Please wait a minute...
金属学报  2023, Vol. 59 Issue (4): 513-522    DOI: 10.11900/0412.1961.2023.00123
  综述 本期目录 | 过刊浏览 |
表面状态对核电关键材料腐蚀和应力腐蚀的影响
韩恩厚1,2,3(), 王俭秋1
1中国科学院金属研究所 中国科学院核用材料与安全评价重点实验室 沈阳 110016
2广东腐蚀科学与技术创新研究院 广州 510535
3华南理工大学 材料科学与工程学院 广州 511442
Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials
HAN En-Hou1,2,3(), WANG Jianqiu1
1CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
2Institute of Corrosion Science and Technology, Guangzhou 510535, China
3School of Materials Science and Engineering, South China University of Technology, Guangzhou 511442, China
引用本文:

韩恩厚, 王俭秋. 表面状态对核电关键材料腐蚀和应力腐蚀的影响[J]. 金属学报, 2023, 59(4): 513-522.
En-Hou HAN, Jianqiu WANG. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. Acta Metall Sin, 2023, 59(4): 513-522.

全文: PDF(2944 KB)   HTML
摘要: 

全球迄今发生的核电安全事件往往是由局部腐蚀造成,而局部腐蚀从表面起始。表面状态如何影响腐蚀,以及辐照和应力与之的交互作用已经成为核电站运行安全性、可靠性、经济性保障的重要技术难题之一。本文系统总结了在过去十余年的国家系列项目支持下,针对核电用关键结构材料在不同表面加工与划伤后微观组织变化、在模拟核电站一回路水中的腐蚀、应力腐蚀和辐照促进应力腐蚀行为,并将这些腐蚀行为与材料的微观组织以及力学、辐照等多因素相关联。结果表明,打磨、划伤和切削加工都会使材料近表面产生不同程度的梯度结构,表面变形层状态存在较大差异。划伤后,在划伤底部存在大于屈服极限的残余压应力。相同粗糙度的切削加工表面,机加工参数不同可以导致深度方向上形成的纳米晶区、晶粒畸变区梯度结构明显不同。这种微观组织与局部应力应变条件使得材料抗腐蚀能力差异显著,例如划伤导致的应力腐蚀裂纹数量与划伤深度正相关。在辐照、腐蚀、应力的联合作用下,辐照促进应力腐蚀敏感性进一步升高。最后展望了未来发展趋势。

关键词 : 表面状态,  腐蚀,  应力腐蚀,  辐照促进应力腐蚀,  核电材料,  不锈钢,  镍基合金    
Abstract:

Global nuclear power events are often caused by local corrosion, which starts at the surface. The effect of the surface state on corrosion and the interaction among corrosion, irradiation, and stress are important technical problems affecting the safety, reliability, and economy of nuclear power plants. In this paper, supported by a series of national projects in the last 10 years, the various surface state effects, for key structural materials used in nuclear power plants after surface finishing, grinding, machining, or scratching, on corrosion and stress corrosion behaviors in the simulated primary water of nuclear power plants are reviewed. The results show that surface grinding, scratching, or cutting can cause the formation of microstructures of different gradients near the surface and also cause large differences in surface deformation. For example, the residual compressive stress is greater than the yield stress in the superficial surface of the scratch; the different cutting parameters can cause the various gradient structures of the nanocrystalline and grain distortion zones to form along the depth of the cutting surface with similar surface roughness. Such microstructures and local stress-strain conditions lead to significant differences in corrosion resistance. For example, the number of stress corrosion cracks is positively correlated with scratch depth. Under the combined action of irradiation, corrosion, and stress, irradiation-assisted stress corrosion is further enhanced. Finally, the future research trend on the topic is forecast.

