| SiC_p/6061Al复合材料的疲劳行为 |
| 于维成;袁金才;王中光 |
| 中国科学院金属研究所;副研究员;中国科学院金属研究所;中国科学院金属研究所 |
|
| FATIGUE BEHAVIOUR OF SiC_p/6061Al COMPOSITE |
| YU Weicheng;YUAN Jincai;WANG Zhongguang Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
于维成;袁金才;王中光. SiC_p/6061Al复合材料的疲劳行为[J]. 金属学报, 1990, 26(6): 127-131.
,
,
.
FATIGUE BEHAVIOUR OF SiC_p/6061Al COMPOSITE[J]. Acta Metall Sin, 1990, 26(6): 127-131.
1 Hurd N J. Mater Sci Technol, 1988; 4: 513 2 Yau S S, Mayer G. Mater Sci Eng, 1986; 82: 45 3 Arsenault R J. Mater Sci Eng, 1984; 64: 171 4 Vogelsang M, Arsenault R J, Fisher R M. Metall Trans, 1986; 17A: 379 5 Laird C. Fatigue and Microsturcture, Metals Park, Ohio: ASM, 1978: 149 6 Chevalier J L, Gibbons D F, Leonard L. J Appl Phys, 1972; 43: 73 7 Mitchell A B, Teer D G. Met Sci J, 1969; 3: 183 |
|