| 高铁转向架用钢G390NH在模拟海洋和工业大气环境下的腐蚀行为及产物演化规律 |
宋嘉良1,2, 江紫雪1,2, 易盼3, 陈俊航1,2, 李曌亮1,2, 骆鸿1,2( ), 董超芳1,2, 肖葵1,2( ) |
1.北京科技大学 新材料技术研究院 北京 100083 2.北京科技大学 腐蚀与防护中心 北京 100083 3.中国电力科学研究院有限公司 北京 100192 |
|
| Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment |
SONG Jialiang1,2, JIANG Zixue1,2, YI Pan3, CHEN Junhang1,2, LI Zhaoliang1,2, LUO Hong1,2( ), DONG Chaofang1,2, XIAO Kui1,2( ) |
1.Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China 2.Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China 3.China Electric Power Research Institute Co., Ltd., Beijing 100192, China |
引用本文:
宋嘉良, 江紫雪, 易盼, 陈俊航, 李曌亮, 骆鸿, 董超芳, 肖葵. 高铁转向架用钢G390NH在模拟海洋和工业大气环境下的腐蚀行为及产物演化规律[J]. 金属学报, 2023, 59(11): 1487-1498.
Jialiang SONG,
Zixue JIANG,
Pan YI,
Junhang CHEN,
Zhaoliang LI,
Hong LUO,
Chaofang DONG,
Kui XIAO.
Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. Acta Metall Sin, 2023, 59(11): 1487-1498.
| 1 |
Li X G, Zhang D W, Liu Z Y, et al. Materials science: Share corrosion data [J]. Nature, 2015, 527: 441
doi: 10.1038/527441a
|
| 2 |
Misawa T, Asami K, Hashimoto K, et al. The mechanism of atmospheric rusting and the protective amorphous rust on low alloy steel [J]. Corros. Sci., 1974, 14: 279
doi: 10.1016/S0010-938X(74)80037-5
|
| 3 |
Ma Y T, Li Y, Wang F H. Weatherability of 09CuPCrNi steel in a tropical marine environment [J]. Corros. Sci., 2009, 51: 1725
doi: 10.1016/j.corsci.2009.04.024
|
| 4 |
Qian Y H, Ma C H, Niu D, et al. Influence of alloyed chromium on the atmospheric corrosion resistance of weathering steels [J]. Corros. Sci., 2013, 74: 424
doi: 10.1016/j.corsci.2013.05.008
|
| 5 |
Chen Y Y, Tzeng H J, Wei L I, et al. Corrosion resistance and mechanical properties of low-alloy steels under atmospheric conditions [J]. Corros. Sci., 2005, 47: 1001
doi: 10.1016/j.corsci.2004.04.009
|
| 6 |
Wang J, Wang Z Y, Ke W. A study of the evolution of rust on weathering steel submitted to the Qinghai salt lake atmospheric corrosion [J]. Mater. Chem. Phys., 2013, 139: 225
doi: 10.1016/j.matchemphys.2013.01.028
|
| 7 |
Zhang Z J, Ding Y X, Liu D J, et al. Microstructure and corrosion resistance of welded joint of SMA490BW and Q345E dissimilar metals for bogies [J]. Hot Work. Technol., 2021, 50(5): 46
|
| 7 |
张政军, 丁阳喜, 刘德佳 等. 转向架用SMA490BW和Q345E异种金属焊接接头组织和耐腐蚀行为 [J]. 热加工工艺, 2021, 50(5):46
|
| 8 |
Zhang Q, Dai F H, Si Y, et al. Microstructure and salt spray corrosion behavior of bogie Q345C steel surfacing weld [J]. Electr. Weld. Mach., 2016, 46(6): 107
|
| 8 |
张 强, 代夫华, 司 毅 等. 转向架用Q345C钢堆焊接头组织及盐雾腐蚀行为 [J]. 电焊机, 2016, 46(6): 107
|
| 9 |
Kamimura T, Hara S, Miyuki H, et al. Composition and protective ability of rust layer formed on weathering steel exposed to various environments [J]. Corros. Sci., 2006, 48: 2799
doi: 10.1016/j.corsci.2005.10.004
|
| 10 |
