| 孪生诱发软化与强化效应的Cu晶体塑性行为模拟 |
郭祥如1,2, 申俊杰1,2( ) |
1.天津理工大学 天津市先进机电系统设计与智能控制重点实验室 天津 300384 2.天津理工大学 机电工程国家级实验教学示范中心 天津 300384 |
|
| Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects |
GUO Xiangru1,2, SHEN Junjie1,2( ) |
1.Tianjin Key Laboratory for Advanced Mechatronic System Design and Intelligent Control, School of Mechanical Engineering, Tianjin University of Technology, Tianjin 300384, China 2.National Demonstration Center for Experimental Mechanical and Electrical Engineering Education, Tianjin University of Technology, Tianjin 300384, China |
引用本文:
郭祥如, 申俊杰. 孪生诱发软化与强化效应的Cu晶体塑性行为模拟[J]. 金属学报, 2022, 58(3): 375-384.
Xiangru GUO,
Junjie SHEN.
Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. Acta Metall Sin, 2022, 58(3): 375-384.
| 1 |
Guo X R, Sun C Y, Li R, et al. A dislocation density based model for twinning induced softening of TWIP steel [J]. Comput. Mater. Sci., 2017, 139: 8
|
| 2 |
Niewczas M, Basinski Z S, Basinski S J, et al. Deformation of copper single crystals to large strains at 4.2K—I. Mechanical response and electrical resistivity [J]. Philos. Mag., 2001, 81A: 1121
|
| 3 |
Seo J H, Park H S, Yoo Y, et al. Origin of size dependency in coherent-twin-propagation-mediated tensile deformation of noble metal nanowires [J]. Nano Lett., 2013, 13: 5112
|
| 4 |
Liang Z Y, Li Y Z, Huang M X. The respective hardening contributions of dislocations and twins to the flow stress of a twinning-induced plasticity steel [J]. Scr. Mater., 2016, 112: 28
|
| 5 |
Luo Z C, Huang M X. Revisit the role of deformation twins on the work-hardening behaviour of twinning-induced plasticity steels [J]. Scr. Mater., 2018, 142: 28
|
| 6 |
Paramatmuni C, Zheng Z B, Rainforth W M, et al. Twin nucleation and variant selection in Mg alloys: An integrated crystal plasticity modelling and experimental approach [J]. Int. J. Plast., 2020, 135: 102778
|
| 7 |
Zhi H H, Zhang C, Antonov S, et al. Investigations of dislocation-type evolution and strain hardening during mechanical twinning in Fe-22Mn-0.6C twinning-induced plasticity steel [J]. Acta Mater., 2020, 195: 371
|
| 8 |
Bertin N, Sills R B, Cai W. Frontiers in the simulation of dislocations [J]. Annu. Rev. Mater. Res., 2020, 50: 437
|
| 9 |
Zhang J, Li H W, Sun X X, et al. A multi-scale MCCPFEM framework: Modeling of thermal interface grooving and deformation anisotropy of titanium alloy with lamellar colony [J]. Int. J. Plast., 2020, 135: 102804
|
| 10 |
Agaram S, Kanjarla A K, Bhuvaraghan B, et al. Dislocation density based crystal plasticity model incorporating the effect of precipitates in IN718 under monotonic and cyclic deformation [J]. Int. J. Plast., 2021, 141: 102990
|
| 11 |
Sun C Y, Guo N, Fu M W, et al. Modeling of slip, twinning and transformation induced plastic deformation for TWIP steel based on crystal plasticity [J]. Int. J. Plast., 2016, 76: 186
|
| 12 |
Guo N, Tang B T, Liu J Y, et al. Characteristic stepwise strain hardening behaviour induced by slip and twinning of large-deformed copper single crystals: Crystal plasticity modelling and simulation [J]. Philos. Mag., 2021, 101: 1245
|
| 13 |
Li X X, Xu D S, Yang R. Crystal plasticity finite element method investigation of the high temperature deformation consistency in dual-phase titanium alloy [J]. Acta Metall. Sin., 2019, 55: 928
|
| 13 |
李学雄, 徐东生, 杨 锐. 双相钛合金高温变形协调性的CPFEM研究 [J]. 金属学报, 2019, 55: 928
|
| 14 |
