Soc Jpn, 1966; 21: 1281 10 #12 11 #12 12 Ito K, Kobayshi M. Met Sci, 1979; 13: 502B |
|