| 厚度减薄对Fe_(81)B_(13.5)Si_(3.5)C_2非晶薄带磁各向异性和磁矩取向分布的影响 |
| 徐祖雄;马如璋 |
| 北京钢铁学院金属物理教研室;副教授;北京学院路30号;北京钢铁学院 |
|
| EFFECTS OF THINNING ON MAGNETIC ANISOTROPY AND DISTRIBUTION OF MOMENTS IN AMORPHOUS ALLOY Fe_(81)B_(13.5)Si_(3.5)C_2 |
| MA Ruzhang Beijing University of Iron and Steel Technology XU Zuxiong Asspcoated professor Spediatty of Metal Physics;Beijing University of from and Steel Technology |
引用本文:
徐祖雄;马如璋. 厚度减薄对Fe_(81)B_(13.5)Si_(3.5)C_2非晶薄带磁各向异性和磁矩取向分布的影响[J]. 金属学报, 1988, 24(1): 141-143.
,
.
EFFECTS OF THINNING ON MAGNETIC ANISOTROPY AND DISTRIBUTION OF MOMENTS IN AMORPHOUS ALLOY Fe_(81)B_(13.5)Si_(3.5)C_2[J]. Acta Metall Sin, 1988, 24(1): 141-143.
1 Kronmuller H, Fahnle M, Domann M, Grimm H, Grimm R, Groeger B. J Magn Magn Mater, 1979; 13: 53 2 林肇华,戴道生.物理学报,1982;31:871 3 Tejedor M, Hernando B. J Phys D. 1980; 13 1709 4 Decker J J. J Appl Phys, 1981; 52: 1905 5 Takahashi M, Ikeda N. Miyazaki T. Jpn J Appl Phys. 1976; 15. 1821 6 Fischer H, Gonser U, Preston R, Wagner HG. J Magn Magn Mater, 1978; 9: 336 7 Ito A, Torikai E, Morimoto S, Shiiki K, Kudo M. Jpn J Appl Phys, 1981; 20: 797 8 Gonser U, Chafari M, Wagner H G, Fischer H. J Phys, colloq. (Paris), 1979; 40: C2--126 9 Chien C L. J Appl Phys, 1976; 47: 2234 10 Gonser U, Ackermann M, Wagner H-G. J Magn Magn Mater, 1983; 31--34: 1605 11 Ok H N, Morrish A H. Phys Rev B, 1981, 23: 2257 12 徐祖雄,马如璋,平爵云.中国科学(A),1985;(1) 44 13 徐祖雄,马如璋,李士.科学通报,1985;(9) 71 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|