| Yb含量对Mg-Gd-Y-Zn-Zr合金微观组织与力学性能的影响 |
王升1, 朱彦丞1, 潘虎成1( ), 李景仁1, 曾志浩1, 秦高梧1,2( ) |
1 东北大学 材料科学与工程学院 材料各向异性与织构教育部重点实验室 沈阳 110819 2 沈阳化工大学 战略材料与部件研究中心 沈阳 110142 |
|
| Effect of Yb Content on Microstructure and Mechanical Property of Mg-Gd-Y-Zn-Zr Alloy |
WANG Sheng1, ZHU Yancheng1, PAN Hucheng1( ), LI Jingren1, ZENG Zhihao1, QIN Gaowu1,2( ) |
1 Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), College of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 2 Research Center for Strategic Materials and Components, Shenyang University of Chemical Technology, Shenyang 110142, China |
引用本文:
王升, 朱彦丞, 潘虎成, 李景仁, 曾志浩, 秦高梧. Yb含量对Mg-Gd-Y-Zn-Zr合金微观组织与力学性能的影响[J]. 金属学报, 2025, 61(3): 499-508.
Sheng WANG,
Yancheng ZHU,
Hucheng PAN,
Jingren LI,
Zhihao ZENG,
Gaowu QIN.
Effect of Yb Content on Microstructure and Mechanical Property of Mg-Gd-Y-Zn-Zr Alloy[J]. Acta Metall Sin, 2025, 61(3): 499-508.
| 1 |
Zheng X B, Du W B, Wang Z H, et al. Remarkably enhanced mechanical properties of Mg-8Gd-1Er-0.5Zr alloy on the route of extrusion, rolling and aging [J]. Mater. Lett., 2018, 212: 155
|
| 2 |
Wang S, Pan H C, Xie D S, et al. Grain refinement and strength enhancement in Mg wrought alloys: A review [J]. J. Magnes. Alloy., 2023, 11: 4128
|
| 3 |
You S H, Huang Y D, Kainer K U, et al. Recent research and developments on wrought magnesium alloys [J]. J. Magnes. Alloy., 2017, 5: 239
|
| 4 |
Pan F S, Jiang B. Development and application of plastic processing technologies of magnesium alloys [J]. Acta Metall. Sin., 2021, 57: 1362
doi: 10.11900/0412.1961.2021.00349
|
| 4 |
潘复生, 蒋 斌. 镁合金塑性加工技术发展及应用 [J]. 金属学报, 2021, 57: 1362
doi: 10.11900/0412.1961.2021.00349
|
| 5 |
Zha M, Wang S Q, Fang Y, et al. Advancement in research of rolled magnesium alloys with high performance [J]. J. Netshape Form. Eng., 2020, 12(5): 20
|
| 5 |
查 敏, 王思清, 方 圆 等. 高性能轧制镁合金研究进展 [J]. 精密成形工程, 2020, 12(5): 20
|
| 6 |
Ding W J, Zeng X Q. Research and applications of magnesium in China [J]. Acta Metall. Sin., 2010, 46: 1450
|
| 6 |
丁文江, 曾小勤. 中国Mg材料研发与应用 [J]. 金属学报, 2010, 46: 1450
doi: 10.3724/SP.J.1037.2010.00386
|
| 7 |
Li J R, Xie D S, Zhang D D, et al. Microstructure evolution mechanism of new low-alloyed high-strength Mg-0.2Ce-0.2Ca alloy during extrusion [J]. Acta Metall. Sin., 2023, 59: 1087
|
| 7 |
李景仁, 谢东升, 张栋栋 等. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理 [J]. 金属学报, 2023, 59: 1087
doi: 10.11900/0412.1961.2022.00290
|
| 8 |
Wu G H, Tong X, Jiang R, et al. Grain refinement of as-cast Mg-RE alloys: Research progress and future prospect [J]. Acta Metall. Sin., 2022, 58: 385
doi: 10.11900/0412.1961.2021.00519
|
| 8 |
吴国华, 童 鑫, 蒋 锐 等. 铸造Mg-RE合金晶粒细化行为研究现状与展望 [J]. 金属学报, 2022, 58: 385
doi: 10.11900/0412.1961.2021.00519
|
| 9 |
Nie J F. Precipitation and hardening in magnesium alloys [J]. Metall. Mater. Trans., 2012, 43A: 3891
|
| 10 |
Li X, Qi W, Zheng K, et al. Enhanced strength and ductility of Mg-Gd-Y-Zr alloys by secondary extrusion [J]. J. Magnes. Alloy., 2013, 1: 54
|
| 11 |
Qin G W, Xie H B, Pan H C, et al. A new class of ordered structure between crystals and quasicrystals [J]. Acta Metall. Sin., 2018, 54: 1490
doi: 10.11900/0412.1961.2018.00357
|
| 11 |
秦高梧, 谢红波, 潘虎成 等. 一类介于晶体与准晶体之间的有序结构 [J]. 金属学报, 2018, 54: 1490
doi: 10.11900/0412.1961.2018.00357
|
| 12 |
Xu C, Zheng M Y, Xu S W, et al. Ultra high-strength Mg-Gd-Y-Zn-Zr alloy sheets processed by large-strain hot rolling and ageing [J]. Mater. Sci. Eng., 2012, A547: 93
|
| 13 |
Zeng X Q, Wu Y J, Peng L M, et al. LPSO structure and aging phases in Mg-Gd-Zn-Zr alloy [J]. Acta Metall. Sin., 2010, 46: 1041
|
| 13 |
曾小勤, 吴玉娟, 彭立明 等. Mg-Gd-Zn-Zr合金中的LPSO结构和时效相 [J]. 金属学报, 2010, 46: 1041
doi: 10.3724/SP.J.1037.2009.00833
|
| 14 |
Fan M Y, Cui Y, Zhang Y, et al. Achieving high strength-ductility synergy in a Mg97Y1Zn1Ho1 alloy via a nano-spaced long-period stacking-ordered phase [J]. J. Magnes. Alloy., 2023, 11: 1321
