| 镍基合金辉光放电阴极溅射表面形貌 |
| 任建世;赵惠林;张功杼 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| OBSERVATION ON SPUTTERING SURFACE OF ALLOYS IN GLOW DISCHARGE |
| REN Jianshi;ZHAO Huilin;ZHANG Gongshu Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
任建世;赵惠林;张功杼. 镍基合金辉光放电阴极溅射表面形貌[J]. 金属学报, 1989, 25(4): 148-150.
,
,
.
OBSERVATION ON SPUTTERING SURFACE OF ALLOYS IN GLOW DISCHARGE[J]. Acta Metall Sin, 1989, 25(4): 148-150.