| K_2O·8TiO_(2(W))/ZL109复合材料在热暴露和热循环条件下的界面反应和界面结构 |
| 沈保罗;李伟;钟毓茂;宁小光;李吉红;叶恒强 |
| 成都科技大学;中国科学院金属研究所固体原子像开放实验室 |
|
| INTERFACIAL REACTION IN K_2O·8TiO_(2(w))/ ZL109 COMPOSITE UNDER THERMAL EXPOSURE OR THERMAL CYCLING |
| SHEN Baoluo;LI Wei;ZHONG Yumao(Chengdu University of Science and Technology);NING Xiaoguang;LI Jihong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences;Shenyang) |
引用本文:
沈保罗;李伟;钟毓茂;宁小光;李吉红;叶恒强. K_2O·8TiO_(2(W))/ZL109复合材料在热暴露和热循环条件下的界面反应和界面结构[J]. 金属学报, 1994, 30(21): 427-431.
,
,
,
,
,
.
INTERFACIAL REACTION IN K_2O·8TiO_(2(w))/ ZL109 COMPOSITE UNDER THERMAL EXPOSURE OR THERMAL CYCLING[J]. Acta Metall Sin, 1994, 30(21): 427-431.
| 1福永秀春,武市通文,太田进.日本复合材料学会志,1982;8:662西田义则,今井恒道,山田守,松原弘美,白柳格,轻金属,1988;38:5153菅沼克昭,藤田辉昭,新原皓一,铃本信幸.铁钢,1989;75:15344土取功,新田明,原信彦,原田秀文.铁钢.1989;75:15265土取功,福永秀春.日本金属学会志,1992;56:3336菅沼克昭.轻金属,1992;42:52 |
|