|
| 15 |
Zhang D D, Yang S, Meng F Z, et al. Compressive creep behavior of extruded Mg-4Sm-2Yb-0.6Zn-0.4Zr alloy [J]. Mater. Sci. Eng., 2021, A809: 140929
|
| 16 |
Matsuda M, Ando S, Nishida M. Dislocation structure in rapidly solidified Mg97Zn1Y2 alloy with long period stacking order phase [J]. Mater. Trans., 2005, 46: 361
|
| 17 |
Tong L B, Chu J H, Sun W T, et al. Achieving an ultra-high strength and moderate ductility in Mg-Gd-Y-Zn-Zr alloy via a decreased-temperature multi-directional forging [J]. Mater. Charact., 2021, 171: 110804
|
| 18 |
Zhang D D, Zhang D P, Bu F Q, et al. Excellent ductility and strong work hardening effect of as-cast Mg-Zn-Zr-Yb alloy at room temperature [J]. J. Alloy. Compd., 2017, 728: 404
|
| 19 |
Xie H, Wu G H, Zhang X L, et al. The role of Yb content on the microstructural evolution and mechanical characteristics of cast Mg-9Gd-0.5Zn-0.2Zr alloy [J]. Mater. Sci. Eng., 2021, A817: 141292
|
| 20 |
Yu Z J, Xu C, Meng J, et al. Microstructure evolution and mechanical properties of a high strength Mg-11.7Gd-4.9Y-0.3Zr (wt%) alloy prepared by pre-deformation annealing, hot extrusion and ageing [J]. Mater. Sci. Eng., 2017, A703: 348
|
| 21 |
Yan Z X, Yang Q, Ma R, et al. Effects of Sm addition on microstructure evolutions and mechanical properties of high-strength Mg-Gd-Sm-Zr extruded alloys [J]. Mater. Sci. Eng., 2022, A831: 142264
|
| 22 |
Yan Z H, Yu Y D, Qian J H, et al. Fabrication of high-strength Mg-Gd-Nd-Zn-Sn-Zr alloy via extrusion and aging [J]. Met. Mater. Int., 2021, 27: 4182
|
| 23 |
Liu Y H, Zhang Z R, Wang J, et al. A novel Mg-Gd-Y-Zn-Cu-Ni alloy with excellent combination of strength and dissolution via peak-aging treatment [J]. J. Magnes. Alloy., 2023, 11: 720
|
| 24 |
Xue Z Y, Ren Y J, Luo W B, et al. Effect of aging treatment on the precipitation behavior and mechanical properties of Mg-9Gd-3Y-1.5Zn-0.5Zr alloy [J]. J. Mater. Eng. Perform., 2017, 26: 5963
|
| 25 |
Zhang Y, Rong W, Wu Y J, et al. Achieving ultra-high strength in Mg-Gd-Ag-Zr wrought alloy via bimodal-grained structure and enhanced precipitation [J]. J. Mater. Sci. Technol., 2020, 54: 160
doi: 10.1016/j.jmst.2020.04.031
|
| 26 |
Zhang D D, Liu C M, Jiang S N, et al. Effects of extrusion process on microstructure, precipitates and mechanical properties of Mg-Gd-Y-Zr-Ag alloys [J]. Mater. Sci. Eng., 2022, A856: 143990
|
| 27 |
Wang K, Wang J F, Dou X X, et al. Microstructure and mechanical properties of large-scale Mg-Gd-Y-Zn-Mn alloys prepared through semi-continuous casting [J]. J. Mater. Sci. Technol., 2020, 52: 72
doi: 10.1016/j.jmst.2020.04.013
|
| 28 |
Liu H, Bai J, Yan K, et al. Comparative studies on evolution behaviors of 14H LPSO precipitates in as-cast and as-extruded Mg-Y-Zn alloys during annealing at 773K [J]. Mater. Des., 2016, 93: 9
|
| 29 |
Fan T W, Tang B Y, Peng L M, et al. First-principles study of long-period stacking ordered-like multi-stacking fault structures in pure magnesium [J]. Scr. Mater., 2011, 64: 942
|
| 30 |
Mansoor A, Du W B, Yu Z J, et al. Improved mechanical performance of double-pass extruded Mg-Gd-Er-Zr alloys with various rare earth contents [J]. Mater. Sci. Eng., 2022, A840: 142922
|
| 31 |
Li S J, Jin J F, Song Y H, et al. Multimodal microstructure of Mg-Gd-Y alloy through an integrated simulation of “process-structure-property” [J]. Acta Metall. Sin., 2022, 58: 114
|
| 31 |
李少杰, 金剑锋, 宋宇豪 等. “工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织 [J]. 金属学报, 2022, 58: 114
doi: 10.11900/0412.1961.2021.00222
|
| 32 |
Luo J, Yan H, Lu L W, et al. Cold rollability improvement by twinning and twin-slip synergy in an Mg-Zn-Gd alloy with rare earth texture [J]. J. Alloys Compd., 2021, 883: 160813
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|