Key words: surface state    corrosion    stress corrosion    irradiation-assisted stress corrosion    nuclear material    stainless steel    nickel-based alloy
收稿日期: 2023-03-24     
ZTFLH:  TG171  
基金资助:国家重点基础研究发展计划项目(2011CB610500);国家重点基础研究发展计划项目(2006CB610500);国家重大科技专项项目(2011ZX06004-009);国家重点研发计划项目(2016YFE0105200);中国科学院重点部署项目(ZDRW-CN-2017-1);中国科学院前沿科学重点研究计划项目(QYZDY-SSW-JSC012)
通讯作者: 韩恩厚,ehhan@scut.edu.cn,主要从事材料腐蚀机理、腐蚀控制技术、装备服役安全评定技术研究与工程应用
Corresponding author: HAN En-Hou, professor, Tel: (020)22309460, E-mail: ehhan@scut.edu.cn
作者简介: 韩恩厚,男,1961年生,教授,博士
图1  不同表面状态690TT合金冷加工影响层截面的TEM像和选区电子衍射花样[11]
图2  690TT合金表面划伤的截面[16]
图3  7种切削加工工艺的核用304不锈钢样品近表面截面的EBSD分析[18]
图4  电解抛光和SiO2机械抛光316L不锈钢样品在核电一回路高温高压水中腐蚀500 h后氧化膜的TEM分析[20]
图5  核用304不锈钢切削加工影响区内变形带腐蚀的TEM形貌[18]
图6  应力腐蚀裂纹沿划伤沟槽晶界、滑移台阶生长[35]
图7  核级304不锈钢无应变与3%应变样品的沿晶氧化与辐照剂量的关系;辐照促进应力腐蚀开裂的敏感性(裂纹数量与长度)与辐照剂量的关系[46]
1 MacDonald P E, Shah V N, Ward L W, et al. Steam generator tube failures [R]. NUREG/CR-6635, Idaho National Engineering Laboratory, Lockheed Idaho Technologies Company, 1996
2 Staehle R W. Assessment of and proposal for a mechanistic interpretation of the SCC of high nickel alloys in lead-containing environments [A]. 11th Int. Conf. Environmental Degradation of Materials in Nuclear Systems [C]. Stevenson, WA, Aug.10-14, 2003
3 Staehle R W, Gorman J A. Quantitative assessment of submodes of stress corrosion cracking on the secondary side of steam generator tubing in pressurized water reactors: Part 1 [J]. Corrosion, 2003, 59: 931
doi: 10.5006/1.3277522
4 Andresen P L. Understanding and predicting stress corrosion cracking (SCC) in hot water [A]. Stress Corrosion Cracking of Nickel Based Alloys in Water-Cooled Nuclear Reactors, The Coriou Effect [M]. Woodhead Publishing: Elsevier, 2016: 169
5 Han E-H, Wang J Q, Wu X Q, et al. Corrosion mechanisms of stainless steel and nickel base alloys in high temperature high pressure water [J]. Acta Metall. Sin., 2010, 46: 1379
doi: 10.3724/SP.J.1037.2010.01379
5 韩恩厚, 王俭秋, 吴欣强 等. 核电高温高压水中不锈钢和镍基合金的腐蚀机制 [J]. 金属学报, 2010, 46: 1379
doi: 10.3724/SP.J.1037.2010.00468
6 Han E-H. Research trends on micro and nano-scale materials degradation in nuclear power plant [J]. Acta Metall. Sin., 2011, 47: 769
6 韩恩厚. 核电站关键材料在微纳米尺度上的环境损伤行为研究——进展与趋势 [J]. 金属学报, 2011, 47: 769
7 Zhang Z M, Wang J Q, Han E-H, et al. Analyses of surface oxide films on ground alloy 690TT after immersion for different times [J]. Acta Metall. Sin., 2011, 47: 823
7 张志明, 王俭秋, 韩恩厚 等. 打磨态690TT合金经不同时间浸泡后表面氧化膜结构分析 [J]. 金属学报, 2011, 47: 823
8 Zhang Z M, Wang J Q, Han E-H, et al. Analyses of surface oxide films on electropolished alloy 690TT after immersion for different times [J]. Acta Metall. Sin., 2011, 47: 831
8 张志明, 王俭秋, 韩恩厚 等. 电解抛光态690TT合金经不同时间浸泡后表面氧化膜结构分析 [J]. 金属学报, 2011, 47: 831
9 Zhang Z M, Wang J Q, Han E-H, et al. Effects of surface condition on corrosion and stress corrosion cracking of alloy 690TT [J]. J. Chin. Soc. Corros. Prot., 2011, 31: 441
9 张志明, 王俭秋, 韩恩厚 等. 表面状态对690TT合金腐蚀及应力腐蚀行为的影响 [J]. 中国腐蚀与防护学报, 2011, 31: 441
10 Zhang Z M, Wang J Q, Han E-H, et al. Influence of dissolved oxygen on oxide films of alloy 690TT with different surface status in simulated primary water [J]. Corros. Sci., 2011, 53: 3623
doi: 10.1016/j.corsci.2011.07.012
