| 含有化合物相的共晶转变理论模型 |
许军锋1,2( ), 张宝东1, Peter K Galenko2 |
1.西安工业大学 材料与化工学院 西安 710021 2.Otto Schott Institute of Materials Research, Friedrich-Schiller-Universit?t Jena, 07743, Germany |
|
| Model of Eutectic Transformation Involving Intermetallic Compound |
XU Junfeng1,2( ), ZHANG Baodong1, Peter K Galenko2 |
1.School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710021, China 2.Otto Schott Institute of Materials Research, Friedrich-Schiller-Universität Jena, 07743, Germany |
引用本文:
许军锋, 张宝东, Peter K Galenko. 含有化合物相的共晶转变理论模型[J]. 金属学报, 2021, 57(10): 1320-1332.
Junfeng XU,
Baodong ZHANG,
Galenko Peter K.
Model of Eutectic Transformation Involving Intermetallic Compound[J]. Acta Metall Sin, 2021, 57(10): 1320-1332.
| 1 |
Zener C. Kinetics of the decomposition of austenite [J]. Trans. Am. Inst. Min. Metall. Eng., 1946, 167: 550
|
| 2 |
Tiller M. The role of interfacial energy during solid state phase transformations [J]. Jernkont. Ann., 1957, 141: 757
|
| 3 |
Tiller W. Liquid Metals and Solidification [M]. Cleveland: American Society for Metals, 1958: 276
|
| 4 |
Jackson K A, Hunt J D. Lamellar and rod eutectic growth [J]. Trans. Metall. Soc. AIME, 1966, 236: 1129
|
| 5 |
Donaghey L F, Tiller W A. On the diffusion of solute during the eutectoid and eutectic transformations, Part I [J]. Mater. Sci. Eng., 1968, A3: 231
|
| 6 |
Trivedi R, Magnin P, Kurz W. Theory of eutectic growth under rapid solidification conditions [J]. Acta Metall., 1987, 35: 971
|
| 7 |
Kurz W, Trivedi R. Eutectic growth under rapid solidification conditions [J]. Metall. Trans., 1991, 22A: 3051
|
| 8 |
Zheng L L, Larson Jr D L, Zhang H. Revised form of Jackson-Hunt theory: Application to directional solidification of MnBi/Bi eutectics [J]. J. Cryst. Growth, 2000, 209: 110
|
| 9 |
Ludwig A, Leibbrandt S. Generalised ‘Jackson-Hunt’ model for eutectic solidification at low and large Peclet numbers and any binary eutectic phase diagram [J]. Mater. Sci. Eng., 2004, A375-377: 540
|
| 10 |
Li J F, Zhou Y H. Eutectic growth in bulk undercooled melts [J]. Acta Mater., 2005, 53: 2351
|
| 11 |
Gao J R. A model for free growth of a lamellar eutectic dendrite with an incident flow [J]. Philos. Trans. Roy. Soc., 2018, 376A: 20170209
|
| 12 |
Li M J, Kuribayashi K. Nucleation-controlled microstructures and anomalous eutectic formation in undercooled Co-Sn and Ni-Si eutectic melts [J]. Metall. Mater. Trans., 2003, 34A: 2999
|
| 13 |
Wei X X, Lin X, Xu W, et al. Remelting-induced anomalous eutectic formation during solidification of deeply undercooled eutectic alloy melts [J]. Acta Mater., 2015, 95: 44
|
| 14 |
Liu L, Li J F, Zhou Y H. Solidification of undercooled eutectic alloys containing a third element [J]. Acta Mater, 2009, 57: 1536
|
| 15 |
Wang N, Kalay Y E, Trivedi R. Eutectic-to-metallic glass transition in the Al-Sm system [J]. Acta Mater., 2011, 59: 6604
|
| 16 |
Dong H, Chen Y Z, Shan G B, et al. On the nonequilibrium interface kinetics of rapid coupled eutectic growth [J]. Metall. Mater. Trans., 2017, 48A: 3823
