| Si和Mn对钢中贝氏体形态和转变动力学的影响 |
| 刘世楷;杨柳;张筠;朱德贵 |
| 西南交通大学材料系;教授;成都市610031;西南交通大学;西南交通大学;西南交通大学 |
|
| INFLUENCE OF Si AND Mn ON MORPHOLOGY OF BAINITIC FERRITE AND KINETICS OF BAINITE TRANSFORMATION IN Fe-C ALLOY |
| LIU Shikai; YANG Liu; ZHANG Jun; ZHU Degui (Southwest Jiaotong University; Chengdu) |
引用本文:
刘世楷;杨柳;张筠;朱德贵. Si和Mn对钢中贝氏体形态和转变动力学的影响[J]. 金属学报, 1992, 28(12): 1-8.
,
,
,
.
INFLUENCE OF Si AND Mn ON MORPHOLOGY OF BAINITIC FERRITE AND KINETICS OF BAINITE TRANSFORMATION IN Fe-C ALLOY[J]. Acta Metall Sin, 1992, 28(12): 1-8.
1 Bhadeshia H K D H, Edmonds D V. Metall Trans, 1979; 10A:895 2 Liu S K, Reynolds W T Jr., Hu H, Shiflet G J, Aaronson H I. Metall Trans, 1985; 16A:457 3 Aaronson H h Liu S K, Reynolds W T Jr., Shiflet G I. J Mater Sci, 1985; 20:4232 4 Reynolds W T Jr., Liu S K, Li F Z, Hartfield S, Aaronson H I. Metall Trans, 1990; 21A:1479 5 Reynolds W T Jr., Li F Z, Shui C K, Aaronson H I. Metall Trans, 1990; 21A:1433 6 杨萍,杨柳,刘世楷.第2届全国贝氏体相变讨论会论文集,1990;10:26 7 Sharma R C, Purdy G R. Metall Trans, 1973; 14A:2303 8 Lee D Y,Marcus H L 见:中国金属学会编译组译,物理冶金进展评论,北京:冶金工业出版社, 1985;457 9 Balluffi R W. In: JohnSon W C, Blakely J M eds., Insterfacial Segregation. Metal Park, Ohio: ASM, 1979:193 10 Enomoto M, White C L, Aaronson H I. Metall Trans, 1988; 19A:1807 11 Guttmann M, McLean D. In: Johnson W C, Blakely J M eds., Interfacial Segregation. Metal Park, Ohio: ASM, 1979:261' |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|