| 一种镍基高温合金的高温HCl腐蚀行为 |
周一鸣1,2, 韩勇军3, 谢光2( ), 郑伟2, 肖炎彬3, 潘阳3, 张健2( ) |
1 中国科学技术大学 材料科学与工程学院 沈阳 110016 2 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 3 中国船舶集团有限公司第七〇五研究所 西安 710077 |
|
| High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere |
ZHOU Yiming1,2, HAN Yongjun3, XIE Guang2( ), ZHENG Wei2, XIAO Yanbin3, PAN Yang3, ZHANG Jian2( ) |
1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3 The 705 Research Institute of China State Shipbuilding Corporation Limited, Xi'an 710077, China |
引用本文:
周一鸣, 韩勇军, 谢光, 郑伟, 肖炎彬, 潘阳, 张健. 一种镍基高温合金的高温HCl腐蚀行为[J]. 金属学报, 2025, 61(5): 770-782.
Yiming ZHOU,
Yongjun HAN,
Guang XIE,
Wei ZHENG,
Yanbin XIAO,
Yang PAN,
Jian ZHANG.
High-Temperature Corrosion Behavior of a Nickel-Based Superalloy in HCl-Containing Atmosphere[J]. Acta Metall Sin, 2025, 61(5): 770-782.
| 1 |
Guo J T. Materials Science and Engineering for Superalloys (I) [M]. Beijing: Science Press, 2008: 4
|
| 1 |
郭建亭. 高温合金材料学 (上册) [M]. 北京: 科学出版社, 2008: 4
|
| 2 |
Zhang J, Wang L, Xie G, et al. Recent progress in research and development of nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2023, 59: 1109
doi: 10.11900/0412.1961.2023.00140
|
| 2 |
张 健, 王 莉, 谢 光 等. 镍基单晶高温合金的研发进展 [J]. 金属学报, 2023, 59: 1109
|
| 3 |
Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 372
|
| 4 |
Li M S. High Temperature Corrosion of Metals [M]. Beijing: Metallurgical Industry Press, 2001: 36
|
| 4 |
李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 36
|
| 5 |
Chang J X, Wang D, Liu T, et al. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy [J]. Corros. Sci., 2015, 98: 585
|
| 6 |
Park S J, Seo S M, Yoo Y S, et al. Effects of Al and Ta on the high temperature oxidation of Ni-based superalloys [J]. Corros. Sci., 2015, 90: 305
|
| 7 |
Chang J X, Wang D, Zhang G, et al. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys [J]. Corros. Sci., 2017, 117: 35
|
| 8 |
Nielsen H P, Frandsen F J, Dam-Johansen K. Lab-scale investigations of high-temperature corrosion phenomena in straw-fired boilers [J]. Energy Fuels, 1999, 13: 1114
|
| 9 |
Zhu R Z, Zuo Y, Guo M J. An approach to mechanism of internal sulphidation-internal oxidation during hot corrosion of Ni-base alloy [J]. Acta Metall. Sin., 1985, 21(6): 39
|
| 9 |
朱日彰, 左 禹, 郭曼玖. 镍基高温合金热腐蚀过程中内硫化-内氧化机制的探讨 [J]. 金属学报, 1985, 21(6): 39
|
| 10 |
Rapp R A. Hot corrosion of materials: A fluxing mechanism? [J]. Corros. Sci., 2002, 44: 209
|
| 11 |
Sato Y, Hara M, Masuda K. High temperature oxidation of laser surface treated Fe-Cr alloys in HCl-containing atmosphere [J]. Mater. Chem. Phys., 1998, 54: 186
|
| 12 |
Sato Y, Young D J. High-temperature corrosion of iron at 900 oC in atmospheres containing HCl and H2O [J]. Oxid. Met., 2001, 55: 243
|
| 13 |
Stott F H, Shih C Y. High-temperature corrosion of iron-chromium alloys in oxidizing-chloridizing conditions [J]. Oxid. Met., 2000, 54: 425
|
| 14 |
Nimmervoll M, Schmid A, Mori G, et al. Surface sulphide formation on high-temperature corrosion resistant alloys in a H2S-HCl-CO2 mixed atmosphere [J]. Corros. Sci., 2021, 181: 109241
|
| 15 |
