成分对真空脱锰法相变控制高硅电工钢{100}织构的影响 |
杨平1( ), 王金华1, 马丹丹1, 庞树芳2, 崔凤娥3 |
1.北京科技大学 材料科学与工程学院 北京 100083 2.鞍钢集团 钢铁研究院 鞍山 114000 3.北京科技大学 新材料技术研究院 北京 100083 |
|
Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing |
YANG Ping1( ), WANG Jinhua1, MA Dandan1, PANG Shufang2, CUI Feng'e3 |
1.School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2.Iron and Steel Research Institute, Angang Group, Anshan 114000, China 3.Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥. 成分对真空脱锰法相变控制高硅电工钢{100}织构的影响[J]. 金属学报, 2022, 58(10): 1261-1270.
Ping YANG,
Jinhua WANG,
Dandan MA,
Shufang PANG,
Feng'e CUI.
Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. Acta Metall Sin, 2022, 58(10): 1261-1270.
1 |
Sung J K, Lee D N, Wang D H, et al. Efficient generation of cube-on-face crystallographic texture in iron and its alloys [J]. ISIJ Int., 2011, 51: 284
doi: 10.2355/isijinternational.51.284
|
2 |
Sung J K, Koo Y M. Magnetic properties of Fe and Fe-Si alloys with {100}<0vw> texture [J]. J. Appl. Phys., 2013, 113: 17A338
|
3 |
Sung J K, Park S M, Shim B Y, et al. Effect of Mn on <100> texture evolution in Fe-Si-Mn alloys [J]. Mater. Sci. Forum, 2012, 702-703: 730
doi: 10.4028/www.scientific.net/MSF.702-703.730
|
4 |
Xie L, Yang P, Zhang N, et al. Formation of {100} textured columnar grain structure in a non-oriented electrical steel by phase transformation [J]. J. Magn. Magn. Mater., 2014, 356: 1
doi: 10.1016/j.jmmm.2013.12.045
|
5 |
Xie L, Yang P, Xia D S, et al. Microstructure and texture evolution in a non-oriented electrical steel during γ→α transformation under various atmosphere conditions [J]. J. Magn. Magn. Mater., 2015, 374: 655
doi: 10.1016/j.jmmm.2014.09.033
|
6 |
Zhang L W, Yang P, Mao W M. Phenomena of Σ3 and orientation gradients in an electrical steel applied α→γ→α transformation [J]. Acta Metall. Sin., 2017, 53: 19
|
6 |
章楼文, 杨 平, 毛卫民. 电工钢相变组织中的Σ3和取向梯度现象 [J]. 金属学报, 2017, 53: 19
|
7 |
Zhang L W, Yang P, Wang J H, et al. Transformation of {100} texture induced by surface effect in ultra-low carbon electrical steel [J]. J. Mater. Sci., 2016, 51: 8087
doi: 10.1007/s10853-016-0078-2
|
8 |
Xie L, He M T, Sun L Y, et al. Columnar grain growth in non-oriented electrical steels via plastic deformation of an initial columnar-grained solidification microstructure [J]. Mater. Lett., 2020, 258: 126797
doi: 10.1016/j.matlet.2019.126797
|
9 |
Xie L, He M T, Wang J T, et al. Abnormal growth of columnar grains and formation of Σ3 grain boundaries in non-oriented electrical steels [J]. Mater. Lett., 2020, 269: 127671
doi: 10.1016/j.matlet.2020.127671
|
10 |
Kovác̆ F, Dz̆ubinský M, Sidor Y. Columnar grain growth in non-oriented electrical steels [J]. J. Magn. Magn. Mater., 2004, 269: 333
doi: 10.1016/S0304-8853(03)00628-0
|
11 |
Yang P, Xia D S, Wang J H, et al. Influences of processing parameters on microstructures, textures and magnetic properties in a Fe-0.43Si-0.5Mn electrical steel subjected to phase transformation treatment [A]. Proceedings of 11th CSM steel congress [C]. Beijing: Metallurgical Industry Press, 2017: 1
|
11 |
杨 平, 夏冬生, 王金华 等. 相变法制备Fe-0.43Si-0.5Mn电工钢时工艺参数对组织结构和磁性能的影响 [A]. 第十一届中国钢铁年会论文集——S10. 电工钢 [C]. 北京: 冶金工业出版社, 2017: 1
|
12 |
