| 稀土Ce对非调质钢中硫化物特征及微观组织的影响 |
刘洁1, 徐乐1( ), 史超2, 杨少朋1,3, 何肖飞1, 王毛球1, 时捷1 |
1.钢铁研究总院 特殊钢研究所 北京 100081 2.内蒙古北方重工业集团有限公司 包头 014033 3.马鞍山钢铁股份有限公司技术中心 马鞍山 243000 |
|
| Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel |
LIU Jie1, XU Le1( ), SHI Chao2, YANG Shaopeng1,3, HE Xiaofei1, WANG Maoqiu1, SHI Jie1 |
1.Institute of Special Steels, Central Iron and Steel Research Institute, Beijing 100081, China 2.Inner Monglia North Heavy Industries Group Corp. Ltd. , Baotou 014033, China 3.The Technology Center of Ma'anshan Iron and Steel Co. Ltd. , Ma'anshan 243000, China |
引用本文:
刘洁, 徐乐, 史超, 杨少朋, 何肖飞, 王毛球, 时捷. 稀土Ce对非调质钢中硫化物特征及微观组织的影响[J]. 金属学报, 2022, 58(3): 365-374.
Jie LIU,
Le XU,
Chao SHI,
Shaopeng YANG,
Xiaofei HE,
Maoqiu WANG,
Jie SHI.
Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. Acta Metall Sin, 2022, 58(3): 365-374.
| 1 |
Stuart H. The properties and processing of microalloyed HSLA steels [J]. JOM, 1991, 43(1): 35
|
| 2 |
Paules J R. Developments in HSLA steel products [J]. JOM, 1991, 43(1): 41
|
| 3 |
Lu J L, Cheng G G, Tan B, et al. Effect of Zr, Al addition on characteristics of MnS and formation of intragranular ferrite in non-quenched and tempered steel [J]. ISIJ Int., 2018, 58: 921
|
| 4 |
Lu J L, Cheng G G, Chen L, et al. Distribution and morphology of MnS inclusions in resulfurized non-quenched and tempered steel with Zr addition [J]. ISIJ Int., 2018, 58: 1307
|
| 5 |
Chen H X, Zhou P, Chen A J, et al. Development of free cutting steel for automobile [J]. Chin. Metall., 2001, (3): 32
|
| 5 |
陈洪星, 周 平, 陈爱洁等. 汽车用易切削钢的开发 [J]. 中国冶金, 2001, (3): 32
|
| 6 |
Li M L. Study on formation behavior and homogenization control of sulfide inclusions in free-cutting non-quenched and tempered steel [D]. Beijing: University of Science and Technology Beijing, 2015
|
| 6 |
李梦龙. 易切削非调质钢中硫化物生成行为与均匀化控制研究 [D]. 北京: 北京科技大学, 2015
|
| 7 |
Sun H, Wu L P, Xie J B, et al. Inclusions modification and improvement of machinability in a non-quenched and tempered steel with Mg treatment [J]. Metall. Res. Technol., 2020, 117: 208
|
| 8 |
Lin S G, Yang H H, Su Y H, et al. CALPHAD-assisted morphology control of manganese sulfide inclusions in free-cutting steels [J]. J. Alloys Compd., 2019, 779: 844
|
| 9 |
Shen P, Fu J X. Morphology study on inclusion modifications using Mg-Ca treatment in resulfurized special steel [J]. Materials, 2019, 12: 197
|
| 10 |
Ma Q Q, Wu C C, Cheng G G, et al. Characteristic and formation mechanism of inclusions in 2205 duplex stainless steel containing rare earth elements [J]. Mater. Today: Proc., 2015, 2(suppl.2): S300
|
| 11 |
Zhang Q S, Min Y, Xu J J, et al. Formation and evolution behavior of inclusions in Al-killed resulfurized free-cutting steel with magnesium treatment [J]. J. Iron Steel Res. Int., 2020, 27: 631
|
| 12 |
Dong H Y, Hu L J, Liang W Y, et al. Effect of rare earth element Ce on corrosion resistance of 316L stainless steel [J]. Corros. Sci. Prot. Technol., 2018, 30: 489
