| 高温蠕变中晶界沉淀强化的一种唯象模型 |
| 李培恩;张俊善;金俊泽 |
| 大连理工大学材料系;大连116024;大连理工大学;大连理工大学 |
|
| A PHENOMENOLOGICAL MODEL FOR GRAIN BOUNDARY PRECIPITATION STRENGTHENING IN HIGH TEMPERATURE CREEP |
| LI Peien;ZHANG Junshan;JIN Junze Dalian University of Technology Department of Materials Engineering;Dalian University of Technology; Dalian 116024 |
引用本文:
李培恩;张俊善;金俊泽. 高温蠕变中晶界沉淀强化的一种唯象模型[J]. 金属学报, 1990, 26(4): 50-53.
,
,
.
A PHENOMENOLOGICAL MODEL FOR GRAIN BOUNDARY PRECIPITATION STRENGTHENING IN HIGH TEMPERATURE CREEP[J]. Acta Metall Sin, 1990, 26(4): 50-53.
1 张俊善,陈卫星,曹智本.金属学报,1989;25:A141 2 Zhang J S, Li P E, Chen W X, Jin J Z. Scr Metall, 1989; 23: 547 3 Matsuo T, Ueki M, Takeyama M, Tanaka R. J Mater Sci, 1987; 22: 1901 4 Horton C A P. Acta Metall, 1972; 20: 477 5 Beckitt F R, Clark B R. Acta Metall, 1967; 15: 113 6 Cottrell A H. The Mechanical Properties of Matter, New York: John Wiley & Sons, 1964: 282 7 Raj S V, Pharr G M. Mater Sci Eng, 1986; 81: 217 8 Mintz B, Campbell P. Mater Sci Technol, 1987; 3: 8451 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|