| 合金成分和热处理对奥氏体不锈钢氢渗透行为的影响 |
| 孙秀魁;徐坚;李依依 |
| 沈阳文化路中国科学院金属研究所;高级工程师;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF COMPOSITION AND HEAT TREATMENT ON HYDROGEN PERMEATION IN AUSTENITIC STAINLESS STEELS |
| SUN Xiukui;XU Jian;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
孙秀魁;徐坚;李依依. 合金成分和热处理对奥氏体不锈钢氢渗透行为的影响[J]. 金属学报, 1988, 24(3): 187-192.
,
,
.
EFFECT OF COMPOSITION AND HEAT TREATMENT ON HYDROGEN PERMEATION IN AUSTENITIC STAINLESS STEELS[J]. Acta Metall Sin, 1988, 24(3): 187-192.
1 Quick N R, Johnson H H. Metall Trans, 1979; 10A: 67 2 Gromov A I, Kovneristyi Y K. Met Sci Heat Trest, 1980; 22: 321 3 Studebaker P, Altstetter C, Conley W. In: Bernstein L M, Thompson A W eds., Hydrogen Effects in Metals, Warrendale: TMS-AIME, 1981: 169 4 Katsuta H, Furukawa K. J Nucl Sci Technol, 1981; 18: 143 5 Outlaw R A, Peterson D T. Metall Trans, 1983; 14A: 1869 6 Tanabe T, Yamanishi Y, Sawada K, Imoto S. J Nucl Mater, 1984; 123: 1568 7 Louthan M R, Derrick R G. Corros Sci, 1975; 15: 565 8 Perng T P, Altstetter C J. Acta Metall, 1986; 34: 1771 9 孙秀魁,徐坚,刘宝昌.真空科学与技术,1986; 6(6) :32 10 冼爱平.金属研究所硕士论文,1985 11 胡学军.金属研究所硕土论文,1986 12 Oriani R A. Acta Metall, 1970; 18: 147 14 肖纪美.不锈钢的金属学问题,北京:冶金工业出版社,1983:420 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|