Chin G Y, Hosford W F, Mendorf D R. Accommodation of constrained deformation in f.c.c. metals by slip and twinning [J]. Proc. Roy. Soc., 1969, 309A: 433
|
| 15 |
Van Houtte P. Simulation of the rolling and shear texture of brass by the Taylor theory adapted for mechanical twinning [J]. Acta Metall., 1978, 26: 591
|
| 16 |
Choi S H, Shin E J, Seong B S. Simulation of deformation twins and deformation texture in an AZ31 Mg alloy under uniaxial compression [J]. Acta Mater., 2007, 55: 4181
|
| 17 |
Tomé C N, Lebensohn R A, Kocks U F. A model for texture development dominated by deformation twinning: Application to zirconium alloys [J]. Acta Metall. Mater., 1991, 39: 2667
|
| 18 |
Kalidindi S R. Modeling anisotropic strain hardening and deformation textures in low stacking fault energy fcc metals [J]. Int. J. Plast., 2001, 17: 837
|
| 19 |
Sun C Y, Guo X R, Huang J, et al. Modelling of plastic deformation on coupling twinning of single crystal TWIP steel [J]. Acta Metall. Sin., 2015, 51: 357
|
| 19 |
孙朝阳, 郭祥如, 黄 杰等. 耦合孪生的TWIP钢单晶体塑性变形行为模拟研究 [J]. 金属学报, 2015, 51: 357
|
| 20 |
Sun C Y, Guo X R, Guo N, et al. Investigation of plastic deformation behavior on coupling twinning of polycrystal TWIP steel [J]. Acta Metall. Sin., 2015, 51: 1507
|
| 20 |
孙朝阳, 郭祥如, 郭 宁等. 耦合孪生的TWIP钢多晶体塑性变形行为研究 [J]. 金属学报, 2015, 52: 1507
|
| 21 |
Beyerlein I J, Mara N A, Bhattacharyya D, et al. Texture evolution via combined slip and deformation twinning in rolled silver-copper cast eutectic nanocomposite [J]. Int. J. Plast., 2011, 27: 121
|
| 22 |
Wu P D, Guo X Q, Qiao H, et al. A constitutive model of twin nucleation, propagation and growth in magnesium crystals [J]. Mater. Sci. Eng., 2015, A625: 140
|
| 23 |
Qiao H, Barnett M R, Wu P D. Modeling of twin formation, propagation and growth in a Mg single crystal based on crystal plasticity finite element method [J]. Int. J. Plast., 2016, 86: 70
|
| 24 |
Wang H, Clausen B, Capolungo L, et al. Stress and strain relaxation in magnesium AZ31 rolled plate: In-situ neutron measurement and elastic viscoplastic polycrystal modeling [J]. Int. J. Plast., 2016, 79: 275
|
| 25 |
Kalidindi S R. Incorporation of deformation twinning in crystal plasticity models [J]. J. Mech. Phys. Solids, 1998, 46: 267
|
| 26 |
Allain S, Chateau J P, Bouaziz O. A physical model of the twinning-induced plasticity effect in a high manganese austenitic steel [J]. Mater. Sci. Eng., 2004, A387: 143
|
| 27 |
Arsenlis A, Parks D M. Modeling the evolution of crystallographic dislocation density in crystal plasticity [J]. J. Mech. Phys. Solids, 2002, 50: 1979
|
| 28 |
Sun Z K, Li F G, Zhu J M. Radial micro-cracks in pile-up region of single-crystal Cu in spherical indentation: Experimental observation and crystal plastic simulation [J]. J. Mater. Sci., 2019, 54: 9875
|
| 29 |
Khan A S, Liu J, Yoon J W, et al. Strain rate effect of high purity aluminum single crystals: Experiments and simulations [J]. Int. J. Plast., 2015, 67: 39
|
| 30 |
Dancette S, Delannay L, Renard K, et al. Crystal plasticity modeling of texture development and hardening in TWIP steels [J]. Acta Mater., 2012, 60: 2135
|
| 31 |
Blewitt T H, Coltman R R, Redman J K. Low-temperature deformation of copper single crystals [J]. J. Appl. Phys., 1957, 28: 651
|
| 32 |
Quey R, Dawson P R, Barbe F. Large-scale 3D random polycrystals for the finite element method: Generation, meshing and remeshing [J]. Comput. Methods Appl. Mech. Eng., 2011, 200: 1729
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|