| 四元Co-Ni-Cr-Al合金高温氧化模式及其转变机理 |
吕云蕾1, 任延杰1,2( ), 冯抗抗1, 周梦妮1, 王文3, 陈荐1, 牛焱1( ) |
1 长沙理工大学 能源与动力工程学院 长沙 410076 2 浙江科技大学 机械与能源工程学院 杭州 310023 3 中国科学院金属研究所 沈阳 110016 |
|
| High Temperature Oxidation Mode and Transformation Mechanism of Quaternary Co-Ni-Cr-Al Alloys |
LV Yunlei1, REN Yanjie1,2( ), FENG Kangkang1, ZHOU Mengni1, WANG Wen3, CHEN Jian1, NIU Yan1( ) |
1 College of Energy and Power Engineering, Changsha University of Science and Technology, Changsha 410076, China 2 School of Mechanical and Energy Engineering, Zhejiang University of Science and Technology, Hangzhou 310023, China 3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
吕云蕾, 任延杰, 冯抗抗, 周梦妮, 王文, 陈荐, 牛焱. 四元Co-Ni-Cr-Al合金高温氧化模式及其转变机理[J]. 金属学报, 2024, 60(7): 947-956.
Yunlei LV,
Yanjie REN,
Kangkang FENG,
Mengni ZHOU,
Wen WANG,
Jian CHEN,
Yan NIU.
High Temperature Oxidation Mode and Transformation Mechanism of Quaternary Co-Ni-Cr-Al Alloys[J]. Acta Metall Sin, 2024, 60(7): 947-956.
| 1 |
Young D J. High Temperature Oxidation and Corrosion of Metals [M]. 2nd Ed., Amsterdam: Elsevier, 2016: 1
|
| 2 |
Lai G Y. High-Temperature Corrosion and Materials Applications [M]. ASM International, 2007: 6
|
| 3 |
Yuan F H, Sun X F, Guan H R, et al. Cyclic oxidation behavior of a cobalt-base superalloy [J]. J. Chin. Soc. Corros. Prot., 2002, 22: 115
|
| 3 |
袁福河, 孙晓峰, 管恒荣 等. 钴基高温合金的循环氧化行为研究 [J]. 中国腐蚀与防护学报, 2002, 22: 115
|
| 4 |
Hou P Y. Impurity effects on alumina scale growth [J]. J. Am. Ceram. Soc., 2003, 86: 660
|
| 5 |
Stott F H, Wood G C, Stringer J. The influence of alloying elements on the development and maintenance of protective scales [J]. Oxid. Met., 1995, 44: 113
|
| 6 |
Wallwork G R, Hed A Z. Mapping of the oxidation products in the ternary Co-Cr-Al system [J]. Oxid. Met., 1971, 3: 213
|
| 7 |
Wallwork G R, Hed A Z. Selection of an alloy composition in the ternary Co-Cr-Al system for oxidation resistance [J]. Oxid. Met., 1971, 3: 243
|
| 8 |
Wood G C, Stott F H. The influence of aluminum additions on the oxidation of Co-Cr alloys at 1000 and 1200oC [J]. Oxid. Met., 1971, 3: 365
|
| 9 |
Irving G N, Stringer J, Whittle D P. The oxidation behavior of Co-Cr-Al alloys at 1000oC [J]. Corrosion, 1977, 33: 56
|
| 10 |
Allam I M, Whittle D P, Stringer J. The oxidation behavior of CoCrAl systems containing active element additions [J]. Oxid. Met., 1978, 12: 35
|
| 11 |
Stott F H, Wood G C, Hobby M G. A comparison of the oxidation behavior of Fe-Cr-Al, Ni-Cr-Al, and Co-Cr-Al alloys [J]. Oxid. Met., 1971, 3: 103
|
| 12 |
Stott F H, Wood G C. The mechanism of oxidation of Ni-Cr-Al alloys at 1000oC-1200oC [J]. Corros. Sci., 1971, 11: 799
|
| 13 |
Giggins C S, Pettit F S. Oxidation of Ni-Cr-Al alloys between 1000℃ and 1200℃ [J]. J. Electrochem. Soc., 1971, 118: 1782
|
| 14 |
Kvernes I A, Kofstad P. The oxidation behavior of some Ni-Cr-Al alloys at high temperatures [J]. Mater. Trans., 1972, 3B: 1511
|
| 15 |
Nijdam T J, Jeurgens L P H, Sloof W G. Effect of partial oxygen pressure on the initial stages of high-temperature oxidation of γ-NiCrAl alloys [J]. Mater. High Temp., 2003, 20: 311
|
| 16 |