11 Zhang Z M, Wang J Q, Han E-H, et al. Characterization of different surface states and its effects on the oxidation behaviours of alloy 690TT [J]. J. Mater. Sci. Technol., 2012, 28: 353
doi: 10.1016/S1005-0302(12)60067-X
12 Zhang Z M, Wang J Q, Han E-H, et al. Effects of surface state and applied stress on stress corrosion cracking of alloy 690TT in lead-containing caustic solution [J]. J. Mater. Sci. Technol., 2012, 28: 785
13 Zhang Z M, Wang J Q, Han E-H, et al. Analysis of surface oxide films formed in hydrogenated primary water on alloy 690TT samples with different surface states [J]. J. Mater. Sci. Technol., 2014, 30: 1181
doi: 10.1016/j.jmst.2014.09.002
14 Zhang Z M, Wang J Q, Han E-H, et al. Analysis of surface oxide film formed on eletropolished alloy 690TT in high temperature and high pressure water with sequentially dissolved hydrogen and oxygen [J]. Acta Metall. Sin., 2015, 51: 85
doi: 10.11900/0412.1961.2014.00351
14 张志明, 王俭秋, 韩恩厚 等. 电解抛光态690TT合金在顺序溶氢/溶氧的高温高压水中表面氧化膜结构分析 [J]. 金属学报, 2015, 51: 85
doi: 10.11900/0412.1961.2014.00351
15 Meng F J, Wang J Q, Han E-H, et al. Effects of scratching on corrosion and stress corrosion cracking of Alloy 690TT at 58oC and 330oC [J]. Corros. Sci., 2009, 51: 2761
doi: 10.1016/j.corsci.2009.07.015
16 Meng F J, Han E-H, Wang J Q, et al. Localized corrosion behavior of scratches on nickel-base alloy 690TT [J]. Electrochim. Acta, 2011, 56: 1781
doi: 10.1016/j.electacta.2010.08.028
17 Wang J Q, Huang F, Han E-H, et al. Microscopic residual stresses beneath a scratch and their effects on scratch-related crack initiation of thermally treated UNS N06690 in high temperature pressurized water [J]. Corrosion, 2013, 69: 893
doi: 10.5006/0858
18 Yan H L, Wang J Q, Zhang Z M, et al. Effects of cutting parameter on microstructure and corrosion behavior of 304 stainless steel in simulated primary water [J]. J. Mater. Sci. Technol., 2022, 122: 219
doi: 10.1016/j.jmst.2021.04.081
19 Zhang Z M, Wang J Q, Han E-H, et al. Effects of surface machining by a lathe on microstructure of near surface layer and corrosion behavior of SA182 grade 304 stainless steel in simulated primary water [J]. Corros. Sci. Technol., 2019, 18: 1
20 Han Y L, Mei J N, Peng Q J, et al. Effect of electropolishing on corrosion of nuclear grade 316L stainless steel in deaerated high temperature water [J]. Corros. Sci., 2016, 112: 625
doi: 10.1016/j.corsci.2016.09.002
21 Han Y L, Mei J N, Peng Q J, et al. Effect of electropolishing on corrosion of alloy 600 in high temperature water [J]. Corros. Sci., 2015, 98: 72
doi: 10.1016/j.corsci.2015.05.026
22 Han Y L, Han E H, Peng Q J, et al. Effects of electropolishing on corrosion and stress corrosion cracking of alloy 182 in high temperature water [J]. Corros. Sci., 2017, 121: 1
doi: 10.1016/j.corsci.2017.03.004
23 Guo Y L, Han E-H, Wang J Q. Effects of surface state on the electrochemical corrosion behavior of nuclear grade 316LN stainless steel [J]. Chin. J. Eng., 2016, 38: 87
23 郭跃岭, 韩恩厚, 王俭秋. 表面状态对核级316LN不锈钢电化学腐蚀行为的影响 [J]. 工程科学学报, 2016, 38: 87
24 Guo Y L, Han E-H, Wang J Q. Effects of surface states on the oxidation behavior of 316LN stainless steel in high temperature pressurized water [J]. Mater. Corros., 2015, 66: 670
