| 非晶态Fe_(75)Cr_5P_(13)C_7合金粉末的耐蚀性研究 |
| 孙中子;王井银 |
| 天津大学材料系防腐教研室;讲师;天津大学 |
|
| CORROSION RESISTANCE OF AMORPHOUS Fe_(75)Cr_5P_(13)C_7 POWDER |
| WANG Jingyin Tianjin University SUN ZhongziLecturer;Department of Materials;Tianjin University |
引用本文:
孙中子;王井银. 非晶态Fe_(75)Cr_5P_(13)C_7合金粉末的耐蚀性研究[J]. 金属学报, 1988, 24(1): 138-140.
,
.
CORROSION RESISTANCE OF AMORPHOUS Fe_(75)Cr_5P_(13)C_7 POWDER[J]. Acta Metall Sin, 1988, 24(1): 138-140.