Nijdam T J, Jeurgens L P H, Sloof W G. Modelling the thermal oxidation of ternary alloys—Compositional changes in the alloy and the development of oxide phases [J]. Acta Mater., 2003, 51: 5295
|
| 17 |
Nijdam T J, Jeurgens L P H, Sloof W G. Promoting exclusive α-Al2O3 growth upon high-temperature oxidation of NiCrAl alloys: Experiment versus model predictions [J]. Acta Mater., 2005, 53: 1643
|
| 18 |
Nijdam T J, Van Der Pers N M, Sloof W G. Oxide phase development upon high temperature oxidation of γ-NiCrAl alloys [J]. Mater. Corros., 2006, 57: 269
|
| 19 |
Wang E P, Liu H F, Guo W, et al. Effect of pre-oxidation temperature on high-temperature cyclic oxidation resistance of Ni-15Cr-5Al-5Si alloy [J]. Mater. Mech. Eng., 2019, 43(2): 39
doi: 10.11973/jxgccl201902008
|
| 19 |
王二鹏, 刘海飞, 郭 文 等. 预氧化温度对Ni-15Cr-5Al-5Si合金抗高温循环氧化性能的影响 [J]. 机械工程材料, 2019, 43(2): 39
doi: 10.11973/jxgccl201902008
|
| 20 |
Niu Y, Zhang X J, Wu Y, et al. The third-element effect in the oxidation of Ni-xCr-7Al (x=0, 5, 10, 15 at.%) alloys in 1 atm O2 at 900-1000oC [J]. Corros. Sci., 2006, 48: 4020
|
| 21 |
Zhang X J, Wang S Y, Gesmundo F, et al. The effect of Cr on the oxidation of Ni-10 at% Al in 1 atm O2 at 900-1000oC [J]. Oxid. Met., 2006, 65: 151
|
| 22 |
Wood G C. Fundamental factors determining the mode of scaling of heat-resistant alloys [J]. Werkst. Corros., 1971, 22: 491
|
| 23 |
Weiser M, Galetz M C, Chater R J, et al. Growth mechanisms of oxide scales on two-phase Co/Ni-base model alloys between 800oC and 900oC [J]. J. Electrochem. Soc., 2020, 167: 021504
|
| 24 |
Weiser M, Galetz M C, Zschau H E, et al. Influence of Co to Ni ratio in γ′-strengthened model alloys on oxidation resistance and the efficacy of the halogen effect at 900oC [J]. Corros. Sci., 2019, 156: 84
|
| 25 |
Gao B, Wang L, Liu Y, et al. High temperature oxidation behaviour of γ′-strengthened Co-based superalloys with different Ni addition [J]. Corros. Sci., 2019, 157: 109
doi: 10.1016/j.corsci.2019.05.036
|
| 26 |
Zenk C H, Neumeier S, Engl N M, et al. Intermediate Co/Ni-base model superalloys—Thermophysical properties, creep and oxidation [J]. Scr. Mater., 2016, 112: 83
|
| 27 |
Bastow B D, Whittle D P, Wood G C. Diffusion-controlled growth of solid solution scales on nickel-cobalt alloys [J]. Corros. Sci., 1976, 16: 57
|
| 28 |
Seraffon M, Simms N J, Sumner J, et al. The development of new bond coat compositions for thermal barrier coating systems operating under industrial gas turbine conditions [J]. Surf. Coat. Technol., 2011, 206: 1529
|
| 29 |
Seraffon M, Simms N J, Sumner J, et al. Oxidation behaviour of NiCrAl and NiCoCrAl bond coatings under industrial gas turbine conditions [J]. Oxid. Met., 2014, 81: 203
|
| 30 |
Ren Y J, Dai T, Guo X H, et al. Scaling behavior of four Co-20Ni-xCr-yAl (x = 8, 15 wt.%; y = 3, 5 wt.%) alloys exposed to 1 atm O2 at 1000oC and 1100oC [J]. Corros. Sci., 2021, 191: 109719
|
| 31 |
Ren Y J, Lv Y L, Dai T, et al. Oxidation behavior of ternary alloys Co-20Ni-3Al and Co-20Ni-5Al in 105 Pa O2 atmosphere at 800-1000oC [J]. J. Chin. Soc. Corros. Prot., 2022, 42: 995
|
| 31 |
任延杰, 吕云蕾, 戴 汀 等. 三元Co-Ni-Al合金在800~1000℃纯氧中的氧化行为研究 [J]. 中国腐蚀与防护学报, 2022, 42: 995
doi: 10.11902/1005.4537.2021.264
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|