|
| 17 |
Magnin P, Trivedi R. Eutectic growth: A modification of the Jackson and Hunt theory [J]. Acta Metall. Mater., 1991, 39: 453
|
| 18 |
Catalina A V, Sen S, Stefanescu D M. A new analytical approach to predict spacing selection in lamellar and rod eutectic systems [J]. Metall. Mater. Trans., 2003, 34A: 383
|
| 19 |
Meng G H, Lin X. Characteristic scale selection of lamellar spacings in binary eutectic solidification [J]. Acta Phys. Sin., 2014, 63: 068104
|
| 19 |
孟广慧, 林 鑫. 二元层片共晶凝固过程的特征尺度选择 [J]. 物理学报, 2014, 63: 068104
|
| 20 |
Wang H F, Liu F, Herlach D M. Kinetics of triple-junctions in eutectic solidification: A sharp interface model [J]. J. Mater. Sci., 2015, 50: 176
|
| 21 |
Galenko P K, Herlach D M. Diffusionless crystal growth in rapidly solidifying eutectic systems [J]. Phys. Rev. Lett., 2006, 96: 150602
|
| 22 |
Xu J F, Galenko P K. Effects of local nonequilibrium in rapid eutectic solidification—Part 1: Statement of the problem and general solution [J]. Math. Methods Appl. Sci., doi: 10.1002/mma.6960
|
| 23 |
Xu J F, Rettenmayr M, Galenko P K. Effects of local nonequilibrium in rapid eutectic solidification—Part 2: Analysis of effects and comparison to experiment [J]. Math. Methods Appl. Sci., doi: 10.1002/mma.7004
|
| 24 |
Azadehranjbar S, Shield J E. Multiple origins of anomalous eutectic microstructure in rapidly solidified Mg-Al alloy [J]. Materialia,
|
| 24 |
2020, 9: 100625
|
| 25 |
Fick A. On liquid diffusion [J]. J. Membr. Sci., 1955, 100: 33
|
| 26 |
Trivedi R, Kurz W. Microstructure selection in eutectic alloy systems [A]. Solidification Processing of Eutectic Alloys [C]. Warrendale, PA: TMS, 1988: 3
|
| 27 |
Trivedi R, Kurz W. Modeling of solidification microstructures in concentrated solutions and intermetallic systems [J]. Metall. Trans., 1990, 21A: 1311
|
| 28 |
Aziz M J. Model for solute redistribution during rapid solidification [J]. J. Appl. Phys., 1982, 53: 1158
|
| 29 |
Galenko P K, Jou D. Rapid solidification as non-ergodic phenomenon [J]. Phys. Rep., 2019, 818: 1
|
| 30 |
Tang L. Research on the microstructure evolution of Al-38.5%Cu hypereutectic alloy at constant and changing growth rates under directional solidification [D]. Xi'an: Northwestern Polytechnical University, 2007
|
| 30 |
唐 玲. Al-38.5%Cu过共晶合金恒速和跃迁变速定向凝固下的组织演化研究 [D]. 西安: 西北工业大学, 2007
|
| 31 |
Fopp P, Kolbe M, Kargl F, et al. Unexpected behavior of the crystal growth velocity at the hypercooling limit [J]. Phys. Rev. Mater. 2020, 4: 073405
|
| 32 |
Teppa O, Taskinen P. Thermodynamic assessment of Ni-B phase diagram [J]. Mater. Sci. Technol., 1993, 9: 205
|
| 33 |
Xu J F, Liu F, Zhang D. Phase selection of undercooled solidification of Ni-4.5wt% B alloy [J]. J. Mater. Res., 2013, 28: 3347
|
| 34 |
Raghavan V. B-Co-Fe (boron-cobalt-iron) [J]. J. Phase Equilib. Diffus., 2012, 33: 392
|
| 35 |
Tokunaga T, Ohtani H, Hasebe M. Thermodynamic study of phase equilibria in the Ni-Fe-B system [J]. J. Phase Equilib., 2005, 46: 1193
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|