| 稀土元素La对AlMgSi合金性能和微结构的影响 |
郑雄1, 赖玉香2( ), 向雪梅1, 陈江华2 |
1 湖南大学 材料科学与工程学院 长沙 410082 2 海南大学 精密仪器高等研究中心 皮米电镜中心 海口 570228 |
|
| Impacts of Rare Earth Element La on Properties and Microstructure of AlMgSi Alloys |
ZHENG Xiong1, LAI Yuxiang2( ), XIANG Xuemei1, CHEN Jianghua2 |
1 College of Materials Science and Engineering, Hunan University, Changsha 410082, China 2 Pico Electron Microscopy Center, Center for Advanced Studies in Precision Instruments, Hainan University, Haikou 570228, China |
引用本文:
郑雄, 赖玉香, 向雪梅, 陈江华. 稀土元素La对AlMgSi合金性能和微结构的影响[J]. 金属学报, 2024, 60(1): 107-116.
Xiong ZHENG,
Yuxiang LAI,
Xuemei XIANG,
Jianghua CHEN.
Impacts of Rare Earth Element La on Properties and Microstructure of AlMgSi Alloys[J]. Acta Metall Sin, 2024, 60(1): 107-116.
| 1 |
Williams J C, Starke Jr E A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775
doi: 10.1016/j.actamat.2003.08.023
|
| 2 |
Pantelakis S G, Alexopoulos N D. Assessment of the ability of conventional and advanced wrought aluminum alloys for mechanical performance in light-weight applications [J]. Mater. Des., 2008, 29: 80
doi: 10.1016/j.matdes.2006.12.004
|
| 3 |
Zandbergen H W, Andersen S J, Jansen J. Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies [J]. Science, 1997, 277: 1221
doi: 10.1126/science.277.5330.1221
|
| 4 |
Murayama M, Hono K. Pre-precipitate clusters and precipitation processes in Al-Mg-Si alloys [J]. Acta Mater., 1999, 47: 1537
doi: 10.1016/S1359-6454(99)00033-6
|
| 5 |
Chen J H, Costan E, van Huis M A, et al. Atomic pillar-based nanoprecipitates strengthen AlMgSi alloys [J]. Science, 2006, 312: 416
pmid: 16627740
|
| 6 |
Vissers R, van Huis M A, Jansen J, et al. The crystal structure of the β' phase in Al-Mg-Si alloys [J]. Acta Mater., 2007, 55: 3815
doi: 10.1016/j.actamat.2007.02.032
|
| 7 |
Chen H N, Lu J B, Kong Y, et al. Atomic scale investigation of the crystal structure and interfaces of the B' precipitate in Al-Mg-Si alloys [J]. Acta Mater., 2020, 185: 193
doi: 10.1016/j.actamat.2019.11.059
|
| 8 |
Andersen S J, Marioara C D, Vissers R, et al. The structural relation between precipitates in Al-Mg-Si alloys, the Al-matrix and diamond silicon, with emphasis on the trigonal phase U1-MgAl2Si2 [J]. Mater. Sci. Eng., 2007, A444: 157
|
| 9 |
Andersen S J, Marioara C D, Frøseth A, et al. Crystal structure of the orthorhombic U2-Al4Mg4Si4 precipitate in the Al-Mg-Si alloy system and its relation to the β' and β" phases [J]. Mater. Sci. Eng., 2005, A390: 127
|
| 10 |
Lai Y X, Jiang B C, Liu C H, et al. Low-alloy-correlated reversal of the precipitation sequence in Al-Mg-Si alloys [J]. J. Alloys Compd., 2017, 701: 94
doi: 10.1016/j.jallcom.2017.01.095
|
| 11 |
Lai Y X, Fan W, Yin M J, et al. Structures and formation mechanisms of dislocation-induced precipitates in relation to the age-hardening responses of Al-Mg-Si alloys [J]. J. Mater. Sci. Technol., 2020, 41: 127
doi: 10.1016/j.jmst.2019.11.001
|
