| 40CrMnSiMoVA钢准贝氏体的疲劳性能 |
| 陈大明;康沫狂;谭若兵 |
| 西北工业大学;副教授;西北工业大学;中国科学院金属研究所 |
|
| FATIGUE PROPERTIES OF META-BAINITE IN STEEL 40CrMnSiMoVA |
| CHEN Daming;KANG Mokuang Northwestern Polytechnical University; Xi'an; TAN Ruobing Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
陈大明;康沫狂;谭若兵. 40CrMnSiMoVA钢准贝氏体的疲劳性能[J]. 金属学报, 1991, 27(6): 64-69.
,
,
.
FATIGUE PROPERTIES OF META-BAINITE IN STEEL 40CrMnSiMoVA[J]. Acta Metall Sin, 1991, 27(6): 64-69.
1 方鸿生,赵如发,郑燕康,陈秀云.金属热处理,1987;(2) :44 2 康沫狂,周鹿宾,陈大明.陕西冶金,1989;(2) :16 3 康沫狂.材料科学进展,1988;2(3) :12 4 杨峥.金属学报,1978;14:409 5 Kang Mokuang, Sun Jialin, Yang Quanmin. Metall Trans, 1990; A21: 853 6 陈大明.西北工业大学博士学位论文,1988 |
|