Metsäjoki J, Huttunen-Saarivirta E, Lepistö T. Corrosion of aluminized and uncoated 9-12% Cr boiler steels in simulated biomass and waste combustion conditions [J]. High Temp. Mater. Process., 2011, 30: 181
|
| 16 |
Metsäjoki J, Huttunen-Saarivirta E, Lepistö T. Oxidation of uncoated and aluminized 9-12% Cr boiler steels at 550-650 oC [J]. J. Mater. Eng. Perform., 2011, 20: 298
|
| 17 |
Żurek J, Wessel E, Niewolak L, et al. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550-650 oC [J]. Corros. Sci., 2004, 46: 2301
|
| 18 |
Parlikar C, Alam Z, Chatterjee D, et al. Oxidation and concomitant effects on the microstructure and high temperature tensile properties of a DS Ni-base superalloy applied with different thicknesses of Pt-aluminide (PtAl) bond coat [J]. Surf. Coat. Technol., 2019, 373: 25
|
| 19 |
Litz J, Rahmel A, Schorr M. Selective carbide oxidation and internal nitridation of the Ni-base superalloys IN 738 LC and IN 939 in air [J]. Oxid. Met., 1988, 30: 95
|
| 20 |
Abels J M, Strehblow H H. A surface analytical approach to the high temperature chlorination behaviour of Inconel 600 at 700 oC [J]. Corros. Sci., 1997, 39: 115
|
| 21 |
Grabke H J, Reese E, Spiegel M. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits [J]. Corros. Sci., 1995, 37: 1023
|
| 22 |
Ning L K, Zheng Z, Tan Y, et al. Study on hot corrosion resistance of a new directional solidification Ni-based superalloy [J]. Acta Metall. Sin., 2009, 45: 161
|
| 22 |
宁礼奎, 郑 志, 谭 毅 等. 一种新型定向凝固镍基高温合金抗热腐蚀性能的研究 [J]. 金属学报, 2009, 45: 161
|
| 23 |
Central South University Department of Metallurgy. Chlorine Metallurgy [M]. Beijing: Metallurgical Industry Press, 1978: 29
|
| 23 |
中南矿冶学院冶金研究室. 氯化冶金 [M]. 北京: 冶金工业出版社, 1978: 29
|
| 24 |
Qiu K Q, Duan W J, Chen Q Y. Rate of metal evaporation under vacuum condition [J]. Nonferrous Met., 2002, 54(2): 48
|
| 24 |
丘克强, 段文军, 陈启元. 金属在真空状态下的蒸发速率 [J]. 有色金属, 2002, 54(2): 48
|
| 25 |
Ye X J, Yang B B, Lai R L, et al. Effect of Nb addition on the internal oxidation of novel Ni-base superalloy [J]. Corros. Sci., 2022, 198: 110100
|
| 26 |
Giggins C S, Pettit F S. Oxidation of Ni-Cr-Al alloys between 1000 oC and 1200 oC [J]. J. Electrochem. Soc., 1971, 118: 1782
|
| 27 |
Deepak K, Mandal S, Athreya C N, et al. Implication of grain boundary engineering on high temperature hot corrosion of alloy 617 [J]. Corros. Sci., 2016, 106: 293
|
| 28 |
Athreya C N, Deepak K, Kim D I, et al. Role of grain boundary engineered microstructure on high temperature steam oxidation behaviour of Ni based superalloy alloy 617 [J]. J. Alloys Compd., 2019, 778: 224
|
| 29 |
Stearns C A, Kohl F J, Fryburg G C. Oxidative vaporization kinetics of Cr2O3 in oxygen from 1000° to 1300 oC [J]. J. Electrochem. Soc., 1974, 121: 945
|
| 30 |
Ren W L, Ouyang F F, Ding B, et al. The influence of CrTaO4 layer on the oxidation behavior of a directionally-solidified nickel-based superalloy at 850-900 oC [J]. J. Alloys Compd., 2017, 724: 565
|
| 31 |
Li D S, Chen G, Li D, et al. Oxidation resistance of nickel-based superalloy Inconel 600 in air at different temperatures [J]. Rare Met., 2021, 40: 3235
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|