|
| 12 |
董海英, 胡丽娟, 梁婉怡等. 稀土Ce对316L不锈钢耐腐蚀性能的影响 [J]. 腐蚀科学与防护技术, 2018, 30: 489
|
| 13 |
Wang L M, Lin Q, Ji J W, et al. New study concerning development of application of rare earth metals in steels [J]. J. Alloys Compd., 2006, 408-412: 384
|
| 14 |
Huang Y, Cheng G G, Xie Y. Modification mechanism of cerium on the inclusions in drill steel [J]. Acta Metall. Sin., 2018, 54: 1253
|
| 14 |
黄 宇, 成国光, 谢 有. 稀土Ce对钎具钢中夹杂物的改质机理研究 [J]. 金属学报, 2018, 54: 1253
|
| 15 |
Huang Y, Cheng G G, Li S J, et al. Precipitation mechanism and thermal stability of primary carbide in Ce microalloyed H13 steel [J]. Acta Metall. Sin., 2019, 55: 1487
|
| 15 |
黄 宇, 成国光, 李世健等. Ce微合金化H13钢中一次碳化物的析出机理及热稳定性研究 [J]. 金属学报, 2019, 55: 1487
|
| 16 |
Torkamani H, Raygan S, Garcia Mateo C, et al. Contributions of rare earth element (La, Ce) addition to the impact toughness of low carbon cast niobium microalloyed steels [J]. Met. Mater. Int., 2018, 24: 773
|
| 17 |
Adabavazeh Z, Hwang W S, Su Y H. Effect of adding cerium on microstructure and morphology of Ce-based inclusions formed in low-carbon steel [J]. Sci. Rep., 2017, 7: 46503
|
| 18 |
Torkamani H, Raygan S, Mateo C G, et al. The Influence of La and Ce addition on inclusion modification in cast niobium micro-alloyed steels [J]. Metals, 2017, 7: 377
|
| 19 |
Liu D L, Wang Y L, Huo X D, et al. Crain refinement and strengthening of low garbon steel by CSP technology [J]. Acta Metall. Sin., 2002, 38: 647
|
| 19 |
柳得橹, 王元立, 霍向东等. CSP低碳钢的晶粒细化与强韧化 [J]. 金属学报, 2002, 38: 647
|
| 20 |
Aranda M M, Kim B, Rementeria R, et al. Effect of prior austenite grain size on pearlite transformation in a hypoeuctectoid Fe-C-Mn steel [J]. Metall. Mater. Trans., 2014, 45A: 1778
|
| 21 |
Zhao H T, Palmiere E J. Effect of austenite grain size on acicular ferrite transformation in a HSLA steel [J]. Mater. Charact., 2018, 145: 479
|
| 22 |
Liang Y L, Yi Y L, Long S L, et al. Effect of rare earth elements on isothermal transformation kinetics in Si-Mn-Mo bainite steels [J]. J. Mater. Eng. Perform., 2014, 23: 4251
|
| 23 |
Jiang Z H, Wang P, Li D Z, et al. Effects of rare earth on microstructure and impact toughness of low alloy Cr-Mo-V steels for hydrogenation reactor vessels [J]. J. Mater. Sci. Technol., 2020, 45: 1
|
| 24 |
Bhattacharya A, Mondal K, Upadhyay C S, et al. A phase-field investigation of the effect of grain-boundary diffusion on austenite to ferrite transformation [J]. Comput. Mater. Sci., 2020, 173: 109428
|
| 25 |
Wang L M, Lin Q, Yue L J, et al. Study of application of rare earth elements in advanced low alloy steels [J]. J. Alloys Compd., 2008, 451: 534
|
| 26 |
Suito H, Ohta H, Morioka S. Refinement of solidification microstructure and austenite grain by fine inclusion particles [J]. ISIJ Int., 2006, 46: 840
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|