Thee C, Hao L, Dong J H, et al. Atmospheric corrosion monitoring of a weathering steel under an electrolyte film in cyclic wet-dry condition [J]. Corros. Sci., 2014, 78: 130
doi: 10.1016/j.corsci.2013.09.008
|
| 11 |
Yamashita M, Konishi H, Kozakura T, et al. In situ observation of initial rust formation process on carbon steel under Na2SO4 and NaCl solution films with wet/dry cycles using synchrotron radiation X-rays [J]. Corros. Sci., 2005, 47: 2492
doi: 10.1016/j.corsci.2004.10.021
|
| 12 |
Dillmann P, Mazaudier F, Hœrlé S. Advances in understanding atmospheric corrosion of iron. I. Rust characterisation of ancient ferrous artefacts exposed to indoor atmospheric corrosion [J]. Corros. Sci., 2004, 46: 1401
doi: 10.1016/j.corsci.2003.09.027
|
| 13 |
Yamashita M, Miyuki H, Matsuda Y, et al. The long term growth of the protective rust layer formed on weathering steel by atmospheric corrosion during a quarter of a century [J]. Corros. Sci., 1994, 36: 283
doi: 10.1016/0010-938X(94)90158-9
|
| 14 |
Singh D D N, Yadav S, Saha J K. Role of climatic conditions on corrosion characteristics of structural steels [J]. Corros. Sci., 2008, 50: 93
doi: 10.1016/j.corsci.2007.06.026
|
| 15 |
Misawa T, Hashimoto K, Shimodaira S. The mechanism of formation of iron oxide and oxyhydroxides in aqueous solutions at room temperature [J]. Corros. Sci., 1974, 14: 131
doi: 10.1016/S0010-938X(74)80051-X
|
| 16 |
Asami K, Kikuchi M. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17 years [J]. Corros. Sci., 2003, 45: 2671
doi: 10.1016/S0010-938X(03)00070-2
|
| 17 |
Allam I M, Arlow J S, Saricimen H. Initial stages of atmospheric corrosion of steel in the Arabian Gulf [J]. Corros. Sci., 1991, 32: 417
doi: 10.1016/0010-938X(91)90123-7
|
| 18 |
Ma Y T, Li Y, Wang F H. The effect of β-FeOOH on the corrosion behavior of low carbon steel exposed in tropic marine environment [J]. Mater. Chem. Phys., 2008, 112: 844
doi: 10.1016/j.matchemphys.2008.06.066
|
| 19 |
Hubbard C R, Snyder R L. RIR-measurement and use in quantitative XRD [J]. Powder Diffr., 1988, 3: 74
doi: 10.1017/S0885715600013257
|
| 20 |
Pan C, Guo M X, Han W, et al. Study of corrosion evolution of carbon steel exposed to an industrial atmosphere [J]. Corros. Eng. Sci. Technol., 2019, 54: 241
doi: 10.1080/1478422X.2019.1574955
|
| 21 |
Zhang H, Du Y X, Li W, et al. Investigation on AC-induced corrosion behavior and product film of X70 steel in aqueous environmental with various ions [J]. Acta Metall. Sin., 2017, 53: 975
|
| 21 |
张 慧, 杜艳霞, 李 伟 等. 不同环境介质中X70钢的交流腐蚀行为及腐蚀产物膜层分析 [J]. 金属学报, 2017, 53: 975
|
| 22 |
Majzlan J, Mazeina L, Navrotsky A. Enthalpy of water adsorption and surface enthalpy of lepidocrocite (γ-FeOOH) [J]. Geochim. Cosmochim. Acta, 2007, 71: 615
doi: 10.1016/j.gca.2006.10.010
|
| 23 |
