| TiAl+La有序合金的室温力学性能 |
| 陈仕奇;曲选辉;雷长明;黄伯云 |
| 中南工业大学 |
|
| ROOM TEMPERATURE MECHANICAL PROPERTIES OF ORDERED TiAl+La ALLOYS |
| CHEN Shiqi;QU Xuanhui;LEI Changming;HUANG Baiyun(Central South University of Technologv;Changsha)(Manuscript received 26 August;1993;in revised form 30 October;1993) |
引用本文:
陈仕奇;曲选辉;雷长明;黄伯云. TiAl+La有序合金的室温力学性能[J]. 金属学报, 1994, 30(1): 20-24.
,
,
,
.
ROOM TEMPERATURE MECHANICAL PROPERTIES OF ORDERED TiAl+La ALLOYS[J]. Acta Metall Sin, 1994, 30(1): 20-24.