25 Ming H L, Zhang Z M, Wang J Z, et al. Effect of surface state on the oxidation behavior of welded 308L in simulated nominal primary water of PWR [J]. Appl. Surf. Sci., 2015, 337: 81
doi: 10.1016/j.apsusc.2015.02.066
26 Ming H L, Zhang Z M, Wang S Y, et al. Short time oxidation behavior of 308L weld metal and 316L stainless steel with different surface state in simulated primary water with 0.1 mg/L dissolved oxygen [J]. Mater. Corros., 2015, 66: 869
27 Guo S, Wang H T, Han E-H. Computational evaluation of the influence of various uniaxial load levels on pit growth of stainless steel under mechanoelectrochemical interactions [J]. J. Electrochem. Soc., 2018, 165: C515
doi: 10.1149/2.1071809jes
28 Wang H T, Han E-H. Ab initio molecular dynamics simulation on interfacial reaction behavior of Fe-Cr-Ni stainless steel in high temperature water [J]. Comput. Mater. Sci., 2018, 149: 143
doi: 10.1016/j.commatsci.2018.03.025
29 Wang H T, Sun X F, Han E-H. The interactions between high temperature water and Fe3O4 (111) by first-principles molecular dynamics simulation [J]. Int. J. Electrochem. Sci., 2018, 13: 2430
30 Sun X F, Wang H T, Han E-H. Effect of Cr doping on the surface characteristics of Ni metal studied with first-principles calculation [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 461
doi: 10.1007/s40195-018-0776-7
31 Yin X R, Wang H T, Han E-H. Effects of solvation and applied potential on the adsorption behaviors of H, O, OH and H2O on Fe(110) surface [J]. Surf. Sci., 2020, 691: 121504
doi: 10.1016/j.susc.2019.121504
32 Yin X R, Sun X F, Wang H T, et al. Adsorption and dissociation of water on halogen pre-adsorbed Ni(111) and Ni-Cr(111) surfaces: A DFT study [J]. Solid State Commun., 2020, 321: 114040
doi: 10.1016/j.ssc.2020.114040
33 Yin X R, Wang H T, Sun S, et al. Comparative study on the adsorption behaviors of O and Cl on Fe(110) surfaces with different Cr content [J]. Mater. Today Commun., 2020, 24: 101122
34 Wang H T, Ding J W, Zhang R F, et al. Atomistic insights into interfacial reactions of FeCr2O4 oxide films in high-temperature water [J]. Int. J. Electrochem. Sci., 2020, 15: 8662
35 Meng F J, Wang J Q, Han E-H, et al. Microstructure near scratch on alloy 690TT and stress corrosion induced by scratching [J]. Acta Metall. Sin., 2011, 47: 839
35 孟凡江, 王俭秋, 韩恩厚 等. 690TT合金划痕显微组织及划伤诱发的应力腐蚀 [J]. 金属学报, 2011, 47: 839
36 Meng F J, Wang J Q, Han E-H, et al. Stress corrosion crack initiation for scratched alloy 690TT in oxygenated high temperature water [J]. J. Chin. Soc. Corros. Prot., 2013, 33: 413
36 孟凡江, 王俭秋, 韩恩厚 等. 划伤690TT合金在高温含氧水中应力腐蚀裂纹萌生的研究 [J]. 中国腐蚀与防护学报, 2013, 33: 413
37 Meng F J, Wu B, Lv Y H, et al. Effect of surface scratch on corrosion behavior of alloy 690TT heat exchanger tubes [J]. Chin. J. Mater. Res., 2021, 35: 827
doi: 10.11901/1005.3093.2021.001
37 孟凡江, 吴 斌, 吕云鹤 等. 表面划伤对690TT合金传热管腐蚀行为的影响 [J]. 材料研究学报, 2021, 35: 827
doi: 10.11901/1005.3093.2021.001
38 Wu B, Ming H L, Zhang Z M, et al. Effect of surface scratch depth on microstructure change and stress corrosion cracking behavior of alloy 690TT steam generator tube [J]. Corros. Sci., 2021, 192: 109792
doi: 10.1016/j.corsci.2021.109792