Majzlan J, Grevel K D, Navrotsky A. Thermodynamics of Fe oxides:Part II. Enthalpies of formation and relative stability of goethite (α-FeOOH), lepidocrocite (γ-FeOOH), and maghemite (γ-Fe2O3) [J]. Am. Mineral., 2003, 88: 855
doi: 10.2138/am-2003-5-614
|
| 24 |
Hara S, Kamimura T, Miyuki H, et al. Taxonomy for protective ability of rust layer using its composition formed on weathering steel bridge [J]. Corros. Sci., 2007, 49: 1131
doi: 10.1016/j.corsci.2006.06.016
|
| 25 |
Rémazeilles C, Refait P. On the formation of β-FeOOH (Akaganéite) in chloride-containing environments [J]. Corros. Sci., 2007, 49: 844
doi: 10.1016/j.corsci.2006.06.003
|
| 26 |
Wu W, Cheng X Q, Zhao J B, et al. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives [J]. Corros. Sci., 2020, 165: 108416
doi: 10.1016/j.corsci.2019.108416
|
| 27 |
Wang Z F, Liu J R, Wu L X, et al. Study of the corrosion behavior of weathering steels in atmospheric environments [J]. Corros. Sci., 2013, 67: 1
doi: 10.1016/j.corsci.2012.09.020
|
| 28 |
Qu Q, Yan C W, Zhang L, et al. Synergism of NaCl and SO2 in the initial atmospheric corrosion of A3 steel [J]. Acta Metall. Sin., 2002, 38: 1062
|
| 28 |
屈 庆, 严川伟, 张 蕾 等. NaCl和SO2在A3钢初期大气腐蚀中的协同效应 [J]. 金属学报, 2002, 38: 1062
|
| 29 |
Evans U R, Taylor C A J. Mechanism of atmospheric rusting [J]. Corros. Sci., 1972, 12: 227
doi: 10.1016/S0010-938X(72)90671-3
|
| 30 |
Misawa T, Kyuno T, Suëtaka W, et al. The mechanism of atmospheric rusting and the effect of Cu and P on the rust formation of low alloy steels [J]. Corros. Sci., 1971, 11: 35
doi: 10.1016/S0010-938X(71)80072-0
|
| 31 |
Gong K, Wu M, Liu G X. Stress corrosion cracking behavior of rusted X100 steel under the combined action of Cl- and HSO3- in a wet-dry cycle environment [J]. Corros. Sci., 2020, 165: 108382
doi: 10.1016/j.corsci.2019.108382
|
| 32 |
Hao L, Zhang S X, Dong J H, et al. Rusting evolution of MnCuP weathering steel submitted to simulated industrial atmospheric corrosion [J]. Metall. Mater. Trans., 2012, 43A: 1724
|
| 33 |
Wang J, Wang Z Y, Ke W. Corrosion behaviour of weathering steel in diluted Qinghai salt lake water in a laboratory accelerated test that involved cyclic wet/dry conditions [J]. Mater. Chem. Phys., 2010, 124: 952
doi: 10.1016/j.matchemphys.2010.07.069
|
| 34 |
Ke W, Dong J H. Study on the rusting evolution and the performance of resisting to atmospheric corrosion for Mn-Cu steel [J]. Acta Metall. Sin., 2010, 46: 1365
doi: 10.3724/SP.J.1037.2010.00489
|
| 34 |
柯 伟, 董俊华. Mn-Cu钢大气腐蚀锈层演化规律及其耐候性的研究 [J]. 金属学报, 2010, 46: 1365
|
| 35 |
Chen W J, Hao L, Dong J H, et al. Effect of sulphur dioxide on the corrosion of a low alloy steel in simulated coastal industrial atmosphere [J]. Corros. Sci., 2014, 83: 155
doi: 10.1016/j.corsci.2014.02.010
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|