| Fe-Mn-C及Fe-Ni-C合金马氏体相变热力学 |
| 徐祖耀;潘牧 |
| 上海交通大学;上海交通大学 |
|
| Acta Metallurgica Sinica<1989.04> |
引用本文:
徐祖耀;潘牧. Fe-Mn-C及Fe-Ni-C合金马氏体相变热力学[J]. 金属学报, 1989, 25(4): 16-22.
,
.
[J]. Acta Metall Sin, 1989, 25(4): 16-22.
1 徐祖耀.金属学报,1979;15:329 2 Hsu T Y (Xu Zuyao), Chang Hongbing, Lou Shoufu. J Mater Sci, 1983; 18: 3206 3 Enomoto M, Aaronson H I. CALPHAD, 1985; 9: 43 4 Foo E-H, Lupis C H P. Acta Metall, 1973; 21: 1409 5 Toop G W. Trans AIME, 1965; 233: 850 6 潘牧,徐祖耀.金属学报待发表. 7 潘牧,徐祖耀.材料科学进展,1988;2(5) :32 8 Wada T, Wada H, Elliot J F, Chipman J. Metall Trans, 1972; 3: 1657 9 Kirchner G, Nishizawa T, Uhrenius B. Metall Trans, 1973; 4: 167 10 Orr R L, Chipman J. Trans AIME, 1967; 239: 630. 11 Breedis J F, Kaufman L. Metall Trans, 1971; 2: 2359 12 Mou Yiwen, Hsu T Y (Xu Zuyao). Acta Metall, 1986; 34: 325 13 Hsu T Y (Xu Zuyao), Chang Hongbing. Acta Metall, 1984; 32: 343 14 Benz R. Metall Trans, 1974; 5: 2217 15 Hsu T Y (Xu Zuyao), Chen Weichong. Scr Metall, 1987; 21: 1289 16 Hillert M, wada T, Wada H. J Iron Steel Inst, 1967; 205 (5) : 539 17 Kaufman L, Nesor H. Z Metallk, 1973; 64; 249 18 Weiss R J, Tauer K J. Phys Rev, 1956; 102: 1490 19 Kirkaldy J S, Thomson B A, Baganis E A. In: Doane, Kirkaldy J S eds., Hardenability Concepts With Applications to Steel, AIME, 1978 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|