39 Wu B, Meng F J, Zhang Z M, et al. Stress corrosion behavior of scratched alloy 690TT steam generator tube in chlorine‐containing high‐temperature pressurized water [J]. Mater. Corros., 2022, 73: 1563
40 Wu B, Ming H L, Meng F J, et al. Effects of surface grinding for scratched alloy 690TT tube in PWR nuclear power plant: Microstructure and stress corrosion cracking [J]. J. Mater. Sci. Technol., 2022, 113: 229
doi: 10.1016/j.jmst.2021.11.009
41 Deng P, Peng Q J, Han E-H, et al. Study of irradiation damage in domestically fabricated nuclear grade stainless steel [J]. Acta Metall. Sin., 2017, 53: 1588
doi: 10.11900/0412.1961.2017.00117
41 邓 平, 彭群家, 韩恩厚 等. 国产核用不锈钢辐照损伤研究 [J]. 金属学报, 2017, 53: 1588
42 Deng P, Peng Q J, Han E-H, et al. Effect of irradiation on corrosion of 304 nuclear grade stainless steel in simulated PWR primary water [J]. Corros. Sci., 2017, 127: 91
doi: 10.1016/j.corsci.2017.08.010
43 Deng P, Peng Q J, Han E-H, et al. Effect of the amount of cold work on corrosion of type 304 nuclear grade stainless steel in high-temperature water [J]. Corrosion, 2017, 73: 1237
doi: 10.5006/2436
44 Deng P, Sun C, Peng Q J, et al. Study on irradiation assisted stress corrosion cracking of nuclear grade 304 stainless steel [J]. Acta Metall. Sin., 2019, 55: 349
doi: 10.11900/0412.1961.2018.00359
44 邓 平, 孙 晨, 彭群家 等. 核用304不锈钢辐照促进应力腐蚀开裂研究 [J]. 金属学报, 2019, 55: 349
45 Deng P, Han E-H, Peng Q J, et al. Corrosion behavior and mechanism of irradiated 304 nuclear grade stainless steel in high-temperature water [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 174
doi: 10.1007/s40195-020-01123-y
46 Deng P, Peng Q J, Han E-H, et al. Proton irradiation assisted localized corrosion and stress corrosion cracking in 304 nuclear grade stainless steel in simulated primary PWR water [J]. J. Mater. Sci. Technol., 2021, 65: 61
doi: 10.1016/j.jmst.2020.04.068
[1] 李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧. 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为[J]. 金属学报, 2023, 59(7): 884-892.
[2] 陈润农, 李昭东, 曹燕光, 张启富, 李晓刚. 9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源[J]. 金属学报, 2023, 59(7): 926-938.
[3] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[4] 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽. EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为[J]. 金属学报, 2023, 59(7): 893-904.
[5] 赵平平, 宋影伟, 董凯辉, 韩恩厚. 不同离子对TC4钛合金电化学腐蚀行为的协同作用机制[J]. 金属学报, 2023, 59(7): 939-946.
[6] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[7] 王滨, 牛梦超, 王威, 姜涛, 栾军华, 杨柯. 含Cu马氏体时效不锈钢的组织与强韧性[J]. 金属学报, 2023, 59(5): 636-646.
[8] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[9] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[10] 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁. 以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升[J]. 金属学报, 2023, 59(4): 523-536.
[11] 常立涛. 压水堆主回路高温水中奥氏体不锈钢加工表面的腐蚀与应力腐蚀裂纹萌生:研究进展及展望[J]. 金属学报, 2023, 59(2): 191-204.
[12] 廖京京, 张伟, 张君松, 吴军, 杨忠波, 彭倩, 邱绍宇. Zr-Sn-Nb-Fe-V合金在过热蒸汽中的周期性钝化-转折行为[J]. 金属学报, 2023, 59(2): 289-296.
[13] 夏大海, 计元元, 毛英畅, 邓成满, 祝钰, 胡文彬. 2024铝合金在模拟动态海水/大气界面环境中的局部腐蚀机制[J]. 金属学报, 2023, 59(2): 297-308.
[14] 胡文滨, 张晓雯, 宋龙飞, 廖伯凯, 万闪, 康磊, 郭兴蓬. 共晶高熵合金AlCoCrFeNi2.1 在H2SO4 溶液中的腐蚀行为[J]. 金属学报, 2023, 59(12): 1644-1654.
[15] 宋嘉良, 江紫雪, 易盼, 陈俊航, 李曌亮, 骆鸿, 董超芳, 肖葵. 高铁转向架用钢G390NH在模拟海洋和工业大气环境下的腐蚀行为及产物演化规律[J]. 金属学报, 2023, 59(11): 1487-1498.