| 12 |
Hirth S M, Marshall G J, Court S A, et al. Effects of Si on the aging behaviour and formability of aluminium alloys based on AA6016 [J]. Mater. Sci. Eng., 2001, A319-321: 452
|
| 13 |
Jin M, Li J, Shao G J. The effects of Cu addition on the microstructure and thermal stability of an Al-Mg-Si alloy [J]. J. Alloys Compd., 2007, 437: 146
doi: 10.1016/j.jallcom.2006.07.113
|
| 14 |
Xiao Q, Liu H Q, Yi D Q, et al. Effect of Cu content on precipitation and age-hardening behavior in Al-Mg-Si-xCu alloys [J]. J. Alloys Compd., 2017, 695: 1005
doi: 10.1016/j.jallcom.2016.10.221
|
| 15 |
Saito T, Wenner S, Osmundsen E, et al. The effect of Zn on precipitation in Al-Mg-Si alloys [J]. Philos. Mag., 2014, 94: 2410
doi: 10.1080/14786435.2014.913819
|
| 16 |
Saito T, Ehlers F J H, Lefebvre W, et al. HAADF-STEM and DFT investigations of the Zn-containing β" phase in Al-Mg-Si alloys [J]. Acta Mater., 2014, 78: 245
doi: 10.1016/j.actamat.2014.06.055
|
| 17 |
Jiao N N, Lai Y X, Chen S L, et al. Atomic-scale roles of Zn element in age-hardened AlMgSiZn alloys [J]. J. Mater. Sci. Technol., 2021, 70: 105
doi: 10.1016/j.jmst.2020.09.009
|
| 18 |
Mørtsell E A, Marioara C D, Andersen S J, et al. Effects of germanium, copper, and silver substitutions on hardness and microstructure in lean Al-Mg-Si alloys [J]. Metall. Mater. Trans., 2015, 46A: 4369
|
| 19 |
Mørtsell E A, Andersen S J, Friis J, et al. Atomistic details of precipitates in lean Al-Mg-Si alloys with trace additions of Ag and Ge studied by HAADF-STEM and DFT [J]. Philos. Mag., 2017, 97: 851
doi: 10.1080/14786435.2017.1281461
|
| 20 |
Mørtsell E A, Marioara C D, Andersen S J, et al. The effects and behaviour of Li and Cu alloying agents in lean Al-Mg-Si alloys [J]. J. Alloys Compd., 2017, 699: 235
doi: 10.1016/j.jallcom.2016.12.273
|
| 21 |
Liu Y, Lai Y X, Chen Z Q, et al. Formation of β"-related composite precipitates in relation to enhanced thermal stability of Sc-alloyed Al-Mg-Si alloys [J]. J. Alloys Compd., 2021, 885: 160942
doi: 10.1016/j.jallcom.2021.160942
|
| 22 |
Xiang X M, Lai Y X, Liu C H, et al. Sn-induced modification of the precipitation pathways upon high-temperature ageing in an Al-Mg-Si alloy [J]. Acta Metall. Sin., 2018, 54: 1273
doi: 10.11900/0412.1961.2018.00125
|
| 22 |
向雪梅, 赖玉香, 刘春辉 等. 微合金化元素Sn对Al-Mg-Si合金高温时效强化相析出路径的改变 [J]. 金属学报, 2018, 54: 1273
doi: 10.11900/0412.1961.2018.00125
|
| 23 |
Wen S P, Xing Z B, Huang H, et al. The effect of erbium on the microstructure and mechanical properties of Al-Mg-Mn-Zr alloy [J]. Mater. Sci. Eng., 2009, A516: 42
|
| 24 |
Yao D M, Xia Y M, Qiu F, et al. Effects of La addition on the elevated temperature properties of the casting Al-Cu alloy [J]. Mater. Sci. Eng., 2011, A528: 1463
|
| 25 |
Zheng Q J, Zhang L L, Jiang H X, et al. Effect mechanisms of micro-alloying element La on microstructure and mechanical properties of hypoeutectic Al-Si alloys [J]. J. Mater. Sci. Technol., 2020, 47: 142
