| Cu含量对SiC/Al-Mg-Si-Cu复合材料自然时效负面效应的影响 |
朱士泽1,2, 王东1( ), 王全兆1, 肖伯律1( ), 马宗义1 |
1.中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2.中国科学技术大学 材料科学与工程学院 沈阳 110016 |
|
| Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites |
ZHU Shize1,2, WANG Dong1( ), WANG Quanzhao1, XIAO Bolv1( ), MA Zongyi1 |
1.Shi -Changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
朱士泽, 王东, 王全兆, 肖伯律, 马宗义. Cu含量对SiC/Al-Mg-Si-Cu复合材料自然时效负面效应的影响[J]. 金属学报, 2021, 57(7): 928-936.
Shize ZHU,
Dong WANG,
Quanzhao WANG,
Bolv XIAO,
Zongyi MA.
Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites[J]. Acta Metall Sin, 2021, 57(7): 928-936.
| 1 |
Zhou L, Zhang P F, Wang Q Z, et al. Multi-scale study on the fracture behavior of hot compression B4C/6061Al composite [J]. Acta Metall. Sin., 2019, 55: 911
|
| 1 |
周 丽, 张鹏飞, 王全兆等. B4C/6061Al复合材料热压缩断裂行为的多尺度研究 [J]. 金属学报, 2019, 55: 911
|
| 2 |
Zhu S Z, Ma G N, Wang D, et al. Suppressed negative influence of natural aging in SiCp/6092Al composites [J]. Mater. Sci. Eng., 2019, A767: 138422
|
| 3 |
Li Y Z, Wang Q Z, Wang W G, et al. Effect of interfacial reaction on age-hardening ability of B4C/6061Al composites [J]. Mater. Sci. Eng., 2015, A620: 445
|
| 4 |
Pogatscher S, Antrekowitsch H, Leitner H, et al. Mechanisms controlling the artificial aging of Al-Mg-Si Alloys [J]. Acta Mater., 2011, 59: 3352
|
| 5 |
Chang C S T, Wieler I, Wanderka N, et al. Positive effect of natural pre-ageing on precipitation hardening in Al-0.44at% Mg-0.38at% Si alloy [J]. Ultramicroscopy, 2009, 109: 585
|
| 6 |
Serizawa A, Hirosawa S, Sato T. Three-dimensional atom probe characterization of nanoclusters responsible for multistep aging behavior of an Al-Mg-Si alloy [J]. Metall. Mater. Trans., 2008, 39A: 243
|
| 7 |
Tao G H, Liu C H, Chen J H, et al. The influence of Mg/Si ratio on the negative natural aging effect in Al-Mg-Si-Cu alloys [J]. Mater. Sci. Eng., 2015, A642: 241
|
| 8 |
Zandbergen H W, Andersen S J, Jansen J. Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies [J]. Science, 1997, 277: 1221
|
| 9 |
Murayama M, Hono K, Miao W F, et al. The effect of Cu additions on the precipitation kinetics in an Al-Mg-Si alloy with excess Si [J]. Metall. Mater. Trans., 2001, 32A: 239
|
| 10 |
Torsæter M, Lefebvre W, Marioara C D, et al. Study of intergrown L and Q′ precipitates in Al-Mg-Si-Cu alloys [J]. Scr. Mater., 2011, 64: 817
|
| 11 |
Ding L P, Jia Z H, Zhang Z Q, et al. The natural aging and precipitation hardening behaviour of Al-Mg-Si-Cu alloys with different Mg/Si ratios and Cu additions [J]. Mater. Sci. Eng., 2015, A627: 119
|
| 12 |
Zandbergen M W, Cerezo A, Smith G D W. Study of precipitation in Al-Mg-Si Alloys by atom probe tomography II. Influence of Cu additions [J]. Acta Mater., 2015, 101: 149
|
| 13 |
Ma G N, Wang D, Liu Z Y, et al. Effect of hot pressing temperature on microstructure and tensile properties of SiC/Al-Zn-Mg-Cu composites [J]. Acta Metall. Sin., 2019, 55: 1319
|
| 13 |
马国楠, 王 东, 刘振宇等. 热压烧结温度对SiC/Al-Zn-Mg-Cu复合材料微观结构与力学性能的影响 [J]. 金属学报, 2019, 55: 1319
|
| 14 |
