| 镀Cu-Ni的碳纤维及其复合材料 |
| 孙守金;张名大 |
| 中国科学院金属研究所五室;研究实习员;中国科学院金属研究所 |
|
| CARBON FIBRE ELECTROPLATED BY Cu-Ni DUPLEX COATING AND ITS COMPOSITE |
| SUN Shoujin;ZHANG Mingda Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
孙守金;张名大. 镀Cu-Ni的碳纤维及其复合材料[J]. 金属学报, 1990, 26(6): 132-136.
,
.
CARBON FIBRE ELECTROPLATED BY Cu-Ni DUPLEX COATING AND ITS COMPOSITE[J]. Acta Metall Sin, 1990, 26(6): 132-136.
1 国谷启一,荒川英夫,阪上正,御法川齐,明山健二,坂本达事.日本金属学会志,1986:50:583 2 Mortimer D A, Nicholas M. J Mater. Sci, 1970, 5: 149. 3 Arakawa H, Kuniya K, Namekawa T, Litzba T. US Pat, 1978: 4 083 719 4 Warren R, Anderson C H, Carlsson M. J Mater Sci, 1978; 13: 178 5 易沛,陈汴琨,吴云书.复合材料学报,1987;4(3) :56 6 Sun Shoujin, Wang Yuqing, Zhang Mingda. In: Li Hengde ed., Proc C-MRS International'90, 18--22 June, 1990, Beijin, in pressed 7 孙守金,王作明,张名大,复合材料学报,1990;7(1) :30 |
|