| 喷雾沉积高硅ZA27合金的组织与性能 |
| 杨留栓;庞礼军;杨根仓;周尧和 |
| 西北工业大学凝固技术国家重点实验室 |
|
| MICROSTRUCTURE AND PROPERTIES OF HIGH Si ALLOY ZA27 PRODUCED BY SPRAY DEPOSITION |
| YANG Liushuan; PANGLijun;YANG Gencang; ZHOU Yaohe (State Key Laboratory of Solidification Processing; Northwestern Polytechnical University;Xi'an; 710072) |
引用本文:
杨留栓;庞礼军;杨根仓;周尧和. 喷雾沉积高硅ZA27合金的组织与性能[J]. 金属学报, 1995, 31(6): 254-260.
,
,
,
.
MICROSTRUCTURE AND PROPERTIES OF HIGH Si ALLOY ZA27 PRODUCED BY SPRAY DEPOSITION[J]. Acta Metall Sin, 1995, 31(6): 254-260.
| 1GervaisE.In:LewisGB,BarnhurstRJ,LoonCAeds.,25thAunnalConferenceofMetallurgists—1986ProceedingsInternationalSymposiumonZinc-Aluminum(ZA)castingAllovs,1986:12曾松岩,段守坤,蒋祖龄,李庆春,孙阳.铸造技术,1991;(5):203李元元,罗俊明,邓灿坤,罗宗强,肖志瑜.广州机电,1992;(1):104DellisMA,keusermansJP,DelannayF.MaterSciEng,1991;A135:2535LoSHJ,DionneS,SahooM,HawthorneHW.JMaterSci,1992;27:56816朱明芳,张力宁,王仕勤,王楠,舒光冀.机械工程材料,1993;17(2):327MykuraN.MurphyS.In:LewisGB,BarnhurstRJ,LoonCAeds.,25thAunnalConferenceofMetallurgists—1986ProceedingsInternationalSymposiumonZinc-Aluminum(ZA)CastingAlloys,1986:45 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|