| SiC晶须显微结构的研究 |
| 徐海钢;朱静;苑洪;宁小光;叶恒强 |
| 冶金工业部钢铁研究总院13室;助理工程师;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;中国科学院金属研究所固体原子象实验室;中国科学院金属研究所固体原子象实验室 |
|
| MICROSTRUCTURE OF SILICON CARBIDE WHISKER |
| XU Haigang;ZHU Jing;YUAN Hong;NING Xiaoguang;YE Hengqiang Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing; Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
徐海钢;朱静;苑洪;宁小光;叶恒强. SiC晶须显微结构的研究[J]. 金属学报, 1990, 26(6): 137-144.
,
,
,
,
.
MICROSTRUCTURE OF SILICON CARBIDE WHISKER[J]. Acta Metall Sin, 1990, 26(6): 137-144.
1 Amelincks S, Strumane G, Webb W W. J Appl Phys, 1960; 31: 1359 2 郭常霖.物理学报,1982;31:1511 3 郭常霖.物理学报,1982;31:1526 4 Changxin, Zhou Yanchun, Xia Fei. Chin J Met Sci Technol, 1987; 3: 289 5 More K L. Proc the 46th Annual Meeting of the Electron Microscopy Society of America, 1988: 568 6 Nutt. S R. J Am Ceram Soc, 1988; 71: 149 7 Karasek K R, Bradley S A, Donner J T, Martin M R, Haynes K L, Yeh H C. J Mater Sci, 1989; 24: 1617 8 Nutt S R. J Am Ceram Soc, 1984; 67: 428 9 郭常霖.物理学报,1965;21:1089 10 Hiraga K. Sci Rep Res Inst, Tohoku Univ, Ser. A: Physics, Chemistry and Metallurgy, 1984; 32: 1 11 Nutt S R, Dura J M. Scr Metall, 1986; 20: 1055 12 De Jong R, McCauley R A, Tambuyser P. J Am Ceram Soc, 1987; 70: C338 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|