Yang P, Zhang L W, Wang J H, et al. Improvement of texture and magnetic properties by surface effect induced transformation in non-oriented Fe-0.82Si-1.37Mn steel sheets [J]. Steel Res. Int., 2018, 89: 1800045
doi: 10.1002/srin.201800045
|
13 |
Kwon S B, Ahn Y K, Jeong Y K, et al. Evolution of cube-on-face texture in Fe-1%Si steel induced by physical contact during the phase transformation from γ to α [J]. Mater. Charact., 2020, 165: 110380
doi: 10.1016/j.matchar.2020.110380
|
14 |
Ahn Y K, Kwon S B, Jeong Y K, et al. Fabrication of cube-on-face textured Fe-1wt%Si and Fe-2wt%Si-1wt%Ni electrical steel using surface nucleation during γ→α phase transformation [J]. Mater. Charact., 2020, 170: 110724
doi: 10.1016/j.matchar.2020.110724
|
15 |
Xie L, Yang P, Zhang N, et al. Texture optimization for intermediate Si-containing non-oriented electrical steel [J]. J. Mater. Eng. Perform., 2014, 23: 3849
doi: 10.1007/s11665-014-1201-7
|
16 |
Tomida T, Tanaka T. Development of (100) texture in silicon steel sheets by removal of manganese and decarburization [J]. ISIJ Int., 1995, 35: 548
doi: 10.2355/isijinternational.35.548
|
17 |
Tomida T. (100)-textured 3% silicon steel sheets by manganese removal and decarburization [J]. J. Appl. Phys., 1996, 79: 5443
doi: 10.1063/1.362332
|
18 |
Tomida T, Uenoya S. Cube oriented 3%Si-1%Mn soft magnetic steel sheets with fine grain structure [J]. IEEE Trans. Magn., 2001, 37: 2318
doi: 10.1109/20.951159
|
19 |
Tomida T, Uenoya S, Sano N. Fine-grained doubly oriented silicon steel sheets and mechanism of cube texture development [J]. Mater. Trans., 2003, 44: 1106
doi: 10.2320/matertrans.44.1106
|
20 |
Tomida T. A new process to develop (100) texture in silicon steel sheets [J]. J. Mater. Eng. Perform., 1996, 5: 316
doi: 10.1007/BF02649333
|
21 |
Mao W M, Wu Y, Yu Y N, et al. Formation mechanism of texture in a new type of doubly oriented cold rolled steel [J]. Iron Steel, 2002, 37(8): 53
|
21 |
毛卫民, 吴 勇, 余永宁 等. 新型冷轧双取向硅钢组织与织构的形成机理 [J]. 钢铁, 2002, 37(8): 53
|
22 |
Wang J H, Yang P, Zhang L W, et al. Formation of a sharp {100}<011> texture in Fe-3%Si-1.7%Mn-0.05%C silicon steel sheets [J]. J. Mater. Sci., 2016, 51: 10116
doi: 10.1007/s10853-016-0240-x
|
23 |
Wang J H, Yang P, Mao W M. Retention and evolution of texture in an electrical steel under vacuum annealing [J]. J. Mater. Sci., 2017, 52: 5462
doi: 10.1007/s10853-017-0790-6
|
24 |
Wang J H, Yang P, Mao W M. Analysis of {100} texture formation in vacuum annealed electrical steel based on elastic anisotropy and surface energy anisotropy [J]. Steel. Res. Int., 2019, 90: 1800320
doi: 10.1002/srin.201800320
|
25 |
Gu C, Yang P, Mao W M. The influence of rolling process on the microstructure, texture and magnetic properties of low grades non-oriented electrical steel after phase transformation annealing [J]. Acta Metall. Sin., 2019, 55: 181
doi: 10.11900/0412.1961.2018.00187
|
25 |
顾 晨, 杨 平, 毛卫民. 轧制工艺对低牌号无取向电工钢相变退火组织、织构与磁性能的影响 [J]. 金属学报, 2019, 55: 181
|
26 |
Wei Z G, Yang P, Gu X F, et al. Transformation textures in pure titanium: Texture memory vs surface effect [J]. Mater. Charact., 2020, 164: 110359
doi: 10.1016/j.matchar.2020.110359
|
27 |
Walter J L. Control of texture in magnetic material by surface energy [J]. J. Appl. Phys., 1965, 36(3): 1213
doi: 10.1063/1.1714176
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|