| 钢中含碳量对化学气相沉积TiN涂层的影响 |
| 陈二保 |
| 华东冶金学院;副教授 |
|
| EFFECT OF CARBON CONTENT INSUBSTRATE ON CVD TiN COATING |
| CHEN Erbao East China Institute of Metallurgy; Maanshan; Anhui |
引用本文:
陈二保. 钢中含碳量对化学气相沉积TiN涂层的影响[J]. 金属学报, 1991, 27(6): 122-125.
.
EFFECT OF CARBON CONTENT INSUBSTRATE ON CVD TiN COATING[J]. Acta Metall Sin, 1991, 27(6): 122-125.
1 陈二保,郭万华.华东冶金学院学报,1987;4(4) :36 2 Kim M S, Chun J S. Proc Eur Conf CVD, 4th, 1983: 517--303 |
|