Ma G N, Wang D, Liu Z Y, et al. An investigation on particle weakening in T6-treated SiC/Al-Zn-Mg-Cu composites [J]. Mater. Charact., 2019, 158: 109966
|
| 15 |
Jin P, Xiao B L, Wang Q Z, et al. Effect of solution temperature on aging behavior and properties of SiCp/Al-Cu-Mg composites [J]. Mater. Sci. Eng., 2011, A528: 1504
|
| 16 |
Edwards G A, Stiller K, Dunlop G L, et al. The precipitation sequence in Al-Mg-Si alloys [J]. Acta Mater., 1998, 46: 3893
|
| 17 |
Bryant J D. The effects of preaging treatments on aging kinetics and mechanical properties in AA6111 aluminum autobody sheet [J]. Metall. Mater. Trans., 1999, 30A: 1999
|
| 18 |
Chang C S T, Banhart J. Low-temperature differential scanning calorimetry of an Al-Mg-Si alloy [J]. Metall. Mater. Trans., 2011, 42A: 1960
|
| 19 |
Dumitraschkewitz P, Uggowitzer P J, Gerstl S S A, et al. Size-dependent diffusion controls natural aging in aluminium alloys [J]. Nat. Commun., 2019, 10: 4746
|
| 20 |
Birol Y. Restoration of the bake hardening response in a naturally aged twin-roll cast AlMgSi automotive sheet [J]. Scr. Mater., 2006, 54: 2003
|
| 21 |
Weng Y Y, Jia Z H, Ding L P, et al. Clustering behavior during natural aging and artificial aging in Al-Mg-Si alloys with different Ag and Cu addition [J]. Mater. Sci. Eng., 2018, A732: 273
|
| 22 |
Pogatscher S, Antrekowitsch H, Leitner H, et al. Influence of the thermal route on the peak-aged microstructures in an Al-Mg-Si aluminum alloy [J]. Scr. Mater., 2013, 68: 158
|
| 23 |
Weng Y Y, Jia Z H, Ding L P, et al. Special segregation of Cu on the habit plane of lath-like β′ and QP2 precipitates in Al-Mg-Si-Cu alloys [J]. Scr. Mater., 2018, 151: 33
|
| 24 |
Jia Z H, Ding L P, Cao L F, et al. The influence of composition on the clustering and precipitation behavior of Al-Mg-Si-Cu alloys [J]. Metall. Mater. Trans., 2017, 48A: 459
|
| 25 |
Saito T, Ehlers F J H, Lefebvre W, et al. Cu atoms suppress misfit dislocations at the β″/Al interface in Al-Mg-Si alloys [J]. Scr. Mater., 2016, 110: 6
|
| 26 |
Chrominski W, Lewandowska M. Precipitation phenomena in ultrafine grained Al-Mg-Si alloy with heterogeneous microstructure [J]. Acta Mater., 2016, 103: 547
|
| 27 |
Zurob H S, Seyedrezai H. A model for the growth of solute clusters based on vacancy trapping [J]. Scr. Mater., 2009, 61: 141
|
| 28 |
Yang W S, Chen G Q, Qiao J, et al. Effect of Mg addition on the microstructure and mechanical properties of SiC nanowires reinforced 6061Al matrix composite [J]. Mater. Sci. Eng., 2017, A689: 189
|
| 29 |
Zhang Q, Ma X Y, Wu G H. Interfacial microstructure of SiCp/Al composite produced by the pressureless infiltration technique [J]. Ceram. Int., 2013, 39: 4893
|
| 30 |
Salvo L, L'Espérance G, Suéry M, et al. Interfacial reactions and age hardening in Al-Mg-Si metal matrix composites reinforced with SiC particles [J]. Mater. Sci. Eng., 1994, A177: 173
|
| 31 |
Shi Z L, Yang J M, Lee J C, et al. The interfacial characterization of oxidized SiC(p)/2014 Al composites [J]. Mater. Sci. Eng., 2001, A303: 46
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|