doi: 10.1016/j.jmst.2019.12.021
|
| 26 |
Zheng Q J, Wu J, Jiang H X, et al. Effect of micro-alloying element La on corrosion behavior of Al-Mg-Si alloys [J]. Corros. Sci., 2021, 179: 109113
doi: 10.1016/j.corsci.2020.109113
|
| 27 |
Chang C H, Lee S L, Hsu T Y, et al. Impact of Cu/Mg ratio on thermal stability of hot extrusion of Al-4.6 pct Cu-Mg-Ag alloys [J]. Metall. Mater. Trans., 2007, 38A: 2832
|
| 28 |
Wang T M, Zhao Y F, Chen Z N, et al. The bimodal effect of La on the microstructures and mechanical properties of in-situ A356-TiB2 composites [J]. Mater. Des., 2015, 85: 724
doi: 10.1016/j.matdes.2015.07.031
|
| 29 |
Jiang H X, Li S X, Zheng Q J, et al. Effect of minor lanthanum on the microstructures, tensile and electrical properties of Al-Fe alloys [J]. Mater. Des., 2020, 195: 108991
doi: 10.1016/j.matdes.2020.108991
|
| 30 |
Sankaran K K, O'neal J E, Sastry S M L. Effects of second-phase dispersoids on deformation behavior of Al-Li alloys [J]. Metall. Trans., 1983, 14A: 2174
|
| 31 |
Liu G, Zhang G J, Ding X D, et al. The influences of multiscale-sized second-phase particles on ductility of aged aluminum alloys [J]. Metall. Mater. Trans., 2004, 35A: 1725
|
| 32 |
Liu G, Zhang G J, Wang R H, et al. Heat treatment-modulated coupling effect of multi-scale second-phase particles on the ductile fracture of aged aluminum alloys [J]. Acta Mater., 2007, 55: 273
doi: 10.1016/j.actamat.2006.08.026
|
| 33 |
Nellist P D, Pennycook S J. The principles and interpretation of annular dark-field Z-contrast imaging [J]. Adv. Imaging Electron Phys., 2000, 113: 147
|
| 34 |
Yang W C, Wang M P, Zhang R R, et al. The diffraction patterns from β" precipitates in 12 orientations in Al-Mg-Si alloy [J]. Scr. Mater., 2010, 62: 705
doi: 10.1016/j.scriptamat.2010.01.039
|
| 35 |
Sauvage X, Bobruk E V, Murashkin M Y, et al. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al-Mg-Si alloys [J]. Acta Mater., 2015, 98: 355
doi: 10.1016/j.actamat.2015.07.039
|
| 36 |
Pande C S, Cooper K P. Nanomechanics of Hall-Petch relationship in nanocrystalline materials [J]. Prog. Mater. Sci., 2009, 54: 689
doi: 10.1016/j.pmatsci.2009.03.008
|
| 37 |
Zhou S H, Napolitano R E. Phase equilibria and thermodynamic limits for partitionless crystallization in the Al-La binary system [J]. Acta Mater., 2006, 54: 831
doi: 10.1016/j.actamat.2005.10.013
|
| 38 |
Chang C S T, Banhart J. Low-temperature differential scanning calorimetry of an Al-Mg-Si alloy [J]. Metall. Mater. Trans., 2011, 42A: 1960
|
| 39 |
Mahidhara R K. Effect of grain size on the superplastic behavior of a 7475 aluminum alloy [J]. J. Mater. Eng. Perform., 1995, 4: 674
doi: 10.1007/BF02646443
|
| 40 |
Hirata T, Oguri T, Hagino H, et al. Influence of friction stir welding parameters on grain size and formability in 5083 aluminum alloy [J]. Mater. Sci. Eng., 2007, A456: 344
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|