硼酸铝晶须增强Al复合材料的性能及界面结构 |
潘进;宁小光;胡魁毅;叶恒强 |
国防科大材料科学与应用化学系;讲师;长沙410073;中国科学院金属研究所固体原子象实验室;中国科学院金属研究所固体原子象实验室;中国科学院金属研究所固体原子象实验室 |
|
MECHANICAL PROPERTIES AND INTERFACIAL STRUCTURES OF ALUMINIUM BORATE WHISKER REINFORCED Al COMPOSITES |
NING Xiaoguang;HU Kuiyi;YE Hengqiang Changsha Institute of Technology; Changsha Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; ShenyangPAN Jin;lecturer;Deparment of Materials Science and Applied Chemistry Changsha Institute of Technology;Changsha 410073 |
引用本文:
潘进;宁小光;胡魁毅;叶恒强. 硼酸铝晶须增强Al复合材料的性能及界面结构[J]. 金属学报, 1993, 29(6): 88-94.
,
,
,
.
MECHANICAL PROPERTIES AND INTERFACIAL STRUCTURES OF ALUMINIUM BORATE WHISKER REINFORCED Al COMPOSITES[J]. Acta Metall Sin, 1993, 29(6): 88-94.
1 Fukunaga H, Gohda K, Ohta N. Trans Jpn Inst Met, 1983; 24: 642 2 福永秀春,合田公一,田端伸雄,材料,1985;34:64 3 Suganuma K, Fujita T, Niihara K, Suzuki N. J Mater Sci Lett, 1989; 8: 808 4 Suganuma K, Fujita T. Suzuki N, Niihara K. J Mater Sci Lett, 1990: 9: 633 5 Fukunaga H, Pan J, Ning X G. Proc 1st Canadian International Composites Conf and Exhi Montreal, Quebec, Canada, 1991: 3C: 2--1 6 隗学礼.内部资料,1992: 7 Ihara M, Imai K, Fukunaga J, Yoshida N. Yogyo-Kyokai-Shi, 1980; 88: 27 |
|